08-08-2011, 11:41 AM #17
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Some sealers do a pretty good job of soaking into the surface of the concrete and a light grind will not remove them. Look for the newest revision of the ASTM to mandate some pretty aggressive grinding.

Even a heavy finishing machine with steel pans can create a dense layer on the surface that is 1/8" thick which will impede vapor movement. We have discussed this issue on other forums referring to a study conducted on a warehouse floor than remains open but very wet after 2 years of drying.

But we are getting away from your initial comment Mwoody, that the CaCl reads low and the rH reads high and there is "no legitimate reasoning for the high rH values."

I believe we can find several reasons for the high rH and we also touched on several reasons why the CaCl can read so low. My job is to help figure out what rH readings tell us about slabs, being sure to substantiate the readings we have with field evidence (because any reading is suspect until it makes sense), and help my clients determine slab condition.

If you suspect a problem with the readings you are getting, let's dissect this slab and see what we can learn! This is the fun part!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Interesting Test Result - eaadams - 05-03-2011, 09:31 AM
RE: Interesting Test Result - Ernesto - 05-03-2011, 03:46 PM
RE: Interesting Test Result - eaadams - 05-03-2011, 04:21 PM
RE: Interesting Test Result - CC Solutions - 05-04-2011, 10:15 AM
RE: Interesting Test Result - eaadams - 05-06-2011, 11:42 AM
RE: Interesting Test Result - CC Solutions - 05-06-2011, 12:26 PM
RE: Interesting Test Result - Ernesto - 05-06-2011, 04:33 PM
RE: Interesting Test Result - CC Solutions - 05-06-2011, 04:41 PM
RE: Interesting Test Result - Ernesto - 05-06-2011, 05:29 PM
RE: Interesting Test Result - eaadams - 05-07-2011, 03:08 AM
RE: Interesting Test Result - CC Solutions - 05-07-2011, 06:08 AM
RE: Interesting Test Result - Ernesto - 05-07-2011, 05:41 PM
RE: Interesting Test Result - CC Solutions - 05-07-2011, 05:47 PM
RE: Interesting Test Result - mwoody - 08-08-2011, 07:50 AM
RE: Interesting Test Result - CC Solutions - 08-08-2011, 09:03 AM
RE: Interesting Test Result - mwoody - 08-08-2011, 09:45 AM
RE: Interesting Test Result - CC Solutions - 08-08-2011, 11:41 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
6 Replies 15,260 Views
Last Post by Ernesto
05-13-2013, 04:51 PM
10 Replies 25,989 Views
Last Post by eaadams
01-18-2013, 04:48 PM
3 Replies 14,962 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 17,985 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 11,347 Views
Last Post by eaadams
07-09-2010, 09:45 AM
14 Replies 46,504 Views
Last Post by CC Solutions
01-15-2010, 09:36 PM
2 Replies 11,962 Views
Last Post by CC Solutions
12-16-2009, 11:45 AM
3 Replies 15,601 Views
Last Post by rthompson
11-04-2008, 10:03 AM

Users browsing this thread:
1 Guest(s)