03-23-2011, 05:13 PM #21
Ernesto Concrete Moisture Expert *****
Status: Offline Posts:606 Threads:33 Joined:Sep 2009
Did I say use a moisture mitigation system on top of the K-15? Where? Cool
Where did I say to put K-15 under the moisture mitigation system? Cool
If there's no contaminants then no shotblasting is needed, you can simply scarify.

But really, what slab in a house is not going to get a floorcovering treatment? The concrete people need to start broom finishing the slabs. Everything sticks better.

Oh and you didn't copy the full text.

Surface Preparation:
Surfaces must be absorptive, clean, free from loose materials,
oil, grease, sealers, curing compounds, waxes, silicates, laitance,
and all other surface contaminants that may inhibit proper bond.
Completely remove cutback adhesive residue or other surface
contaminants by shotblasting. All surfaces to be treated must
have a profile of CSP 2-3 (similar to light broom finish), as
defined by ICRI (International Concrete Repair Institute,
Guideline No. 03732).
Surface areas requiring patching or leveling must be treated
using Durabond® Webcrete® 95, Webcrete 98 or Duralevel®
83P Fast Set patches/underlayments on top of the D-261
Extreme Moisture Vapor Barrier Coating according to label
instructions. Durabond Extreme Primer must be used prior to
the installation of these cementitious products

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
Concrete floor and laminate - morrisey - 03-21-2011, 08:03 AM
RE: Concrete floor and laminate - CC Solutions - 03-21-2011, 01:19 PM
RE: Concrete floor and laminate - morrisey - 03-21-2011, 01:29 PM
RE: Concrete floor and laminate - Ernesto - 03-21-2011, 04:34 PM
RE: Concrete floor and laminate - CC Solutions - 03-21-2011, 05:03 PM
RE: Concrete floor and laminate - eaadams - 03-21-2011, 08:57 PM
RE: Concrete floor and laminate - morrisey - 03-22-2011, 03:40 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 05:53 AM
RE: Concrete floor and laminate - morrisey - 03-22-2011, 06:01 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 06:17 AM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 08:13 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 09:01 AM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 02:43 PM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 03:47 PM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 07:23 PM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 06:20 AM
RE: Concrete floor and laminate - eaadams - 03-23-2011, 09:28 AM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 09:56 AM
RE: Concrete floor and laminate - eaadams - 03-23-2011, 10:17 AM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 03:19 PM
RE: Concrete floor and laminate - Ernesto - 03-23-2011, 05:13 PM
RE: Concrete floor and laminate - CC Solutions - 03-24-2011, 06:28 AM
RE: Concrete floor and laminate - Ernesto - 03-24-2011, 08:31 AM
RE: Concrete floor and laminate - CC Solutions - 03-24-2011, 08:42 AM
RE: Concrete floor and laminate - Ernesto - 03-24-2011, 07:52 PM
RE: Concrete floor and laminate - Ernesto - 03-25-2011, 07:28 AM
RE: Concrete floor and laminate - eaadams - 03-25-2011, 09:24 AM
RE: Concrete floor and laminate - Ernesto - 03-25-2011, 05:16 PM
RE: Concrete floor and laminate - eaadams - 03-25-2011, 07:26 PM
RE: Concrete floor and laminate - Ernesto - 03-26-2011, 07:03 PM
RE: Concrete floor and laminate - eaadams - 03-26-2011, 09:36 PM
RE: Concrete floor and laminate - T_Schneider - 03-28-2011, 05:31 AM
RE: Concrete floor and laminate - eaadams - 03-28-2011, 09:45 AM
RE: Concrete floor and laminate - T_Schneider - 03-28-2011, 10:33 AM
RE: Concrete floor and laminate - eaadams - 03-28-2011, 09:14 PM
RE: Concrete floor and laminate - Ernesto - 03-28-2011, 09:22 PM
RE: Concrete floor and laminate - T_Schneider - 03-29-2011, 07:34 AM
RE: Concrete floor and laminate - Ernesto - 03-29-2011, 05:17 PM
RE: Concrete floor and laminate - morrisey - 03-30-2011, 04:38 AM
RE: Concrete floor and laminate - T_Schneider - 03-30-2011, 05:39 AM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 12:08 PM
RE: Concrete floor and laminate - eaadams - 03-31-2011, 12:16 PM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 12:16 PM
RE: Concrete floor and laminate - Ernesto - 03-31-2011, 06:46 PM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 07:02 PM
RE: Concrete floor and laminate - Ernesto - 04-01-2011, 06:53 AM
RE: Concrete floor and laminate - CC Solutions - 04-01-2011, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 12,359 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 31,316 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 41,647 Views
Last Post by eaadams
11-08-2013, 01:41 PM
21 Replies 76,744 Views
Last Post by CCR
07-19-2013, 05:14 PM
35 Replies 106,163 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 15,392 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 96,428 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 6,158 Views
Last Post by eaadams
03-23-2012, 09:40 AM
2 Replies 13,468 Views
Last Post by eaadams
12-23-2011, 12:06 PM
23 Replies 77,402 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM

Users browsing this thread:
1 Guest(s)