03-21-2011, 08:03 AM #1
morrisey Newbie *
Status: Offline Posts:5 Threads:1 Joined:Mar 2011
The Reader's Digest version of our saga is that 4 years ago we had laminate flooring installed (over previously carpeted/tiled areas) in 75% of our home (built in 1987)--. The laminate began to bubble at many of the seams. After a protracted time of dealing with one of the national home improvement chains, they agreed to replace the laminate. When they began pulling up the old laminate --black mold everywhere. We've now been out of our home for 2+ weeks while it goes through mold remediation. It appears that there were 2 possible causes of the problem-- the underlayment was improperly installed and we have a "wet slab" (90%+ rh). The area that had previously been tiled had no mold whatsoever
The question -- we still want to re-install laminate. Will a sealer, such as MVP and a higher grade, properly installed underlayment solve our problem or are we doomed to tile and carpet??








Messages In This Thread
Concrete floor and laminate - morrisey - 03-21-2011, 08:03 AM
RE: Concrete floor and laminate - CC Solutions - 03-21-2011, 01:19 PM
RE: Concrete floor and laminate - morrisey - 03-21-2011, 01:29 PM
RE: Concrete floor and laminate - Ernesto - 03-21-2011, 04:34 PM
RE: Concrete floor and laminate - CC Solutions - 03-21-2011, 05:03 PM
RE: Concrete floor and laminate - eaadams - 03-21-2011, 08:57 PM
RE: Concrete floor and laminate - morrisey - 03-22-2011, 03:40 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 05:53 AM
RE: Concrete floor and laminate - morrisey - 03-22-2011, 06:01 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 06:17 AM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 08:13 AM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 09:01 AM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 02:43 PM
RE: Concrete floor and laminate - CC Solutions - 03-22-2011, 03:47 PM
RE: Concrete floor and laminate - Ernesto - 03-22-2011, 07:23 PM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 06:20 AM
RE: Concrete floor and laminate - eaadams - 03-23-2011, 09:28 AM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 09:56 AM
RE: Concrete floor and laminate - eaadams - 03-23-2011, 10:17 AM
RE: Concrete floor and laminate - CC Solutions - 03-23-2011, 03:19 PM
RE: Concrete floor and laminate - Ernesto - 03-23-2011, 05:13 PM
RE: Concrete floor and laminate - CC Solutions - 03-24-2011, 06:28 AM
RE: Concrete floor and laminate - Ernesto - 03-24-2011, 08:31 AM
RE: Concrete floor and laminate - CC Solutions - 03-24-2011, 08:42 AM
RE: Concrete floor and laminate - Ernesto - 03-24-2011, 07:52 PM
RE: Concrete floor and laminate - Ernesto - 03-25-2011, 07:28 AM
RE: Concrete floor and laminate - eaadams - 03-25-2011, 09:24 AM
RE: Concrete floor and laminate - Ernesto - 03-25-2011, 05:16 PM
RE: Concrete floor and laminate - eaadams - 03-25-2011, 07:26 PM
RE: Concrete floor and laminate - Ernesto - 03-26-2011, 07:03 PM
RE: Concrete floor and laminate - eaadams - 03-26-2011, 09:36 PM
RE: Concrete floor and laminate - T_Schneider - 03-28-2011, 05:31 AM
RE: Concrete floor and laminate - eaadams - 03-28-2011, 09:45 AM
RE: Concrete floor and laminate - T_Schneider - 03-28-2011, 10:33 AM
RE: Concrete floor and laminate - eaadams - 03-28-2011, 09:14 PM
RE: Concrete floor and laminate - Ernesto - 03-28-2011, 09:22 PM
RE: Concrete floor and laminate - T_Schneider - 03-29-2011, 07:34 AM
RE: Concrete floor and laminate - Ernesto - 03-29-2011, 05:17 PM
RE: Concrete floor and laminate - morrisey - 03-30-2011, 04:38 AM
RE: Concrete floor and laminate - T_Schneider - 03-30-2011, 05:39 AM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 12:08 PM
RE: Concrete floor and laminate - eaadams - 03-31-2011, 12:16 PM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 12:16 PM
RE: Concrete floor and laminate - Ernesto - 03-31-2011, 06:46 PM
RE: Concrete floor and laminate - CC Solutions - 03-31-2011, 07:02 PM
RE: Concrete floor and laminate - Ernesto - 04-01-2011, 06:53 AM
RE: Concrete floor and laminate - CC Solutions - 04-01-2011, 07:56 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 14,030 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 36,193 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 44,349 Views
Last Post by eaadams
11-08-2013, 01:41 PM
21 Replies 82,409 Views
Last Post by CCR
07-19-2013, 05:14 PM
35 Replies 115,004 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 16,952 Views
Last Post by eaadams
01-30-2013, 04:43 PM
32 Replies 103,961 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
0 Replies 6,658 Views
Last Post by eaadams
03-23-2012, 09:40 AM
2 Replies 14,335 Views
Last Post by eaadams
12-23-2011, 12:06 PM
23 Replies 83,162 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM

Users browsing this thread:
2 Guest(s)