Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
ASR is tough, but can be repaired. Typically you have to remove some of the surface and add a new layer of cementitious material. There are those who advocate an assembly system where a dimpled material with an upper hard surface is installed, allowing the floor below to breath and therefor not letting the moisture build in the slab aggravating the ASR. I have seen some flood the floor with lithium nitrate attempting to bind the reactive silicate constituents and keep them from reacting with the alkali cement.

We midwesterners don't see ASR as often as some in the south and west, (knocking on wood....) but the one time I had to deal with it I scarified the concrete down an inch and added a new top layer of cement.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Old concrete slab moisture - DeanC - 03-10-2011, 09:26 AM
RE: Old concrete slab moisture - eaadams - 03-10-2011, 10:20 AM
RE: Old concrete slab moisture - Leie Sualua - 03-14-2011, 12:16 PM
RE: Old concrete slab moisture - CC Solutions - 03-14-2011, 12:48 PM
RE: Old concrete slab moisture - Leie Sualua - 03-14-2011, 02:39 PM
RE: Old concrete slab moisture - CC Solutions - 03-15-2011, 02:12 PM
RE: Old concrete slab moisture - DeanC - 03-15-2011, 03:14 PM
RE: Old concrete slab moisture - Ernesto - 03-16-2011, 07:05 PM
RE: Old concrete slab moisture - CC Solutions - 03-16-2011, 08:43 PM
RE: Old concrete slab moisture - Ernesto - 03-17-2011, 09:56 AM
RE: Old concrete slab moisture - CC Solutions - 03-17-2011, 10:43 AM
RE: Old concrete slab moisture - Ernesto - 03-17-2011, 06:04 PM
RE: Old concrete slab moisture - CC Solutions - 03-17-2011, 08:07 PM
RE: Old concrete slab moisture - Ernesto - 03-18-2011, 07:29 AM
RE: Old concrete slab moisture - Ernesto - 03-18-2011, 10:37 AM
RE: Old concrete slab moisture - Ernesto - 03-18-2011, 05:43 PM
RE: Old concrete slab moisture - eaadams - 03-24-2011, 09:34 PM
RE: Old concrete slab moisture - Ernesto - 03-25-2011, 05:53 PM
RE: Old concrete slab moisture - CC Solutions - 04-01-2011, 08:00 AM
RE: Old concrete slab moisture - eaadams - 04-01-2011, 09:02 AM
RE: Old concrete slab moisture - CC Solutions - 04-01-2011, 09:06 AM
RE: Old concrete slab moisture - Ernesto - 04-01-2011, 03:30 PM
RE: Old concrete slab moisture - CC Solutions - 04-01-2011, 09:00 PM
RE: Old concrete slab moisture - foxgeorge - 12-15-2011, 01:20 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 8,614 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 11,244 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 28,243 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 7,349 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
4 Replies 8,968 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
16 Replies 44,828 Views
Last Post by Ernesto
04-15-2014, 02:30 PM
9 Replies 39,902 Views
Last Post by eaadams
11-08-2013, 01:41 PM
2 Replies 10,093 Views
Last Post by eaadams
09-27-2013, 10:26 AM
35 Replies 100,920 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 14,464 Views
Last Post by eaadams
01-30-2013, 04:43 PM

Users browsing this thread:
1 Guest(s)