(07-25-2012, 08:59 PM)Rubensgt40 Wrote:  Correct me if I'm wrong JD, but I assumed your point was relating to the portion of slab immediately below the probe having the upward passage of RH "blocked", so to speak, and drying slightly different to the surrounding slab?

Exactly.... Obviously if you plug the hole with a rubber stopper it will retain moisture. Conversely if you leave the hole open you will dry the slab out at the 40% deep hole you drilled.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Rapid RH probe out of calibration? - Rubensgt40 - 07-22-2012, 08:02 PM
RE: Rapid RH probe out of calibration? - CCR - 07-23-2012, 11:23 AM
RE: Rapid RH probe out of calibration? - Rubensgt40 - 07-23-2012, 08:53 PM
RE: Rapid RH probe out of calibration? - eaadams - 07-24-2012, 03:12 PM
RE: Rapid RH probe out of calibration? - CC Solutions - 07-24-2012, 03:59 PM
RE: Rapid RH probe out of calibration? - eaadams - 07-24-2012, 04:05 PM
RE: Rapid RH probe out of calibration? - rapidrhrep - 07-25-2012, 08:22 AM
RE: Rapid RH probe out of calibration? - Rubensgt40 - 07-25-2012, 08:59 PM
RE: Rapid RH probe out of calibration? - CC Solutions - 07-30-2012, 04:42 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
1 Replies 5,791 Views
Last Post by rapidrhrep
05-07-2015, 04:18 PM
7 Replies 20,421 Views
Last Post by rapidrhrep
02-20-2014, 01:49 PM
1 Replies 9,376 Views
Last Post by CC Solutions
04-29-2013, 06:50 PM
3 Replies 19,177 Views
Last Post by CC Solutions
02-21-2011, 02:50 PM

Users browsing this thread:
1 Guest(s)