07-12-2012, 12:50 PM #18
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
I have a 2nd tester now using a puddy like caulking between the cap and sleve / concrete. Fails often but doesn't prevent surface moisture from coming out.

Is there such a thing as a duct type tape that breaths? like a mesh tape? I'd be more comfortable with that.

In reality I picture a new wagner product. It would be a cylinder (battery shaped) made to fit in the meter hole. It would fill the hole and prevent debris from entering and then I would also have a metal core running the full length so I could remove it with a [edit: magnet]. If you wanted to get fancy you could integrate a mushroom cap shape to it to protect the edges.








Messages In This Thread
Can tape over the probe cause erroneous readings? - CC Solutions - 10-04-2011, 04:00 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 04:07 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 10-12-2011, 06:50 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 10-12-2011, 06:54 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-25-2012, 11:38 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 06-26-2012, 05:52 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 04:57 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-01-2012, 08:42 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-01-2012, 09:09 AM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 12:44 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 01:20 PM
RE: Can tape over the probe cause erroneous readings? - rthompson - 07-03-2012, 02:02 PM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-03-2012, 02:17 PM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-09-2012, 01:27 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-10-2012, 10:47 AM
RE: Can tape over the probe cause erroneous readings? - CC Solutions - 07-12-2012, 06:06 AM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-12-2012, 07:41 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 07-12-2012, 12:50 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 07-24-2013, 04:47 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 07-31-2013, 01:05 PM
RE: Can tape over the probe cause erroneous readings? - CCR - 08-01-2013, 04:08 AM
RE: Can tape over the probe cause erroneous readings? - eaadams - 06-02-2014, 10:17 PM
RE: Can tape over the probe cause erroneous readings? - Ernesto - 06-03-2014, 03:49 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
2 Replies 16,860 Views
Last Post by CC Solutions
09-02-2011, 06:25 AM

Users browsing this thread:
1 Guest(s)