Well my guess is the same as what happened with me, in the exact same situation (latex sealer, miracle glue, failure immediately.... Hey, are you me, posting when I have those blackout periods??? Confused )

Anyway, I probed the slab for depth readings and found it varied between 4 and 9 inches. Exclamation

What kind of concrete installers get that sloppy? Maybe they aren't backfilling the cement truck tracks as the truck backs out? It sure makes a poor slab when the thickness varies!!!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

07-19-2013, 05:14 PM #22
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
4-9 is QUITE a range. Maybe they were charging by the yard ($ cha-ching). I just wish they'd quit power troweling the heck out of new concrete. Isn't anybody out there listening, reading, or learning anything from their mistakes???

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Possibly Related Threads...
Thread / Author Replies / Views Last Post
35 Replies 122,228 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 18,255 Views
Last Post by eaadams
01-30-2013, 04:43 PM
33 Replies 100,276 Views
Last Post by eaadams
11-21-2012, 10:19 AM
2 Replies 14,994 Views
Last Post by eaadams
12-23-2011, 12:06 PM
46 Replies 163,507 Views
Last Post by CC Solutions
04-01-2011, 07:56 AM

Users browsing this thread:
1 Guest(s)