All Species
A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z
Common Name | Botanical Name | Specific Gravity | Verified |
---|---|---|---|
A Koura | Lophira alata | 0.94 | |
Aba | Lophira alata | 0.94 | |
Abacateiro | Hieronyma alchorneoides | 0.58 | |
Triplochiton scleroxylon | 0.32 | ||
Abacu | Tieghemella heckelii | 0.60 | |
Abako | Tieghemella heckelii | 0.60 | |
Abaku | Tieghemella heckelii | 0.60 | |
Abang | Chlorophora excelsa | 0.70 | |
Abang | Chlorophora regia | 0.59 | |
Buxus sempervirens | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Abbihal | Erythrophloeum densiflorum | 0.68 | |
Abecou | Tieghemella heckelii | 0.60 | |
Abeille | Manilkara bidentata | 0.95 | |
Abem | Berlinia acuminata | 0.64 | |
Abenbele | Pouteria izabalensis | 0.64 | |
Abnus | Diospyros ebenum | 0.84 | |
Abogo | Isoberlinia doka | 0.63 | |
Abome | Musanga cecropioides | 0.23 | |
Aborzok | Mammea africana | 0.69 | |
Aborzole | Mammea africana | 0.69 | |
Abotoasebie | Mammea africana | 0.69 | |
Abotzok | Mammea africana | 0.69 | |
Abrico do Para | Mammea americana | 0.74 | |
Abricot | Mammea americana | 0.74 | |
Abricot de Saint Domingue | Mammea americana | 0.74 | |
Abricot des Antilles | Mammea americana | 0.74 | |
Abricot du Pays | Mammea americana | 0.74 | |
Abricoteiro | Mammea americana | 0.74 | |
Abricotier | Mammea americana | 0.74 | |
Abricotier d'Amerique | Mammea americana | 0.74 | |
Abrompesowa | Mammea africana | 0.69 | |
Abura | Mitragyna ciliata | 0.52 | |
Abura | Mitragyna stipulosa | 0.53 | |
Diospyros ebenum | 0.94 | ||
Albizia lebbeck | 0.54 | ||
Acacia | Albizia procera | 0.55 | |
Robinia pseudoacacia | 0.69 | ||
Hura crepitans | 0.40 | ||
Acaiquara | Minquartia guianensis | 0.83 | |
Swietenia macrophylla | 0.47 | ||
Acajou | Swietenia mahagoni | 0.57 | |
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Acajou de Cuba | Sickingia salvadorense | 0.65 | |
Acajou de Cuba | Swietenia mahagoni | 0.57 | |
Acajou de Saint Domingue | Swietenia mahagoni | 0.57 | |
Acajou de St. Domingue | Sickingia salvadorense | 0.65 | |
Acajou de St. Domingue | Swietenia mahagoni | 0.57 | |
Acajou des Antilles | Swietenia mahagoni | 0.57 | |
Swietenia macrophylla | 0.47 | ||
Acajou Rouge | Cedrela huberi | 0.40 | 4 |
Cedrela odorata | 0.39 | ||
Khaya nyassica | 0.44 | ||
Acana | Manilkara bidentata | 0.95 | |
Acana | Pouteria izabalensis | 0.64 | |
Acana | Pouteria pomifera | 0.84 | |
Tabebuia serratifolia | 0.99 | ||
Acapu | Minquartia guianensis | 0.83 | |
Acar-Huacapu | Minquartia guianensis | 0.83 | |
Acaricaara | Minquartia guianensis | 0.83 | |
Acaricoara | Minquartia guianensis | 0.83 | |
Acaricuara | Minquartia guianensis | 0.83 | |
Acarioba | Minquartia guianensis | 0.83 | |
Acariquara | Minquartia guianensis | 0.83 | |
Hura crepitans | 0.40 | ||
Platymiscium pinnatum | 0.87 | ||
Diospyros ebenum | 0.94 | ||
Achi | Brachystegia laurentii | 0.57 | |
Achiwa | Vochysia guianensis | 0.52 | |
Acrot | Aleurites moluccana | 0.14 | |
Hura crepitans | 0.40 | ||
Hura crepitans | 0.40 | ||
Ada | Terminalia ivorensis | 0.54 | |
Ada boumbra | Terminalia ivorensis | 0.54 | |
Adaan | Albizia procera | 0.55 | |
Adarouna | Catostemma fragrans | 0.66 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.80 | ||
Adirondack Spruce | Picea glauca | 0.36 | 3 |
Adjouaba | Dacryodes le testui | 0.56 | |
Turraeanthus africanus | 0.51 | ||
Terminalia superba | 0.40 | ||
Terminalia superba | 0.40 | ||
Afara Duclu | Terminalia ivorensis | 0.54 | |
Afara Dudu | Terminalia ivorensis | 0.54 | |
Afara-Dudu | Terminalia ivorensis | 0.54 | |
Afas | Vitex cofassus | 0.67 | |
Afia | Terminalia ivorensis | 0.54 | |
Terminalia superba | 0.40 | ||
Afo | Poga oleosa | 0.39 | |
Terminalia superba | 0.40 | ||
Afop Zam | Mitragyna stipulosa | 0.53 | |
Terminalia superba | 0.40 | ||
Afrikaans Padoek | Pterocarpus soyauxii | 0.64 | |
African Apple | Mammea africana | 0.69 | |
African Apricot | Mammea africana | 0.69 | |
African Black Walnut | Mansonia altissima | 0.55 | |
African Boxwood | Gonioma kamassi | 0.85 | |
African Brazil Nut | Poga oleosa | 0.39 | |
Triplochiton scleroxylon | 0.32 | ||
African Cherry | Tieghemella heckelii | 0.60 | |
Pterocarpus soyauxii | 0.64 | ||
African Corkwood | Musanga cecropioides | 0.23 | |
African Ebony | Diospyros ebenum | 0.94 | 10 |
Turraeanthus africanus | 0.51 | ||
African Greenheart | Piptadeniastrum africanum | 0.63 | |
African Greenheart | Terminalia ivorensis | 0.54 | |
African Homalium | Homalium dolicophyllum | 0.63 | |
African Linden | Mitragyna stipulosa | 0.53 | |
African Mahogany | Khaya nyassica | 0.44 | 2 |
African Mammea Apple | Mammea africana | 0.69 | |
African Mammy Apple | Mammea africana | 0.69 | |
African Mango | Irvingia gabonensis | 0.76 | |
Triplochiton scleroxylon | 0.32 | ||
African Oak | Chlorophora excelsa | 0.70 | |
African Oak | Lophira alata | 0.94 | |
African Padauk | Pterocarpus soyauxii | 0.64 | 4 |
African Pterygota | Pterygota bequaertii | 0.53 | |
African Pterygota | Pterygota macrocarpa | 0.54 | |
African Rosewood | Guibourtia coleosperma | 0.66 | |
Turraeanthus africanus | 0.51 | ||
African Teak | Chlorophora excelsa | 0.70 | |
African Tulip | Spathodea campanulata | 0.25 | |
African Tuliptree | Spathodea campanulata | 0.25 | |
African Walnut | Lovoa trichiliodes | 0.46 | |
African Walnut | Mansonia altissima | 0.55 | |
Triplochiton scleroxylon | 0.32 | ||
African Yellow Wood | Terminalia ivorensis | 0.54 | |
Microberlinia brazzavillensis | 0.77 | ||
Pterocarpus soyauxii | 0.64 | ||
Pterocarpus soyauxii | 0.64 | ||
Pterocarpus soyauxii | 0.64 | ||
Pterocarpus soyauxii | 0.64 | ||
Afrormosia | Pericopsis elata | 0.65 | 2 |
Afun | Mansonia altissima | 0.55 | |
Afzelia | Afzelia bipindensis | 0.62 | |
Afzelia | Afzelia pachyloba | 0.62 | |
Afzelia | Afzelia quanzensis | 0.62 | |
Aga Umbrella Tree | Musanga cecropioides | 0.23 | |
Agamokive | Tieghemella heckelii | 0.60 | |
Agamokwe | Tieghemella heckelii | 0.60 | |
Aganananga | Catostemma fragrans | 0.66 | |
Aganokpe | Tieghemella heckelii | 0.60 | |
Aganokwe | Mimusops heckelii | 0.55 | |
Aganokwe | Tieghemella heckelii | 0.60 | |
Turraeanthus africanus | 0.51 | ||
Agbion | Piptadeniastrum africanum | 0.63 | |
Agboin | Piptadeniastrum africanum | 0.63 | |
Agbome | Musanga cecropioides | 0.23 | |
Agbons | Irvingia gabonensis | 0.76 | |
Turraeanthus africanus | 0.51 | ||
Turraeanthus africanus | 0.51 | ||
Turraeanthus africanus | 0.51 | ||
Aggai | Dillenia pentagyna | 0.55 | |
Terminalia superba | 0.40 | ||
Agidilif | Mitragyna stipulosa | 0.53 | |
Aglaia | Aglaia gigantea | 0.54 | |
Agofa | Mitragyna ciliata | 0.52 | |
Agoho | Casuarina equisetifolia | 0.87 | |
Agoko | Casuarina equisetifolia | 0.87 | |
Agoo | Casuarina equisetifolia | 0.87 | |
Agoso | Casuarina equisetifolia | 0.87 | |
Agoumi | Musanga cecropioides | 0.23 | |
Agracejo | Gossypiospermum praecox | 0.77 | |
Agracejo de Monte | Gossypiospermum praecox | 0.77 | |
Aguacatillo | Hieronyma alchorneoides | 0.58 | |
Aguacatillo | Hyeronyma laxiflora | 0.58 | |
Aguano | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Aguano | Swietenia mahagoni | 0.57 | |
Aguaras | Tetragastris altissima | 0.74 | |
Aguay | Pouteria pomifera | 0.84 | |
Agui | Chlorophora excelsa | 0.70 | |
Agulasing | Aglaia gigantea | 0.54 | |
Pometia pinnata | 0.60 | ||
Agyemkama | Musanga cecropioides | 0.23 | |
Ahorn | Acer campestre | 0.55 | |
Ahsang | Vitex cofassus | 0.67 | |
Taxodium distichum | 0.46 | ||
Taxodium distichum | 0.46 | ||
Ai Fra Mas | Intsia bijuga | 0.65 | |
Pometia pinnata | 0.60 | ||
Aibu | Syzygium buettnerianum | 0.73 | |
Aimela | Syzygium buettnerianum | 0.73 | |
Ainee | Artocarpus hirsuta | 0.52 | |
Ainunura | Gonystylus macrophyllum | 0.54 | |
Aisarufa | Syzygium buettnerianum | 0.73 | |
Aiyanepelo | Artocarpus hirsuta | 0.52 | |
Aiyo | Afzelia quanzensis | 0.62 | |
Aizella | Intsia bijuga | 0.65 | |
Aizella | Intsia palembanica | 0.65 | |
Aj’ | Caryocar villosum | 0.76 | |
Ajama | Musanga cecropioides | 0.23 | |
Ajo | Cordia alliodora | 0.51 | |
Ajo ajo | Cordia alliodora | 0.51 | |
Ajoajo | Cordia alliodora | 0.51 | |
Triplochiton scleroxylon | 0.32 | ||
Akagaouan | Bombax brevicuspe | 0.35 | |
Terminalia superba | 0.40 | ||
Akasanumu | Piptadeniastrum africanum | 0.63 | |
Ake | Pterygota bequaertii | 0.53 | |
Ake | Pterygota macrocarpa | 0.54 | |
Ake | Testulea gabonensis | 0.76 | |
Akeche | Antiaris toxicaria | 0.35 | |
Akede | Chlorophora excelsa | 0.70 | |
Akewa | Testulea gabonensis | 0.76 | |
Akewe | Testulea gabonensis | 0.76 | |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Pometia pinnata | 0.60 | ||
Akle | Albizia procera | 0.55 | |
Akleng parang | Albizia procera | 0.55 | |
Ako | Antiaris toxicaria | 0.35 | |
Pometia pinnata | 0.60 | ||
Akoga | Lophira alata | 0.94 | |
Akogka | Lophira alata | 0.94 | |
Akogo | Lophira alata | 0.94 | |
Akok | Beilschmiedia mannii | 0.62 | |
Akolodo | Brachystegia laurentii | 0.57 | |
Terminalia superba | 0.40 | ||
Akot | Drypetes gossweileri | 0.63 | |
Akpakosso | Mitragyna stipulosa | 0.53 | |
Akpakpla | Lophira alata | 0.94 | |
Akrod | Aleurites moluccana | 0.14 | |
Castanea sativa | 0.51 | ||
Pterocarpus soyauxii | 0.64 | ||
Cedrela odorata | 0.39 | ||
Pometia pinnata | 0.60 | ||
Akwakwa | Oxystigma oxyphyllum | 0.53 | |
Tabebuia serratifolia | 0.99 | ||
Alal | Pinus insularis | 0.50 | |
Alalangad | Albizia procera | 0.55 | |
Alamag | Aglaia gigantea | 0.54 | |
Populus tremuloides | 0.38 | ||
Tabebuia serratifolia | 0.99 | ||
Alangilan | Canangium odoratum | 0.28 | |
Pometia pinnata | 0.60 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Alaska Cedar | Chamaecyparis nootkatensis | 0.44 | 3 |
Chamaecyparis nootkatensis | 0.44 | ||
Chamaecyparis nootkatensis | 0.44 | ||
Larix laricina | 0.53 | ||
Tsuga heterophylla | 0.45 | ||
Chamaecyparis nootkatensis | 0.44 | ||
Albero di Paternoster | Melia azedarach | 0.51 | |
Albizzia | Albizia procera | 0.55 | |
Tabebuia serratifolia | 0.99 | ||
Alcarreto | Aspidosperma desmanthum | 0.65 | |
Alcornoque | Mora excelsa | 0.89 | |
Alder | Alnus glutinosa | 0.41 | |
Alder | Alnus nepalensis | 0.26 | |
Alnus rubra | 0.41 | ||
Alelaila | Melia azedarach | 0.51 | |
Aleli | Melia azedarach | 0.51 | |
Alexandrian Laurel | Calophyllum inophyllum | 0.55 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Prioria copaifera | 0.42 | ||
Aligna | Afzelia bipindensis | 0.62 | |
Aligna | Afzelia pachyloba | 0.62 | |
Aligna | Afzelia quanzensis | 0.62 | |
Alilaila | Melia azedarach | 0.51 | |
Al-langigan | Canangium odoratum | 0.28 | |
Allen Ele | Microberlinia brazzavillensis | 0.77 | 3 |
Liquidambar styraciflua | 0.52 | ||
Alm | Ulmus glabra | 0.53 | |
Almaciga | Agathis borneensis | 0.41 | |
Almaciga | Agathis philippinensis | 0.33 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.80 | ||
Almendrillo | Caryocar villosum | 0.76 | |
Almendr—n | Caryocar villosum | 0.76 | |
Almendro | Caryocar villosum | 0.76 | |
Almendro | Dipteryx odorata | 0.82 | |
Almendro | Terminalia amazonia | 0.76 | |
Almendro | Terminalia amazonica | 0.76 | |
Almiqui | Manilkara bidentata | 0.95 | |
Almon | Shorea contorta | 0.37 | 4 |
Almon | Shorea leprosula | 0.50 | 4 |
Almon | Shorea leptoclados | 0.38 | 4 |
Almon | Shorea smithiana | 0.43 | 4 |
Alm Žndro | Caryocar villosum | 0.76 | |
Aloe | Excoecaria agallocha | 0.42 | |
Alona Wood | Lovoa trichiliodes | 0.46 | |
Alone | Bombax brevicuspe | 0.35 | |
Alone | Bombax chevalieri | 0.51 | |
Pometia pinnata | 0.60 | ||
Abies amabilis | 0.43 | ||
Abies lasiocarpa | 0.32 | ||
Tabebuia serratifolia | 0.99 | ||
Aluppe | Bassia latifolia | 0.82 | |
Abies amabilis | 0.43 | ||
Amacey | Tetragastris altissima | 0.74 | |
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Tabebuia serratifolia | 0.99 | ||
Amapa Prieta | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Amapa Rana | Brosimum rubescens | 0.63 | |
Amapola | Spathodea campanulata | 0.25 | |
Amarante | Peltogyne porphyrocardia | 0.69 | |
Amarante | Peltogyne venosa | 0.69 | |
Amaranth | Peltogyne porphyrocardia | 0.69 | |
Amaranth | Peltogyne venosa | 0.69 | |
Amaratante | Peltogyne venosa | 0.69 | |
Plathymenia reticulata | 0.56 | ||
Plathymenia reticulata | 0.56 | ||
Amarillo | Cordia alliodora | 0.51 | |
Amarillo Carabazuelo | Terminalia amazonia | 0.76 | |
Amarillo Carabazuelo | Terminalia amazonica | 0.76 | |
Amarillo de Panama | Terminalia amazonia | 0.76 | |
Amarillon | Terminalia amazonia | 0.76 | |
Amat | Tetramerista glabra | 0.73 | |
Amaya | Musanga cecropioides | 0.23 | |
Amazakoue | Guibourtia ehie | 0.71 | 4 |
Amazoue | Guibourtia ehie | 0.71 | 4 |
Pterocarpus angolensis | 0.59 | ||
Am-bop | Mitragyna stipulosa | 0.53 | |
Amboyna | Pterocarpus indicus | 0.57 | 3 |
Ambugis | Koordersiodendron pinnatum | 0.71 | |
Amburana | Amburana cearensis | 0.58 | 4 |
Amburana cearensis | 0.58 | ||
Plathymenia reticulata | 0.56 | ||
Fraxinus americana | 0.60 | ||
Fraxinus pennsylvanica | 0.56 | ||
American Basswood | Tilia americana | 0.37 | 1 |
American Beech | Fagus grandifolia | 0.64 | 1 |
Betula alleghaniensis | 0.62 | ||
Betula papyrifera | 0.55 | ||
Fraxinus nigra | 0.49 | ||
Prunus serotina | 0.50 | ||
Juglans nigra | 0.55 | ||
American Chestnut | Castanea dentata | 0.43 | 1 |
Diospyros virginiana | 0.71 | ||
American Elm | Ulmus americana | 0.50 | 1 |
Tsuga canadensis | 0.40 | ||
American Holly | Ilex opaca | 0.55 | 3 |
American Tornbeam | Carpinus caroliniana | 0.64 | |
Larix laricina | 0.53 | ||
American Light Cordia | Cordia alliodora | 0.51 | |
Tilia americana | 0.37 | ||
Tilia americana | 0.37 | ||
Swietenia macrophylla | 0.47 | ||
Pinus elliottii | 0.59 | ||
Pinus palustris | 0.59 | ||
Platanus occidentalis | 0.49 | ||
Platanus occidentalis | 0.49 | ||
American PlanetreeSee other common name American Sycamore for verified SG for this same botanical name. | Platanus occidentalis | 0.49 | |
Liquidambar styraciflua | 0.52 | ||
Quercus rubra | 0.63 | ||
Pinus resinosa | 0.46 | ||
Liquidambar styraciflua | 0.52 | ||
American Sycamore | Platanus occidentalis | 0.49 | 1 |
Liriodendron tulipifera | 0.42 | ||
Juglans nigra | 0.55 | ||
American Western PlaneSee other common name American Sycamore for verified SG for this same botanical name. | Platanus occidentalis | 0.49 | |
Betula papyrifera | 0.55 | ||
Liriodendron tulipifera | 0.42 | ||
Pinus strobus | 0.35 | ||
Americkaans MahonieSee other common name True Mahogany for verified SG for this same botanical name. | Swietenia macrophylla | 0.47 | |
Swietenia macrophylla | 0.47 | ||
Amesclao | Tetragastris altissima | 0.74 | |
Amire | Terminalia ivorensis | 0.54 | |
Amongian | Pygeum turnerianum | 0.44 | |
Microberlinia brazzavillensis | 0.77 | ||
Ampas | Koompassia malaccensis | 0.76 | |
Ampira | Terminalia ivorensis | 0.54 | |
Amugan | Pygeum turnerianum | 0.44 | |
Amugis | Koordersiodendron pinnatum | 0.71 | |
Amunu | Podocarpus guatemalensis | 0.54 | |
Amunu | Podocarpus neriifolia | 0.48 | |
Terminalia superba | 0.40 | ||
Anakin | Virola surinamensis | 0.51 | |
Anamenila | Lovoa trichiliodes | 0.46 | |
Anang | Diospyros pyrrhocarpa | 0.69 | 14 |
Anang Gulod | Diospyros inclusa | 0.70 | 14 |
Anangibang | Canangium odoratum | 0.28 | |
Anangilan | Canangium odoratum | 0.28 | |
Anangossiti | Terminalia amazonia | 0.76 | |
Anani | Vochysia guianensis | 0.52 | |
Ananiwana | Hyeronyma laxiflora | 0.58 | |
Anapla | Albizia procera | 0.55 | |
Anatolia | Pterygota bequaertii | 0.53 | |
Anatolia | Pterygota macrocarpa | 0.54 | |
Andaman Gurjun | Dipterocarpus grandiflorus | 0.68 | |
Andaman Padauk | Pterocarpus dalbergioides | 0.65 | 3 |
Pterocarpus indicus | 0.57 | ||
Pterocarpus indicus | 0.57 | ||
Andaman Thingan | Hopea odorata | 0.63 | |
Andinding | Mitragyna ciliata | 0.52 | |
Andiniding | Mitragyna ciliata | 0.52 | |
Andiroba | Carapa guianensis | 0.57 | 2 |
Andjung | Didelotia brevipaniculata | 0.54 | |
Andoc | Irvingia gabonensis | 0.76 | |
Andok | Irvingia gabonensis | 0.76 | |
Andok Oba | Irvingia gabonensis | 0.76 | |
Andoum | Antiaris toxicaria | 0.35 | |
Andoung | Didelotia brevipaniculata | 0.54 | |
Turraeanthus africanus | 0.51 | ||
Anegre | Aningeria altissima | 0.42 | |
Anegre | Aningeria dombeyi | 0.39 | |
Anegre | Aningeria robusta | 0.42 | |
Anesita | Melia azedarach | 0.51 | |
An'fekan | Musanga cecropioides | 0.23 | |
Angale | Poga oleosa | 0.39 | |
Angaria | Phoebe hainesiana | 0.43 | |
Angatuan | Alangium meyeri | 0.56 | |
An-gba | Beilschmiedia mannii | 0.62 | |
An-gbere | Irvingia gabonensis | 0.76 | |
Amburana cearensis | 0.58 | ||
Angelim Rajado | Marmaroxylon racemosum | 1.07 | |
Angelin Rajado | Marmaroxylon racemosum | 1.07 | |
Anglai | Intsia palembanica | 0.65 | |
Ang-Menga-Menga | Staudtia stipitata | 0.79 | |
Angouchi | Terminalia amazonia | 0.76 | |
Pterocarpus indicus | 0.57 | ||
Angsana | Pterocarpus indicus | 0.57 | 3 |
Angu | Dipterocarpus basilanicus | 0.54 | |
Angu | Dipterocarpus warburgii | 0.53 | |
Angu | Pterocarpus marsupium | 0.71 | 4 |
Angu | Pterocarpus vernalis | 0.63 | |
Turraeanthus africanus | 0.51 | ||
Aniba Rosewood | Aniba duckei | 0.56 | |
Anidja | Terminalia ivorensis | 0.54 | |
Aniegre | Aningeria altissima | 0.42 | |
Aniegre | Aningeria dombeyi | 0.39 | |
Aniegre | Aningeria robusta | 0.42 | |
Hymenaea courbaril | 0.83 | ||
Aninapla | Albizia procera | 0.55 | |
Aningeria | Aningeria altissima | 0.42 | |
Aningeria | Aningeria dombeyi | 0.39 | |
Aningeria | Aningeria robusta | 0.42 | |
Aningeria Blanc | Aningeria altissima | 0.42 | |
Aningre | Aningeria altissima | 0.42 | |
Aningre | Aningeria dombeyi | 0.39 | |
Aningre | Aningeria robusta | 0.42 | |
Aningueri Blanc | Aningeria dombeyi | 0.39 | |
Aningueri Blanc | Aningeria robusta | 0.42 | |
Anjalli | Artocarpus hirsuta | 0.52 | |
Anjili | Artocarpus hirsuta | 0.52 | |
Anoano | Vitex cofassus | 0.67 | |
Anoi | Aleurites moluccana | 0.14 | |
Anokye | Guibourtia ehie | 0.71 | 4 |
Millettia laurentii | 0.81 | ||
Anongo | Turpinia ovalifolia | 0.36 | |
Anoniwana | Hieronyma alchorneoides | 0.58 | |
Anono | Xanthophyllum excelsum | 0.67 | |
Ansiopi | Anisoptera costata | 0.52 | |
Antiaris | Antiaris toxicaria | 0.35 | |
Antillen Mahogani | Swietenia mahagoni | 0.57 | |
Antipolo | Artocarpus hirsuta | 0.52 | |
Anubing | Artocarpus ovata | 0.46 | |
Turraeanthus africanus | 0.51 | ||
Anyi | Mansonia altissima | 0.55 | |
Tabebuia serratifolia | 0.99 | ||
Apa | Afzelia bipindensis | 0.62 | |
Apa | Afzelia pachyloba | 0.62 | |
Apa | Afzelia quanzensis | 0.62 | |
Turraeanthus africanus | 0.51 | ||
Turraeanthus africanus | 0.51 | ||
Turraeanthus africanus | 0.51 | ||
Apegya | Mammea africana | 0.69 | |
Turraeanthus africanus | 0.51 | ||
Api | Diplodiscus paniculatus | 0.62 | |
Apia | Morus mesozygia | 0.71 | |
Apitan | Pygeum turnerianum | 0.44 | |
Apitong | Dipterocarpus basilanicus | 0.54 | |
Apitong | Dipterocarpus grandiflorus | 0.68 | |
Apitong | Dipterocarpus warburgii | 0.53 | |
Apixuna | Micropholis guianensis | 0.67 | |
Shorea negrosensis | 0.59 | ||
Apopo | Lovoa trichiliodes | 0.46 | |
Turraeanthus africanus | 0.51 | ||
Apple | Malus pumila | 0.64 | |
Aprend | Mansonia altissima | 0.55 | |
Apricot | Mammea americana | 0.74 | |
Aprono | Mansonia altissima | 0.55 | |
Aptakas | Calophyllum inophyllum | 0.55 | |
Aquacatillo | Hieronyma alchorneoides | 0.58 | |
Aquacatillo | Hyeronyma laxiflora | 0.58 | |
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Tabebuia serratifolia | 0.99 | ||
Araca | Terminalia amazonia | 0.76 | |
Aracan | Aspidosperma desmanthum | 0.65 | |
Araciuba | Minquartia guianensis | 0.83 | |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Aralta | Minquartia guianensis | 0.83 | |
Arangen | Aglaia gigantea | 0.54 | |
Pterocarpus soyauxii | 0.64 | ||
Swietenia macrophylla | 0.47 | ||
Araracanga | Aspidosperma desmanthum | 0.65 | |
Ararauba | Aspidosperma desmanthum | 0.65 | |
Triplochiton scleroxylon | 0.32 | ||
Arariba | Sickingia salvadorense | 0.65 | |
Araruet | Pygeum africanum | 0.61 | |
Arata Minquar | Minquartia guianensis | 0.83 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.80 | ||
Hymenaea courbaril | 0.83 | ||
Aratta | Minquartia guianensis | 0.83 | |
Araucaria angustifolia | 0.49 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Arbe a Buerre | Caryocar villosum | 0.76 | |
Arbol de Indias | Aleurites moluccana | 0.14 | |
Arbol de Paternoster | Melia azedarach | 0.51 | |
Arbol del Ajo | Cordia alliodora | 0.51 | |
Hura crepitans | 0.40 | ||
Thuja occidentalis | 0.31 | ||
Thuja occidentalis | 0.31 | ||
Thuja plicata | 0.32 | ||
Hura crepitans | 0.40 | ||
Arbre de Paternoster | Melia azedarach | 0.51 | |
Arbutus menziesii | 0.64 | ||
Pinus sylvestris | 0.45 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Hura crepitans | 0.40 | ||
Hura crepitans | 0.40 | ||
Arenillo | Catostemma fragrans | 0.66 | |
Triplochiton scleroxylon | 0.32 | ||
Hura crepitans | 0.40 | ||
Aricurana | Hieronyma alchorneoides | 0.58 | |
Quercus alba | 0.68 | ||
Picea engelmannii | 0.35 | ||
Quercus alba | 0.68 | ||
Arjun | Terminalia arjuna | 0.71 | |
Arkansas Oak | Quercus arkansana | 0.53 | |
Arkansas Water Oak | Quercus arkansana | 0.53 | |
Armaniuri | Anisoptera costata | 0.52 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.80 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.80 | ||
Aromilla | Terminalia amazonica | 0.76 | |
Aroo | Casuarina equisetifolia | 0.87 | |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Arrida | Campnosperma brevipetiolata | 0.33 | |
Aru | Casuarina equisetifolia | 0.87 | |
Tabebuia serratifolia | 0.99 | ||
Shorea negrosensis | 0.59 | ||
Arupag | Aglaia gigantea | 0.54 | |
Hymenaea courbaril | 0.83 | ||
Asaka | Tieghemella heckelii | 0.60 | |
Asam | Mangifera altissima | 0.52 | |
Asam | Mangifera indica | 0.53 | |
Pometia pinnata | 0.60 | ||
Asamfona | Aningeria altissima | 0.42 | |
Asan | Populus ciliata | 0.37 | |
Asang Bitum | Vitex cofassus | 0.67 | |
Asapoko | Pouteria izabalensis | 0.64 | |
Asas | Bridelia aubrevillei | 0.59 | |
Fraxinus americana | 0.60 | ||
Ash | Fraxinus excelsior | 0.58 | 14 |
Fraxinus nigra | 0.49 | ||
Fraxinus pennsylvanica | 0.56 | ||
Ashleaf Maple | Acer negundo | 0.45 | 2 |
Hura crepitans | 0.40 | ||
Asomba | Anisoptera costata | 0.52 | |
Asore | Lophira alata | 0.94 | |
Populus tremuloides | 0.38 | ||
Populus tremuloides | 0.38 | ||
Hura crepitans | 0.40 | ||
Turraeanthus africanus | 0.51 | ||
Buxus sempervirens | 0.83 | ||
Assan | Musanga cecropioides | 0.23 | |
Assang | Musanga cecropioides | 0.23 | |
Assas | Bridelia aubrevillei | 0.59 | |
Asseng | Musanga cecropioides | 0.23 | |
Assia | Dacryodes le testui | 0.56 | |
Hymenaea courbaril | 0.83 | ||
Ata ata | Diospyros mindanaensis | 0.78 | 14 |
Pometia pinnata | 0.60 | ||
Atchiupon | Mitragyna ciliata | 0.52 | |
Ateje | Cordia collococea | 0.50 | |
Atereba | Eschweilera sagotiana | 0.90 | |
Atha | Mesua ferrea | 0.92 | |
Atiokouo | Beilschmiedia mannii | 0.62 | |
Atiokwo | Beilschmiedia mannii | 0.62 | |
Atlantic White Cedar | Chamaecyparis thyoides | 0.32 | 1 |
Cedrela odorata | 0.39 | ||
Attaka | Mitragyna parvifolia | 0.59 | |
Atui | Piptadeniastrum africanum | 0.63 | |
Atzapolquahuitl | Pouteria pomifera | 0.84 | |
Atzapotl | Pouteria izabalensis | 0.64 | |
Aulne Noir | Alnus glutinosa | 0.41 | |
Aune | Alnus glutinosa | 0.41 | |
Aune Commune | Alnus glutinosa | 0.41 | |
Aupar Kwipari | Loxopterygium sagotii | 0.62 | |
Aus | Manilkara bidentata | 0.95 | |
Ausabo | Manilkara bidentata | 0.95 | |
Araucaria cunninghamii | 0.44 | ||
Australian Beefwood | Casuarina equisetifolia | 0.87 | |
Australian Black Acacia | Acacia melanoxylon | 0.54 | |
Australian Blackwood | Acacia melanoxylon | 0.54 | |
Australian Cedar | Cedrela toona | 0.47 | |
Callitris glauca | 0.59 | ||
Australian Grey Bastard Box | Eucalyptus hemiphloia | 0.93 | |
Australian Maple | Flindersia pimenteliana | 0.51 | |
Australian Maple | Flindersia pubescens | 0.60 | |
Eucalyptus obliqua | 0.68 | ||
Australian Pine | Casuarina equisetifolia | 0.87 | |
Australian Red Cedar | Cedrela toona | 0.47 | |
Australian Red-Cedar | Cedrela toona | 0.47 | |
Australian silky oak | Grevillea robusta | 0.54 | |
Australian Silky-Oak | Grevillea robusta | 0.54 | |
Austrian Oak | Quercus petraea | 0.65 | |
Quercus robur | 0.57 | ||
Pinus strobus | 0.35 | ||
Ausubo | Manilkara bidentata | 0.95 | |
Ausus | Excoecaria agallocha | 0.42 | |
Hymenaea courbaril | 0.83 | ||
Avellano | Aleurites moluccana | 0.14 | |
Avenbok | Carpinus betulus | 0.61 | |
Avewotse | Morus mesozygia | 0.71 | |
Avispillo | Phoebe elongata | 0.62 | |
Turraeanthus africanus | 0.51 | ||
Avodire | Turraeanthus africanus | 0.51 | 2 |
Avoga | Poga oleosa | 0.39 | |
Millettia stuhlmannii | 0.83 | ||
Pometia pinnata | 0.60 | ||
Pometia pinnata | 0.60 | ||
Awari | Pterygota bequaertii | 0.53 | |
Awari | Pterygota macrocarpa | 0.54 | |
Awenshin | Terminalia ivorensis | 0.54 | |
Millettia laurentii | 0.81 | ||
Awoung | Millettia laurentii | 0.81 | 14 |
Axlewood | Anogeissus latifolia | 0.66 | |
Ayas | Excoecaria agallocha | 0.42 | |
Aye | Morus mesozygia | 0.71 | |
Ayni | Artocarpus hirsuta | 0.52 | |
Triplochiton scleroxylon | 0.32 | ||
Triplochiton scleroxylon | 0.32 | ||
Triplochiton scleroxylon | 0.32 | ||
Azobe | Lophira alata | 0.94 | |
Hymenaea courbaril | 0.83 | ||
Azucarero | Tetragastris altissima | 0.74 | |
Azucarito blanco | Tetragastris altissima | 0.74 | |
Azza | Afzelia bipindensis | 0.62 | |
Azza | Afzelia pachyloba | 0.62 | |
Azza | Afzelia quanzensis | 0.62 | |
A | B | C | D | E | F | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z | |||
Common Name | Botanical Name | Specific Gravity | Verified |
Ba | Mitragyna stipulosa | 0.53 | |
Pterocarpus soyauxii | 0.64 | ||
Shorea negrosensis | 0.59 | ||
Baboen | Virola koschnyi | 0.51 | |
Baboen | Virola surinamensis | 0.51 | |
Baboenhout | Virola surinamensis | 0.51 | |
Baboenoedoe | Virola surinamensis | 0.51 | |
Baboon | Virola surinamensis | 0.51 | |
Baboonhout | Virola surinamensis | 0.51 | |
Baboonwood | Virola surinamensis | 0.51 | |
Babou | Tieghemella heckelii | 0.6 | |
Babu | Tieghemella heckelii | 0.6 | |
Babun | Virola koschnyi | 0.51 | |
Babun | Virola surinamensis | 0.51 | |
Badam | Terminalia procera | 0.54 | |
Triplochiton scleroxylon | 0.32 | ||
Bafn ooi | Intsia bijuga | 0.65 | |
Bagac | Dipterocarpus grandiflorus | 0.68 | |
Bagarilao | Xanthophyllum excelsum | 0.67 | |
Bagaulan | Xanthophyllum excelsum | 0.67 | |
Bagnu | Populus ciliata | 0.37 | |
Bagobo | Diplodiscus paniculatus | 0.62 | |
Bagosantol | Sandoricum vidalii | 0.65 | |
Shorea negrosensis | 0.59 | ||
Bagunarem | Lagerstroemia piriformis | 0.67 | |
Bagunaum | Lagerstroemia piriformis | 0.67 | |
Bagwain | Tieghemella heckelii | 0.6 | |
Bagyi | Terminalia ivorensis | 0.54 | |
Bahi | Terminalia ivorensis | 0.54 | |
Bahia | Mitragyna ciliata | 0.52 | |
Bahia | Mitragyna stipulosa | 0.53 | |
Bai | Terminalia ivorensis | 0.54 | |
Bai-ah | Vitex cofassus | 0.67 | |
Bai-ti | Terminalia ivorensis | 0.54 | |
Pometia pinnata | 0.6 | ||
Baji | Terminalia ivorensis | 0.54 | |
Bajii | Terminalia ivorensis | 0.54 | |
Bak | Anisoptera costata | 0.52 | |
Bakain | Melia azedarach | 0.51 | |
Bakalau | Aglaia gigantea | 0.54 | |
Bakana | Chlorophora excelsa | 0.7 | |
Bakayan | Melia azedarach | 0.51 | |
Bakia | Mitragyna ciliata | 0.52 | |
Bako | Tieghemella heckelii | 0.6 | |
Baku | Mimusops heckelii | 0.55 | |
Baku | Tieghemella heckelii | 0.6 | |
Bakundu | Lophira alata | 0.94 | |
Shorea negrosensis | 0.59 | ||
Balata | Manilkara bidentata | 0.95 | |
Balata burue | Manilkara bidentata | 0.95 | |
Balata franc | Manilkara bidentata | 0.95 | |
Balata gomme | Manilkara bidentata | 0.95 | |
Balata rouge | Manilkara bidentata | 0.95 | |
Balau | Anisoptera curtisii | 0.52 | |
Balau | Shorea guiso | 0.75 | |
Balau | Shorea plagata | 0.75 | |
Balau merah | Shorea guiso | 0.75 | |
Balau merah | Shorea plagata | 0.75 | |
Taxodium distichum | 0.46 | ||
Baldcypress | Taxodium distichum | 0.46 | 1 |
Diospyros ebenum | 0.94 | ||
Terminalia superba | 0.4 | ||
Balek angin | Alphitonia philippinensis | 0.35 | |
Balia | Heritiera javanica | 0.65 | |
Baligan | Anisoptera costata | 0.52 | |
Populus balsamifera | 0.34 | ||
Populus trichocarpa | 0.35 | ||
Populus balsamifera | 0.34 | ||
Balobo | Diplodiscus paniculatus | 0.62 | |
Balobo | Xanthophyllum excelsum | 0.67 | |
Balogo | Diplodiscus paniculatus | 0.62 | |
Pometia pinnata | 0.6 | ||
Balsa | Ochroma pyramidale syn. O. lagopus | 0.14 | 4 |
Balsa | Ochroma pyramidale | 0.14 | 4 |
Abies amabilis | 0.43 | ||
Abies balsamea | 0.35 | ||
Abies lasiocarpa | 0.32 | ||
Picea engelmannii | 0.35 | ||
Balsam cottonwood | Populus balsamifera | 0.34 | 1 |
Abies amabilis | 0.43 | ||
Balsam fir | Abies balsamea | 0.35 | 1 |
Abies lasiocarpa | 0.32 | ||
Balsamo | Myroxylon balsamum | 0.83 | 4 |
Balsamo | Protium decandrum | 0.54 | 4 |
Balsamo | Protium paraense | 0.56 | 4 |
Balsamo | Protium sagotianum | 0.56 | 4 |
Balsamo de Cayeput | Melaleuca leucadendron syn. M. quinquenervia | 0.72 | 4 |
Populus balsamifera | 0.34 | ||
Picea rubens | 0.4 | ||
Liquidambar styraciflua | 0.52 | ||
Liquidambar styraciflua | 0.52 | ||
Pinus sylvestris | 0.45 | ||
Pinus sylvestris | 0.45 | ||
Baltic redwood | Pinus sylvestris | 0.45 | 14 |
Baltic white pine | Picea abies | 0.43 | |
Baltic whitewood | Picea abies | 0.43 | |
Balugo | Diplodiscus paniculatus | 0.62 | |
Balugug | Diplodiscus paniculatus | 0.62 | |
Balui | Aglaia gigantea | 0.54 | |
Baluknit | Lagerstroemia piriformis | 0.67 | |
Balung ayam | Heritiera javanica | 0.65 | |
Balungai | Diplodiscus paniculatus | 0.62 | |
Triplochiton scleroxylon | 0.32 | ||
Ban pipal | Populus ciliata | 0.37 | |
Banabang-bugtung | Lagerstroemia piriformis | 0.67 | |
Banabang-dinglas | Lagerstroemia piriformis | 0.67 | |
Banabang-tinaan | Lagerstroemia piriformis | 0.67 | |
Banafat | Vitex cofassus | 0.67 | |
Banak | Iryanthera spp. | 0.58 | |
Banak | Virola koschnyi | 0.51 | |
Banak | Virola spp. | 0.45 | 2 |
Banak | Virola surinamensis | 0.51 | |
Bancolier | Aleurites moluccana | 0.14 | |
Bancoulier | Aleurites moluccana | 0.14 | |
Banderhola | Duabanga sonneratioides | 0.37 | |
Bang | Chlorophora excelsa | 0.7 | |
Bang nuoc | Terminalia procera | 0.54 | |
Shorea negrosensis | 0.59 | ||
Banghi | Chlorophora excelsa | 0.7 | |
Bangikat poplar | Populus ciliata | 0.37 | |
Bangkahasi | Koordersiodendron pinnatum | 0.71 | |
Bangkalari | Koordersiodendron pinnatum | 0.71 | |
Pometia pinnata | 0.6 | ||
Bangluai | Pygeum turnerianum | 0.44 | |
Banidi | Terminalia ivorensis | 0.54 | |
Banig | Xanthophyllum excelsum | 0.67 | |
Bankalis | Tetramerista glabra | 0.73 | |
Khaya nyassica | 0.44 | ||
Bankile | Lophira alata | 0.94 | |
Pinus banksiana | 0.43 | ||
Pinus banksiana | 0.43 | ||
Bankulnussbaum | Aleurites moluccana | 0.14 | |
Banohoera | Vitex cofassus | 0.67 | |
Banzu | Piptadeniastrum africanum | 0.63 | |
Baoti | Anisoptera costata | 0.52 | |
Diospyros virginiana | 0.71 | ||
Barabu | Peltogyne porphyrocardia | 0.69 | |
Barabu | Peltogyne venosa | 0.69 | |
Barakbak | Xanthophyllum excelsum | 0.67 | |
Baramalli | Catostemma fragrans | 0.66 | |
Baraman | Catostemma fragrans | 0.66 | |
Baramanni | Catostemma fragrans | 0.66 | |
Barata | Pouteria izabalensis | 0.64 | |
Barauna | Schinopsis spp. | 1.21 | |
Barbachele | Vochysia ferruginea | 0.52 | |
Barbachele | Vochysia guianensis | 0.52 | |
Barba-chole | Vochysia guianensis | 0.52 | |
Barbara chele | Vochysia ferruginea | 0.52 | |
Barbara chele | Vochysia guianensis | 0.52 | |
Barbara chele | Vochysia lehmanni | 0.52 | |
Barbara Chele | Vochysia tomentosa | 0.52 | |
Barbo | Diplodiscus paniculatus | 0.62 | |
Barilla de agua | Micropholis guianensis | 0.67 | |
Baripung | Anisoptera costata | 0.52 | |
Barka locust | Byrsonima coriacea | 0.68 | |
Barka-locust | Byrsonima coriacea | 0.68 | |
Barobo | Diplodiscus paniculatus | 0.62 | |
Barolo | Diplodiscus paniculatus | 0.62 | |
Baromalli | Catostemma fragrans | 0.66 | |
Baroto | Diplodiscus paniculatus | 0.62 | |
Pterocarpus soyauxii | 0.64 | ||
Baru | Dipteryx odorata | 0.82 | |
Baruba | Diplodiscus paniculatus | 0.62 | |
Barubu | Diplodiscus paniculatus | 0.62 | |
Barujo | Dipteryx odorata | 0.82 | |
Pterocarpus soyauxii | 0.64 | ||
Pometia pinnata | 0.6 | ||
Basilan | Dipterocarpus basilanicus | 0.54 | |
Basilan apitong | Dipterocarpus basilanicus | 0.54 | |
Basinau | Aglaia gigantea | 0.54 | |
Basio | Terminalia ivorensis | 0.54 | |
Basit | Lagerstroemia piriformis | 0.67 | |
Fraxinus nigra | 0.49 | ||
Basket elm | Ulmus crassifolia | 0.62 | |
Basobo | Diplodiscus paniculatus | 0.62 | |
Basoeng | Anisoptera cochinchinensis | 0.52 | |
Pinus taeda | 0.51 | ||
Bassi | Terminalia ivorensis | 0.54 | |
Tilia americana | 0.37 | ||
Libocedrus decurrens | 0.37 | ||
Bastard cedar | Virola koschnyi | 0.51 | |
Celtis occidentalis | 0.53 | ||
Bastard lignum vitae | Tabebuia serratifolia | 0.99 | 4 |
Swietenia macrophylla | 0.47 | ||
Bastard mahogany | Mammea africana | 0.69 | |
Bastard pine | Pinus caribaea | 0.7 | |
Bastermopane | Guibourtia coleosperma | 0.66 | |
Bat | Excoecaria agallocha | 0.42 | |
Magnolia grandiflora | 0.5 | ||
Bat«Nigak«iy | Excoecaria agallocha | 0.42 | |
Bata kadapu | Mitragyna parvifolia | 0.59 | |
Bataan | Shorea negrosensis | 0.59 | 4 |
Batabanapu | Mitragyna parvifolia | 0.59 | |
Bataganapu | Mitragyna parvifolia | 0.59 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Hymenaea courbaril | 0.83 | ||
Batik | Erythrophloeum densiflorum | 0.68 | |
Batikalag | Lagerstroemia piriformis | 0.67 | |
Batitinan | Lagerstroemia piriformis | 0.67 | |
Batobato | Xanthophyllum excelsum | 0.67 | |
Batobatong-babae | Xanthophyllum excelsum | 0.67 | |
Triplochiton scleroxylon | 0.32 | ||
Bats souari | Caryocar villosum | 0.76 | |
Batukanag | Aglaia gigantea | 0.54 | |
Bauaobo | Diplodiscus paniculatus | 0.62 | |
Baule | Mansonia altissima | 0.55 | |
Baurai | Anisoptera costata | 0.52 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Umbellularia californica | 0.55 | ||
Bay mahogany | Swietenia mahagoni | 0.57 | |
Nyssa aquatica | 0.5 | ||
Baya | Mitragyna ciliata | 0.52 | |
Baya | Mitragyna stipulosa | 0.53 | |
Terminalia superba | 0.4 | ||
Shorea negrosensis | 0.59 | ||
Baye | Terminalia ivorensis | 0.54 | |
Bay laurel | Umbellularia californica | 0.55 | 3 |
Swietenia macrophylla | 0.47 | ||
Pometia pinnata | 0.6 | ||
Bayott | Anisoptera curtisii | 0.52 | |
Pometia pinnata | 0.6 | ||
Pometia pinnata | 0.6 | ||
Swietenia macrophylla | 0.47 | ||
Beach calophyllum | Calophyllum inophyllum | 0.55 | |
Beach she oak | Casuarina equisetifolia | 0.87 | |
Bead tree | Melia azedarach | 0.51 | |
Beadtree | Melia azedarach | 0.51 | |
Beauty leaf | Calophyllum inophyllum | 0.55 | |
Beay | Beilschmiedia mannii | 0.62 | |
Be-ay | Beilschmiedia mannii | 0.62 | |
Bebe | Dipterocarpus basilanicus | 0.54 | |
Bebe | Dipterocarpus grandiflorus | 0.68 | |
Bebe | Dipterocarpus warburgii | 0.53 | |
Bebe | Pterocarpus marsupium | 0.71 | 4 |
Bebe | Pterocarpus vernalis | 0.63 | |
Bebuta | Excoecaria agallocha | 0.42 | |
Becuiba | Virola surinamensis | 0.51 | |
Tilia americana | 0.37 | ||
Fagus grandifolia | 0.64 | ||
Beefwood | Casuarina equisetifolia | 0.87 | |
Beefwood | Manilkara bidentata | 0.95 | |
Tilia americana | 0.37 | ||
Tilia americana | 0.37 | ||
Behetta champagam | Mesua ferrea | 0.92 | |
Behra | Chloroxylon swietenia | 0.88 | |
Behru | Chloroxylon swietenia | 0.88 | |
Be-ie | Terminalia ivorensis | 0.54 | |
Beiya | Mitragyna stipulosa | 0.53 | |
Belandi | Cedrela toona | 0.47 | |
Belarbre | Mora excelsa | 0.89 | |
Bel-bel | Pinus insularis | 0.5 | |
Belengbe | Lophira alata | 0.94 | |
Belgaum walnut | Aleurites moluccana | 0.14 | |
Fraxinus excelsior | 0.58 | ||
Belian | Madhuca sp. | 0.97 | |
Belile | Melia azedarach | 0.51 | |
Swietenia macrophylla | 0.47 | ||
Bella | Chloroxylon swietenia | 0.88 | |
Bella maria | Vochysia lehmanni | 0.52 | |
Bella Maria | Vochysia tomentosa | 0.52 | |
Bella rosa | Anisoptera curtisii | 0.52 | |
Belle-tu | Irvingia gabonensis | 0.76 | |
Bemoonba | Iryanthera spp. | 0.58 | |
Benchaloi | Anisoptera curtisii | 0.52 | |
Bendora | Intsia bijuga | 0.65 | |
Bengaris | Koompassia malaccensis | 0.76 | |
Benge | Guibourtia arnoldiana | 0.70 | 2 |
Benguet pine | Pinus insularis | 0.5 | |
Benin walnut | Lovoa trichiliodes | 0.46 | |
Benquet pine | Pinus insularis | 0.5 | |
Berangan | Castanopsis acuminatissima | 0.56 | |
Berau | Aleurites moluccana | 0.14 | |
Bere | Melia azedarach | 0.51 | |
Berembang bukit | Duabanga sonneratioides | 0.37 | |
Berg Gronfoeloe | Qualea paraensis | 0.58 | |
Bergek | Quercus petraea | 0.65 | |
Berlinia | Berlinia acuminata | 0.64 | |
Berniung | Koompassia malaccensis | 0.76 | |
Berua | Anisoptera costata | 0.52 | |
Beruni | Artocarpus hirsuta | 0.52 | |
Terminalia superba | 0.4 | ||
Beso | Vitex cofassus | 0.67 | |
Bete | Mansonia altissima | 0.55 | |
Bethabara | Tabebuia serratifolia | 0.99 | 4 |
Betis | Madhuca sp. | 0.97 | |
Betula alleghaniensis | 0.62 | ||
Beukenhout | Rapanea melanophleos | 0.74 | |
Bevu | Melia azedarach | 0.51 | |
Beya | Mitragyna ciliata | 0.52 | |
Beya | Mitragyna stipulosa | 0.53 | |
Beyo | Afzelia bipindensis | 0.62 | |
Beyo | Afzelia pachyloba | 0.62 | |
Beyo | Afzelia quanzensis | 0.62 | |
Bharhul | Chloroxylon swietenia | 0.88 | |
Bhera | Chloroxylon swietenia | 0.88 | |
Bhiraa | Chloroxylon swietenia | 0.88 | |
Bhirwa | Chloroxylon swietenia | 0.88 | |
Bibolo | Lovoa trichiliodes | 0.46 | |
Bicuhyba | Virola surinamensis | 0.51 | |
Bicui | Iryanthera spp. | 0.58 | |
Bicuiba | Virola koschnyi | 0.51 | |
Bidi-tu | Beilschmiedia mannii | 0.62 | |
Pometia pinnata | 0.6 | ||
Bi-eh | Piptadeniastrum africanum | 0.63 | |
Magnolia grandiflora | 0.5 | ||
Swietenia macrophylla | 0.47 | ||
Pinus lambertiana | 0.36 | ||
Pinus ponderosa | 0.4 | ||
Carya lacinosa | 0.69 | ||
Swietenia macrophylla | 0.47 | ||
Bigleaf maple | Acer macrophyllum | 0.48 | 1 |
Swietenia macrophylla | 0.47 | ||
Bigtooth aspen | Populus grandidentata | 0.39 | 1 |
Bihiri | Chloroxylon swietenia | 0.88 | |
Bijasal | Pterocarpus marsupium | 0.71 | 4 |
Bijol-goch | Grewia elastica | 0.63 | |
Bilgu | Chloroxylon swietenia | 0.88 | |
Bili devdari | Dysoxylum malabaricum | 0.62 | |
Bilinga | Afzelia quanzensis | 0.62 | |
Billu | Chloroxylon swietenia | 0.88 | |
Liquidambar styraciflua | 0.52 | ||
Liquidambar styraciflua | 0.52 | ||
Fraxinus americana | 0.6 | ||
Fraxinus americana | 0.6 | ||
Bimla | Grewia elastica | 0.63 | |
Shorea negrosensis | 0.59 | ||
Bindang | Agathis borneensis | 0.41 | |
Bindang | Agathis philippinensis | 0.33 | |
Bintangor | Calophyllum inophyllum | 0.55 | |
Bintangor | Calophyllum tomentosum | 0.59 | |
Bios de fer | Pygeum africanum | 0.61 | |
Pometia pinnata | 0.6 | ||
Biot | Sandoricum vidalii | 0.65 | |
Biotu | Calophyllum inophyllum | 0.55 | |
Betula alleghaniensis | 0.62 | ||
Betula lenta | 0.65 | ||
Betula papyrifera | 0.55 | ||
Birch | Betula sp. | 0.61 | |
Acer saccharum | 0.63 | ||
Pinus ponderosa | 0.4 | ||
Bitan | Melia azedarach | 0.51 | |
Bitanghol | Calophyllum inophyllum | 0.55 | |
Bitanghol | Calophyllum tomentosum | 0.59 | |
Bitaog | Calophyllum inophyllum | 0.55 | |
Bitaog | Calophyllum tomentosum | 0.59 | |
Bitehe | Beilschmiedia mannii | 0.62 | |
Bitehi | Beilschmiedia mannii | 0.62 | |
Biti | Vitex cofassus | 0.67 | |
Bitis | Madhuca sp. | 0.97 | |
Bitter Almond | Pygeum africanum | 0.61 | |
Bitter amandel | Pygeum africanum | 0.61 | |
Carya aquatica | 0.62 | ||
Carya illinoensis | 0.66 | ||
Carya aquatica | 0.62 | ||
Carya cordiformis | 0.66 | ||
Bitternut hickory | Carya cordiformis | 0.66 | 1 |
Bitum | Vitex cofassus | 0.67 | |
Bitum | Vitex parviflora | 0.68 | |
Biyuch | Calophyllum inophyllum | 0.55 | |
Biyuuch | Calophyllum inophyllum | 0.55 | |
Bjimbo | Mammea africana | 0.69 | |
Black afara | Terminalia ivorensis | 0.54 | |
Black alder | Alnus glutinosa | 0.41 | |
Fraxinus americana | 0.6 | ||
Black ash | Fraxinus nigra | 0.49 | 1 |
Black bark | Terminalia ivorensis | 0.54 | |
Betula alleghaniensis | 0.62 | ||
Betula lenta | 0.65 | ||
Betula papyrifera | 0.55 | ||
Black bully | Manilkara zapota | 0.71 | |
Black cherry | Prunus serotina | 0.50 | 1 |
Black cottonwood | Populus trichocarpa | 0.35 | 1 |
Taxodium distichum | 0.46 | ||
Albizia lebbeck | 0.54 | ||
Diospyros ebenum | 0.94 | ||
Nyssa aquatica | 0.5 | ||
Nyssa sylvatica | 0.5 | ||
Pinus ponderosa | 0.4 | ||
Black Kakaralli | Eschweilera sagotiana | 0.9 | |
Black kakeralli | Eschweilera sagotiana | 0.9 | |
Magnolia grandiflora | 0.5 | ||
Black locust | Robinia pseudoacacia | 0.69 | 1 |
Black manwood | Minquartia guianensis | 0.83 | |
Black maple | Acer nigrum | 0.57 | 1 |
Acer saccharum | 0.63 | ||
Black mora | Mora excelsa | 0.89 | |
Quercus coccinea | 0.67 | ||
Quercus kelloggii | 0.53 | ||
Quercus rubra | 0.63 | ||
Black Oak | Quercus velutina | 0.61 | 1 |
Pinus banksiana | 0.43 | ||
Pinus contorta | 0.41 | ||
Pinus ponderosa | 0.4 | ||
Black pine | Podocarpus neriifolia | 0.48 | |
Black sally | Acacia melanoxylon | 0.54 | |
Black spruce | Picea mariana | 0.42 | 1 |
Picea sitchensis | 0.4 | ||
Acer nigrum | 0.57 | ||
Black tupelo | Nyssa sylvatica | 0.50 | 1 |
Black varnish tree | Melanorrhoea spp. | 0.75 | |
Black walnut | Juglans nigra | 0.55 | 1 |
Black wattle | Acacia melanoxylon | 0.54 | |
Black willow | Salix alba | 0.38 | |
Black willow | Salix nigra | 0.39 | 1 |
Black-barked terminalia | Terminalia ivorensis | 0.54 | |
Pinus ponderosa | 0.4 | ||
Blackwood | Acacia melanoxylon | 0.54 | |
Bletui | Mammea africana | 0.69 | |
Bletune | Mammea africana | 0.69 | |
Blie | Terminalia ivorensis | 0.54 | |
Terminalia superba | 0.4 | ||
Turraeanthus africanus | 0.51 | ||
Turraeanthus africanus | 0.51 | ||
Liquidambar styraciflua | 0.52 | ||
Liquidambar styraciflua | 0.52 | ||
Abies balsamea | 0.35 | ||
Acer saccharum | 0.63 | ||
Bloodwood | Brosimum rubescens | 0.96 | 16 |
Bloodwood | Pterocarpus angolensis | 0.59 | 14 |
Fraxinus pennsylvanica | 0.56 | ||
Blue ash | Fraxinus quadrangulata | 0.58 | 1 |
Blue beech | Carpinus caroliniana | 0.64 | |
Pseudotsuga menziesii | 0.48 | ||
Blue gum | Eucalyptus tereticornis | 0.82 | |
Quercus macrocarpa | 0.64 | ||
Liriodendron tulipifera | 0.42 | ||
Blue spruce | Picea glauca | 0.36 | 3 |
Bo | Mitragyna stipulosa | 0.53 | |
Pterocarpus soyauxii | 0.64 | ||
Diospyros virginiana | 0.71 | ||
Bobang | Chlorophora excelsa | 0.7 | |
Bobbie manja | Mangifera indica | 0.53 | |
Bobich | Cedrela toona | 0.47 | |
Bobo | Irvingia gabonensis | 0.76 | |
Boboi | Irvingia gabonensis | 0.76 | |
Boborae | Irvingia gabonensis | 0.76 | |
Boborau | Irvingia gabonensis | 0.76 | |
Boborou | Irvingia gabonensis | 0.76 | |
Boboru | Irvingia gabonensis | 0.76 | |
Bocachico | Piptadeniastrum africanum | 0.63 | |
Bocapi | Staudtia stipitata | 0.79 | |
Bodare | Maclura pomifera | 0.72 | |
Bodark | Maclura pomifera | 0.72 | |
Bodo | Mitragyna ciliata | 0.52 | |
Bodock | Maclura pomifera | 0.72 | |
Bodua | Mansonia altissima | 0.55 | |
Boei | Mitragyna stipulosa | 0.53 | |
Boeji mahonie | Loxopterygium sagotii | 0.62 | |
Boepasa | Vitex cofassus | 0.67 | |
Boesi mahonie | Loxopterygium sagotii | 0.62 | |
Boeti | Manilkara bidentata | 0.95 | |
Boewah kareh | Aleurites moluccana | 0.14 | |
Picea mariana | 0.42 | ||
Bogamani | Virola surinamensis | 0.51 | |
Bogo | Beilschmiedia mannii | 0.62 | |
Boh | Mitragyna stipulosa | 0.53 | |
Bohun | Cordia alliodora | 0.51 | |
Boilam | Swintonia sp. | 0.62 | |
Bois agouti | Minquartia guianensis | 0.83 | |
Buxus sempervirens | 0.83 | ||
Pterocarpus soyauxii | 0.64 | ||
Bois corne | Byrsonima coriacea | 0.68 | |
Bois cruseau | Vochysia guianensis | 0.52 | |
Bois d'amande | Hieronyma alchorneoides | 0.58 | |
Bois d'arc | Maclura pomifera | 0.72 | |
Bois de coumarouna | Dipteryx odorata | 0.82 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Bois de fer | Casuarina equisetifolia | 0.87 | |
Bois de Rhodes | Cordia alliodora | 0.51 | |
Bois de rose | Aniba duckei | 0.56 | |
Dalbergia frutescens | 1.02 | ||
Pterocarpus soyauxii | 0.64 | ||
Hymenaea courbaril | 0.83 | ||
Bois de vin | Hieronyma alchorneoides | 0.58 | |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Hura crepitans | 0.4 | ||
Bois macaque | Marmaroxylon racemosum | 1.07 | |
Bois pourpre | Peltogyne venosa | 0.69 | |
Bois puurpre | Peltogyne porphyrocardia | 0.69 | |
Bois rouge | Melia azedarach | 0.51 | |
Pterocarpus soyauxii | 0.64 | ||
Bois serpent | Marmaroxylon racemosum | 1.07 | |
Bois soumis | Cordia alliodora | 0.51 | |
Bois tan | Byrsonima coriacea | 0.68 | |
Pterocarpus soyauxii | 0.64 | ||
Bois violet | Peltogyne porphyrocardia | 0.69 | |
Bois voilet | Peltogyne venosa | 0.69 | |
Bois zebra | Marmaroxylon racemosum | 1.07 | |
Bojep | Irvingia gabonensis | 0.76 | |
Bojon | Cordia alliodora | 0.51 | |
Bok bok | Xanthophyllum excelsum | 0.67 | |
Bokapi | Staudtia stipitata | 0.79 | |
Bokenyama | Morus mesozygia | 0.71 | |
Pterocarpus soyauxii | 0.64 | ||
Bokoka | Lophira alata | 0.94 | |
Bokoli | Mammea africana | 0.69 | |
Bokombo | Musanga cecropioides | 0.23 | |
Terminalia superba | 0.4 | ||
Bokonge | Millettia laurentii | 0.81 | 14 |
Pterocarpus soyauxii | 0.64 | ||
Bokuibe | Musanga cecropioides | 0.23 | |
Bokundu | Piptadeniastrum africanum | 0.63 | |
Bokungo | Piptadeniastrum africanum | 0.63 | |
Bokungu | Piptadeniastrum africanum | 0.63 | |
Bolador | Terminalia amazonia | 0.76 | |
Bolato | Diplodiscus paniculatus | 0.62 | |
Bolengo | Afzelia bipindensis | 0.62 | |
Bolengo | Afzelia pachyloba | 0.62 | |
Boliki | Mammea africana | 0.69 | |
Bolletri | Manilkara bidentata | 0.95 | |
Bolletrie | Manilkara bidentata | 0.95 | |
Bolo | Diplodiscus paniculatus | 0.62 | |
Pometia pinnata | 0.6 | ||
Bomanga | Brachystegia laurentii | 0.57 | |
Bombax | Bombax chevalieri | 0.51 | |
Bombay white cedar | Dysoxylum malabaricum | 0.62 | |
Bombulu | Lovoa trichiliodes | 0.46 | |
Bomitel blanco | Cordia alliodora | 0.51 | |
Bompegya | Mammea africana | 0.69 | |
Bona | Morus mesozygia | 0.71 | |
Bona | Terminalia ivorensis | 0.54 | |
Bondu | Didelotia brevipaniculata | 0.54 | |
Bongola | Morus mesozygia | 0.71 | |
Bongossi | Lophira alata | 0.94 | |
Boniatillo | Phoebe elongata | 0.62 | |
Bonkese | Morus mesozygia | 0.71 | |
Bonkole | Lophira alata | 0.94 | |
Bonkonko | Antiaris toxicaria | 0.35 | |
Bonsum | Phoebe hainesiana | 0.43 | |
Pometia pinnata | 0.6 | ||
Bonyor | Poga oleosa | 0.39 | |
Bonzale | Beilschmiedia mannii | 0.62 | |
Bonzo | Chlorophora excelsa | 0.7 | |
Boonnak | Mesua ferrea | 0.92 | |
Bopala | Irvingia gabonensis | 0.76 | |
Bope | Staudtia stipitata | 0.79 | |
Bope bambale | Staudtia stipitata | 0.79 | |
Bopi-le | Mitragyna stipulosa | 0.53 | |
Borneo camphorwood | Dryobalanops lanceolata | 0.69 | |
Borneo keruing | Dipterocarpus warburgii | 0.53 | |
Borneo rosewood | Melanorrhoea spp. | 0.75 | |
Borneo teak | Intsia bijuga | 0.65 | |
Borneo teak | Intsia palembanica | 0.65 | |
Borneo yacal | Hopea odorata | 0.63 | |
Boroua | Mansonia altissima | 0.55 | |
Borowe | Manilkara bidentata | 0.95 | |
Bosasa | Staudtia stipitata | 0.79 | |
Boshi swa | Alnus nepalensis | 0.26 | |
Bosneak | Mesua ferrea | 0.92 | |
Bosnian maple | Acer platanus | 0.54 | |
Bossengue | Musanga cecropioides | 0.23 | |
Bossi | Terminalia ivorensis | 0.54 | |
Bostamarinde | Marmaroxylon racemosum | 1.07 | |
Bosulu | Pterocarpus soyauxii | 0.64 | 4 |
Shorea negrosensis | 0.59 | ||
Boti | Terminalia ivorensis | 0.54 | |
Botrie | Manilkara bidentata | 0.95 | |
Pterocarpus soyauxii | 0.64 | ||
Bouchi-caju | Anacardium excelsum | 0.33 | |
Boumbia | Terminalia ivorensis | 0.54 | |
Bouna | Terminalia ivorensis | 0.54 | |
Bourafete | Mitragyna ciliata | 0.52 | |
Bouri | Terminalia ivorensis | 0.54 | |
Bousi tamarin | Marmaroxylon racemosum | 1.07 | |
Bow wood | Maclura pomifera | 0.72 | |
Tabebuia serratifolia | 0.99 | ||
Nyssa aquatica | 0.5 | ||
Tabebuia serratifolia | 0.99 | ||
Box | Buxus sempervirens | 0.83 | 13 |
Boxelder | Acer negundo | 0.45 | 2 |
Boxwood | Buxus sempervirens | 0.83 | 13 |
Cornus florida | 0.72 | ||
Boxwood | Gonioma kamassi | 0.85 | |
Boxwood maracaibo | Gossypiospermum praecox | 0.77 | |
Boza | Mammea africana | 0.69 | |
Abies balsamea | 0.35 | ||
Bragba | Terminalia ivorensis | 0.54 | |
Brauna | Schinopsis spp. | 1.21 | |
Araucaria angustifolia | 0.49 | ||
Brazilian cedar | Cedrela odorata | 0.39 | 4 |
Brazilian Cherry | Hymenaea courbaril | 0.83 | 16 |
Bowdichia spp | 0.8 | ||
Diplotropis purpurea | 0.84 | ||
Brazilian ebony | Swartzia leiocalycina | 1 | 4 |
Hymenaea courbaril | 0.83 | ||
Brazilian mahogany | Plathymenia reticulata | 0.56 | 13 |
Swietenia macrophylla | 0.47 | ||
Platymiscium pinnatum | 0.87 | ||
Araucaria angustifolia | 0.49 | ||
Brazilian Rosewood | Dalbergia nigra | 0.84 | 2 |
Dalbergia frutescens | 1.02 | ||
Plathymenia reticulata | 0.56 | ||
Plathymenia reticulata | 0.56 | ||
Brazillian Oak | Amburana cearensis | 0.58 | 4 |
Couratari pulchra | 0.53 | ||
Couratari guianensis | 0.53 | ||
Tabebuia serratifolia | 0.99 | ||
Breiapfel | Manilkara zapota | 0.71 | |
Breu manga | Tetragastris altissima | 0.74 | |
Breu preto | Tetragastris altissima | 0.74 | |
Breugrande | Tetragastris altissima | 0.74 | |
Brewer oak | Quercus garryanna | 0.68 | |
Brimstone-wood | Terminalia ivorensis | 0.54 | |
Pinus ponderosa | 0.4 | ||
Thuja plicata | 0.32 | ||
Tsuga heterophylla | 0.45 | ||
Pseudotsuga menziesii | 0.48 | ||
Thuja plicata | 0.32 | ||
Tsuga heterophylla | 0.45 | ||
Pseudotsuga menziesii | 0.48 | ||
British elm | Ulmus procera | 0.53 | 13 |
British Guiana cedar | Cedrela odorata | 0.39 | 4 |
British Honduras cedar | Cedrela odorata | 0.39 | 4 |
British Honduras pitch pine | Pinus caribaea | 0.7 | |
British Honduras yellowwood | Podocarpus guatemalensis | 0.54 | |
Swietenia macrophylla | 0.47 | ||
Broad leaved peppermint | Eucalyptus dives | 0.68 | |
Broadleaf | Terminalia guyanensis | 0.6 | |
Acer macrophyllum | 0.48 | ||
Swietenia macrophylla | 0.47 | ||
Bro-kpah | Homalium dolicophyllum | 0.63 | |
Brown African padauk | Pterocarpus angolensis | 0.59 | 14 |
Fraxinus nigra | 0.49 | ||
Brown oak | Quercus petraea | 0.65 | |
Brown silverballi | Cordia alliodora | 0.51 | |
Brown-top stringy bark | Eucalyptus obliqua | 0.68 | 14 |
Eucalyptus obliqua | 0.68 | ||
Brunswick spruce | Picea glauca | 0.36 | 3 |
Brush Box | Tristania decorticata | 1.03 | |
Btaches | Calophyllum inophyllum | 0.55 | |
Buah keras | Aleurites moluccana | 0.14 | |
Guibourtia arnoldiana | 0.7 | ||
Bubinga | Guibourtia demeusei | 0.72 | 14 |
Guibourtia ehie | 0.71 | ||
Bubinga | Guibourtia pellegriniana | 0.8 | 13 |
Bubinga | Guibourtia tessmannii | 0.8 | 13 |
Bubu | Pinus insularis | 0.5 | |
Taxodium distichum | 0.46 | ||
Buckeye | Aesculus octandra | 0.24 | |
Bucuiba | Virola surinamensis | 0.51 | |
Bufoki | Staudtia stipitata | 0.79 | |
Bug'aom | Lagerstroemia piriformis | 0.67 | |
Bug'arom | Lagerstroemia piriformis | 0.67 | |
Buguarom | Lagerstroemia piriformis | 0.67 | |
Buhanan | Heritiera javanica | 0.65 | |
Buis d'Amerique | Gossypiospermum praecox | 0.77 | |
Bukao | Diplodiscus paniculatus | 0.62 | |
Bukundu | Piptadeniastrum africanum | 0.63 | |
Bul-bul | Pinus insularis | 0.5 | |
Pinus ponderosa | 0.4 | ||
Magnolia grandiflora | 0.5 | ||
Bulletwood | Manilkara bidentata | 0.95 | |
Bully | Manilkara bidentata | 0.95 | |
Bully tree | Manilkara bidentata | 0.95 | |
Bullywood | Terminalia amazonia | 0.76 | |
Bulokossa | Mitragyna stipulosa | 0.53 | |
Buma | Terminalia ivorensis | 0.54 | |
Buna | Terminalia ivorensis | 0.54 | |
Cornus florida | 0.72 | ||
Shorea negrosensis | 0.59 | ||
Bunnark | Mesua ferrea | 0.92 | |
Bunya bunya | Araucaria cunninghamii | 0.44 | 3 |
Bur Oak | Quercus macrocarpa | 0.64 | 1 |
Burak | Canangium odoratum | 0.28 | |
Burm | Cedrela toona | 0.47 | |
Burma cedar | Cedrela toona | 0.47 | |
Burma padauk | Pterocarpus macrocarpus | 0.79 | 3 |
Burokossa | Mitragyna stipulosa | 0.53 | |
Buru | Diplodiscus paniculatus | 0.62 | |
Burus | Chloroxylon swietenia | 0.88 | |
Burusang | Diplodiscus paniculatus | 0.62 | |
Buruta | Chloroxylon swietenia | 0.88 | |
Burutu | Chloroxylon swietenia | 0.88 | |
Triplochiton scleroxylon | 0.32 | ||
Bush oak | Chlorophora excelsa | 0.7 | |
Bush teak | Chlorophora excelsa | 0.7 | |
Buta-buta | Excoecaria agallocha | 0.42 | |
Buta-kadambe | Mitragyna parvifolia | 0.59 | |
Butternut | Juglans cinerea | 0.38 | 1 |
Diospyros virginiana | 0.71 | ||
Platanus occidentalis | 0.49 | ||
Platanus occidentalis | 0.49 | ||
Platanus occidentalis | 0.49 | ||
Buttonwood | Acer pseudoplatanus | 0.57 | 13 |
Platanus occidentalis | 0.49 | ||
Butungan | Xanthophyllum excelsum | 0.67 | |
Butusu | Tieghemella heckelii | 0.6 | |
Butwiome | Musanga cecropioides | 0.23 | |
Bwagashanga | Chlorophora excelsa | 0.7 | |
Millettia laurentii | 0.81 | ||
Swietenia macrophylla | 0.47 | ||
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Prunus serotina | 0.5 | ||
Prioria copaifera | 0.42 | ||
Cabrit | Zanthoxylum rhetsa | 0.56 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Platymiscium pinnatum | 0.87 | ||
Cadeno | Pseudosamanea guachapele | 0.58 | |
Tabebuia serratifolia | 0.99 | ||
Hymenaea courbaril | 0.83 | ||
Swietenia macrophylla | 0.47 | ||
CagŸ’ | Caryocar villosum | 0.76 | |
Cahu | Anacardium excelsum | 0.33 | |
Caimitillo | Micropholis guianensis | 0.67 | |
Cajarana | Anacardium excelsum | 0.33 | |
Cajou | Anacardium excelsum | 0.33 | |
Caju | Anacardium excelsum | 0.33 | |
Caju assu | Anacardium excelsum | 0.33 | |
Caju da Malta | Anacardium excelsum | 0.33 | |
Caju da matta | Anacardium excelsum | 0.33 | |
Caju do campo | Anacardium excelsum | 0.33 | |
Cajuca | Virola surinamensis | 0.51 | |
Cajuco | Virola koschnyi | 0.51 | |
Cajuea | Virola surinamensis | 0.51 | |
Cajueiro do campos | Anacardium excelsum | 0.33 | |
Cajuela | Hieronyma alchorneoides | 0.58 | |
Cajuhy | Anacardium excelsum | 0.33 | |
Cajuvana | Anacardium excelsum | 0.33 | |
Calamander wood | Diospyros celebica | 0.9 | 13 |
Calamansanay | Neonauclea calycinia | 0.79 | |
California black oak | Quercus kelloggii | 0.53 | 4 |
California laurel | Umbellularia californica | 0.55 | 3 |
Populus balsamifera | 0.34 | ||
Libocedrus decurrens | 0.37 | ||
California red fir | Abies magnifica | 0.38 | 1 |
California redwood | Sequoia sempervirens | 0.35 | |
California redwood | Sequoia sempervirens | 0.4 | |
Platanus occidentalis | 0.49 | ||
Libocedrus decurrens | 0.37 | ||
Picea sitchensis | 0.4 | ||
Libocedrus decurrens | 0.37 | ||
Californian redwood | Sequoia sempervirens | 0.35 | |
Californian redwood | Sequoia sempervirens | 0.4 | |
Pinus lambertiana | 0.36 | ||
Pinus ponderosa | 0.4 | ||
Pinus lambertiana | 0.36 | ||
Cal-que-lidze-na | Manilkara zapota | 0.71 | |
Calum calum | Hieronyma alchorneoides | 0.58 | |
Camagon | Diospyros celebica | 0.9 | 13 |
Camagon | Diospyros mindanaensis | 0.78 | 14 |
Camala | Virola surinamensis | 0.51 | |
Camaroncillo | Mitragyna ciliata | 0.52 | |
Camaru | Dipteryx odorata | 0.82 | |
Camashi | Staudtia stipitata | 0.79 | |
Camaticaro | Virola surinamensis | 0.51 | |
Cambala | Chlorophora regia | 0.59 | |
Cambara | Erisma uncinatum | 0.51 | |
Cambara | Vochysia ferruginea | 0.52 | |
Cambara | Vochysia guianensis | 0.52 | |
Cambara | Vochysia lehmanni | 0.52 | |
Cambara | Vochysia tomentosa | 0.52 | |
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Camiri nut | Aleurites moluccana | 0.14 | |
Swietenia macrophylla | 0.47 | ||
Camphor tree | Cinnamomum camphora | 0.38 | |
Camphre noir | Ocotea comoriensis | 0.51 | |
Campnosperma | Campnosperma brevipetiolata | 0.33 | |
Pterocarpus soyauxii | 0.64 | ||
Tabebuia serratifolia | 0.99 | ||
Tsuga canadensis | 0.4 | ||
Pinus strobus | 0.35 | ||
Fraxinus americana | 0.6 | ||
Populus tremuloides | 0.38 | ||
Abies balsamea | 0.35 | ||
Fagus grandifolia | 0.64 | ||
Ulmus thomasii | 0.63 | ||
Abies balsamea | 0.35 | ||
Tsuga canadensis | 0.4 | ||
Acer saccharum | 0.63 | ||
Quercus rubra | 0.63 | ||
Pinus resinosa | 0.46 | ||
Picea rubens | 0.4 | ||
Ulmus thomasii | 0.63 | ||
Betula alleghaniensis | 0.62 | ||
Canadian spruce | Picea glauca | 0.36 | 3 |
Picea mariana | 0.42 | ||
Betula papyrifera | 0.55 | ||
Liriodendron tulipifera | 0.42 | ||
Betula alleghaniensis | 0.62 | ||
Pinus strobus | 0.35 | ||
Canaguate | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Canalete | Cordia alliodora | 0.51 | |
Canalete de humo | Cordia alliodora | 0.51 | |
Canaletta | Cordia alliodora | 0.51 | |
Cananga | Canangium odoratum | 0.28 | |
Canary sassafras | Doryphora sassafras | 0.49 | |
Liriodendron tulipifera | 0.42 | ||
Liriodendron tulipifera | 0.42 | ||
Plathymenia reticulata | 0.56 | ||
Candela | Plathymenia reticulata | 0.56 | 13 |
Candelera | Cordia collococea | 0.5 | |
Candelillo | Magnolia sororum | 0.52 | |
Candelillo | Magnolia yoroconte | 0.52 | |
Candelo | Byrsonima coriacea | 0.68 | |
Candelo | Hieronyma alchorneoides | 0.58 | |
Candelo | Hyeronyma laxiflora | 0.58 | |
Candle berry | Byrsonima coriacea | 0.68 | |
Candle nut | Aleurites moluccana | 0.14 | |
Candlenut | Aleurites moluccana | 0.14 | |
Candlenut siris | Aleurites moluccana | 0.14 | |
Candlenut tree | Aleurites moluccana | 0.14 | |
Fraxinus americana | 0.6 | ||
Canelito | Vochysia lehmanni | 0.52 | |
Canelo | Hieronyma alchorneoides | 0.58 | |
Prioria copaifera | 0.42 | ||
Caniste | Pouteria izabalensis | 0.64 | |
Caniste | Pouteria pomifera | 0.84 | |
Canistel | Pouteria izabalensis | 0.64 | |
Canistel | Pouteria pomifera | 0.84 | |
Hymenaea courbaril | 0.83 | ||
Betula papyrifera | 0.55 | ||
Chamaecyparis nootkatensis | 0.44 | ||
Thuja plicata | 0.32 | ||
Liriodendron tulipifera | 0.42 | ||
Canshan | Terminalia amazonia | 0.76 | |
Canshan | Terminalia amazonica | 0.76 | |
Canxun | Terminalia guyanensis | 0.6 | |
Swietenia macrophylla | 0.47 | ||
Platymiscium pinnatum | 0.87 | ||
Caoba | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Caoba | Swietenia mahagoni | 0.57 | |
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Caoba de Santo Domingo | Sickingia salvadorense | 0.65 | |
Caoba de Santo Domingo | Swietenia mahagoni | 0.57 | |
Caoba del pais | Podocarpus guatemalensis | 0.54 | |
Caoba dominicana | Sickingia salvadorense | 0.65 | |
Caoba Dominicana | Swietenia mahagoni | 0.57 | |
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Caobilla | Podocarpus guatemalensis | 0.54 | |
Caobilla | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Caobilla | Swietenia mahagoni | 0.57 | |
Hymenaea courbaril | 0.83 | ||
Capa | Cordia alliodora | 0.51 | |
Capa amarillo | Cordia alliodora | 0.51 | |
Capa de olor | Cordia alliodora | 0.51 | |
Capa de sabana | Cordia alliodora | 0.51 | |
Capa de tabaco | Couratari pulchra | 0.53 | 4 |
Capa Prieto | Cordia alliodora | 0.51 | |
Capa sabana | Cordia alliodora | 0.51 | |
Cape beech | Rapanea melanophleos | 0.74 | |
Cape boxwood | Gonioma kamassi | 0.85 | |
Cape lilac | Melia azedarach | 0.51 | |
Prunus serotina | 0.5 | ||
Prunus serotina | 0.5 | ||
Prunus serotina | 0.5 | ||
Prunus serotina | 0.5 | ||
Carabali | Piptadeniastrum africanum | 0.63 | |
Caracoli | Anacardium excelsum | 0.33 | |
Carbonero | Piptadeniastrum africanum | 0.63 | |
Cargamanto | Hieronyma alchorneoides | 0.58 | |
Cargamento | Hyeronyma laxiflora | 0.58 | |
Caribaea-den | Pinus caribaea | 0.7 | |
Caribbean longleaf pitch pine | Pinus caribaea | 0.7 | |
Caribbean pine | Pinus caribaea | 0.7 | |
Caribbean pitch pine | Pinus caribaea | 0.7 | |
Carne asada | Hyeronyma laxiflora | 0.58 | |
Carneasada | Hieronyma alchorneoides | 0.58 | |
Carneasada | Hyeronyma laxiflora | 0.58 | |
Carolina linden | Tilia americana | 0.37 | |
Populus deltoides | 0.4 | ||
Acer rubrum | 0.54 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Carpathian beech | Fagus sylvatica | 0.67 | 13 |
Carpin | Carpinus betulus | 0.61 | |
Carpy | Carpinus betulus | 0.61 | |
Carvalho sedoso | Grevillea robusta | 0.54 | |
Casaco | Hieronyma alchorneoides | 0.58 | |
Casaco | Hyeronyma laxiflora | 0.58 | |
Abies amabilis | 0.43 | ||
Caschou | Anacardium excelsum | 0.33 | |
Casco | Hieronyma alchorneoides | 0.58 | |
Cashu | Anacardium excelsum | 0.33 | |
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Castelo | Gossypiospermum praecox | 0.77 | |
Casuarina | Casuarina equisetifolia | 0.87 | |
Casuarins | Casuarina equisetifolia | 0.87 | |
Cat spruce | Picea glauca | 0.36 | 3 |
Hura crepitans | 0.4 | ||
Catalpa | Catalpa speciosa | 0.37 | |
Hymenaea courbaril | 0.83 | ||
Catatu | Hieronyma alchorneoides | 0.58 | |
Hura crepitans | 0.4 | 2 | |
Catawba | Catalpa speciosa | 0.37 | |
Cativo | Prioria copaifera | 0.42 | 2 |
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Cauri | Terminalia ivorensis | 0.54 | |
Prioria copaifera | 0.42 | ||
Cay sao ba | Hopea odorata | 0.63 | |
Cebo | Virola surinamensis | 0.51 | |
Ceceru | Morus mesozygia | 0.71 | |
Cedar | Acacia melanoxylon | 0.54 | |
Cedar | Cedrela odorata | 0.39 | 4 |
Thuja occidentalis | 0.31 | ||
Cedar elm | Ulmus crassifolia | 0.62 | |
Cedar lightwood | Acacia melanoxylon | 0.54 | |
Cedar of Lebanon | Cedrus libani | 0.53 | 13 |
Pinus glabra | 0.44 | ||
Pinus palustris | 0.59 | ||
Ceder | Cedrela huberi | 0.4 | 4 |
Cedrat | Cedrela huberi | 0.4 | 4 |
Cedre du Liban | Cedrus libani | 0.53 | 13 |
Cedre rouge | Cedrela huberi | 0.4 | 4 |
Cedre rouge | Cedrela odorata | 0.39 | 4 |
Cedre rouge | Cedrela toona | 0.47 | |
Cedrela odorata | 0.39 | ||
Cedrela odorata | 0.39 | ||
Cedrela odorata | 0.39 | ||
Cedremacho | Hieronyma alchorneoides | 0.58 | |
Cedrillo | Huertea cubensis | 0.34 | |
Cedrillo | Virola surinamensis | 0.51 | |
Cedrinho | Erisma uncinatum | 0.51 | |
Cedro | Cedrela huberi | 0.4 | 4 |
Cedro | Cedrela odorata | 0.39 | 4 |
Cedro | Cedrela toona | 0.47 | |
Cedro branco | Cedrela huberi | 0.4 | 4 |
Cedrela odorata | 0.39 | ||
Cedro del Libano | Cedrus libani | 0.53 | 13 |
Swietenia macrophylla | 0.47 | ||
Cedrela odorata | 0.39 | ||
Cedrela odorata | 0.39 | ||
Cedro macho | Hyeronyma laxiflora | 0.58 | |
Cedrela odorata | 0.39 | ||
Cedro oloroso | Cedrela odorata | 0.39 | 4 |
Cedro rana | Vochysia guianensis | 0.52 | |
Cedro red | Cedrela odorata | 0.39 | 4 |
Cedrela odorata | 0.39 | ||
Cedrorana | Vochysia ferruginea | 0.52 | |
Cedrorana | Vochysia guianensis | 0.52 | |
Swietenia macrophylla | 0.47 | ||
Cedro-rana | Vochysia guianensis | 0.52 | |
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Celery-top pine | Phyllocladus rhomboidalis | 0.6 | |
Central American cedar | Cedrela odorata | 0.39 | 4 |
Swietenia macrophylla | 0.47 | ||
Cerejeira | Amburana cearensis | 0.58 | 4 |
Cerejeira rajada | Amburana cearensis | 0.58 | 4 |
Amburana cearensis | 0.58 | ||
Amburana cearensis | 0.58 | ||
Amburana cearensis | 0.58 | ||
Cereza cimarrona | Cordia collococea | 0.5 | |
Prunus serotina | 0.5 | ||
Prunus serotina | 0.5 | ||
Prunus avium | 0.58 | ||
Cerlang laut | Heritiera javanica | 0.65 | |
Ceylon satinwood | Chloroxylon swietenia | 0.88 | |
Cha wa ta pho | Anisoptera costata | 0.52 | |
Swietenia macrophylla | 0.47 | ||
Pometia pinnata | 0.6 | ||
Pterocarpus indicus | 0.57 | ||
Chaliviande | Virola surinamensis | 0.51 | |
Chalviande | Virola surinamensis | 0.51 | |
Chambo caspi | Vochysia hondurensis | 0.52 | |
Chamfuta | Afzelia quanzensis | 0.62 | |
Chamfuti | Afzelia quanzensis | 0.62 | |
Platymiscium pinnatum | 0.87 | ||
Champ | Michelia excelsa | 0.42 | |
Champ | Michelia sp. | 0.42 | |
Champaca | Michelia excelsa | 0.42 | |
Champaca | Michelia sp. | 0.42 | |
Champak | Michelia excelsa | 0.42 | |
Nyssa sylvatica | 0.5 | ||
Chan thip | Tarrietia sylvatica | 0.82 | |
Chan vit | Vitex cofassus | 0.67 | |
Chanfuta | Afzelia quanzensis | 0.62 | |
Chanfuti | Afzelia quanzensis | 0.62 | |
Changugo | Byrsonima coriacea | 0.68 | |
Chanun | Populus ciliata | 0.37 | |
Chan-vit | Vitex cofassus | 0.67 | |
Chaparro | Byrsonima coriacea | 0.68 | |
Chaparro de chinche | Byrsonima coriacea | 0.68 | |
Chapel | Aspidosperma desmanthum | 0.65 | |
Chaperna | Aspidosperma desmanthum | 0.65 | |
Shorea negrosensis | 0.59 | ||
Chaquiro | Podocarpus guatemalensis | 0.54 | |
Charapilla | Dipteryx odorata | 0.82 | |
Charm | Campnosperma brevipetiolata | 0.33 | |
Charme | Carpinus betulus | 0.61 | |
Chasemiich | Terminalia amazonia | 0.76 | |
Chasemiich | Terminalia arjuna | 0.71 | |
Chasemiich | Terminalia ivorensis | 0.54 | |
Chasemiich | Terminalia procera | 0.54 | |
Chati | Pygeum africanum | 0.61 | |
Chauku | Casuarina equisetifolia | 0.87 | |
Chavuku | Casuarina equisetifolia | 0.87 | |
Chawari | Caryocar villosum | 0.76 | |
Chicharron amarillo | Terminalia guyanensis | 0.6 | |
Che ke | Hopea odorata | 0.63 | |
Chein | Melia azedarach | 0.51 | |
Chela | Polyalthia fragans | 0.46 | |
Chelampai | Mitragyna parvifolia | 0.59 | |
Chelaun | Populus ciliata | 0.37 | |
Chemnen | Afzelia quanzensis | 0.62 | |
Chempaka | Michelia excelsa | 0.42 | |
Chempaka | Michelia sp. | 0.42 | |
Chen | Piptadeniastrum africanum | 0.63 | |
Chenchen | Antiaris toxicaria | 0.35 | |
Quercus robur | 0.57 | ||
Chene caparo | Cordia alliodora | 0.51 | |
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Chengai | Balanocarpus heimii | 0.78 | |
Chengai batu | Balanocarpus heimii | 0.78 | |
Chengal | Anisoptera costata | 0.52 | |
Chengal | Balanocarpus heimii | 0.78 | |
Chengal | Hopea odorata | 0.63 | |
Chengal kampong | Hopea odorata | 0.63 | |
Chengal mas | Hopea odorata | 0.63 | |
Chengal pasir | Hopea odorata | 0.63 | |
Chengal pulau | Hopea odorata | 0.63 | |
Prunus avium | 0.58 | ||
Prunus serotina | 0.5 | ||
Cherry | Pygeum africanum | 0.61 | |
Cherry bark oak | Quercus falcata var. pagodaefolia | 0.68 | 1 |
Betula lenta | 0.65 | ||
Cherry mahogany | Tieghemella heckelii | 0.6 | |
Castanea dentata | 0.43 | ||
Castanea sativa | 0.51 | ||
Chestnut white oak | Quecus prinus | 0.66 | 1 |
Chewing gum tree | Manilkara zapota | 0.71 | |
Chewstick | Vochysia guianensis | 0.52 | |
Swietenia macrophylla | 0.47 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Tabebuia serratifolia | 0.99 | ||
Chicazapote | Pouteria pomifera | 0.84 | |
Chicharro | Terminalia amazonia | 0.76 | |
Chicharron | Terminalia guyanensis | 0.6 | |
Chichica | Aspidosperma desmanthum | 0.65 | |
Chicle | Manilkara zapota | 0.71 | |
Chicle macho | Manilkara zapota | 0.71 | |
Chicle tree | Manilkara zapota | 0.71 | |
Chicltree | Manilkara zapota | 0.71 | |
Chico | Manilkara zapota | 0.71 | |
Chico zapote | Pouteria izabalensis | 0.64 | |
Chicosapote | Manilkara zapota | 0.71 | |
Chicot | Gymnocladus dioicus | 0.4 | |
Chicozapota | Manilkara bidentata | 0.95 | |
Chicozapote | Manilkara bidentata | 0.95 | |
Chicozapote | Manilkara zapota | 0.71 | |
Chiculte | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Chiculte | Swietenia mahagoni | 0.57 | |
Swietenia macrophylla | 0.47 | ||
Chiczapotl | Manilkara zapota | 0.71 | |
Chikado | Cedrela toona | 0.47 | |
Buxus sempervirens | 0.83 | ||
Chikuma | Rapanea melanophleos | 0.74 | |
Chilauni | Schima wallichii | 0.62 | |
Araucaria angustifolia | 0.49 | ||
Chilla | Excoecaria agallocha | 0.42 | |
Chamaecyparis thyoides | 0.32 | ||
Chimbulla | Vochysia lehmanni | 0.52 | |
Chimbulla | Vochysia tomentosa | 0.52 | |
Chimbuya | Vochysia ferruginea | 0.52 | |
Chimbuya | Vochysia guianensis | 0.52 | |
Hymenaea courbaril | 0.83 | ||
Chinaberry | Melia azedarach | 0.51 | |
Chinaberry lilaila | Melia azedarach | 0.51 | |
Chinaberry tree | Melia azedarach | 0.51 | |
Chinatree | Melia azedarach | 0.51 | |
Chinese guger tree | Schima wallichii | 0.62 | |
Chi-nga mas | Balanocarpus heimii | 0.78 | |
Chingal | Balanocarpus heimii | 0.78 | |
Castanea dentata | 0.43 | ||
Chinkapin | Castanopsis chrysophylla | 0.44 | |
Chinna kadambu | Mitragyna parvifolia | 0.59 | |
Chinni | Morus alba | 0.6 | |
Chinyok | Garuga pinnata | 0.51 | |
Chiquibul | Manilkara zapota | 0.71 | |
Prunus serotina | 0.5 | ||
Choboch | Heritiera javanica | 0.65 | |
Choboch | Heritiera ornithocephala | 0.7 | |
Prunus serotina | 0.5 | ||
Prunus serotina | 0.5 | ||
Chopwoch | Heritiera javanica | 0.65 | |
Chopwoch | Heritiera ornithocephala | 0.7 | |
Chouk | Casuarina equisetifolia | 0.87 | |
Chowku | Casuarina equisetifolia | 0.87 | |
Choyo | Intsia bijuga | 0.65 | |
Cedrela odorata | 0.39 | ||
Chula-maram | Casuarina equisetifolia | 0.87 | |
Chumplak | Heritiera javanica | 0.65 | |
Chumpraek | Heritiera javanica | 0.65 | |
Chumprag | Heritiera javanica | 0.65 | |
Chumprak | Heritiera javanica | 0.65 | |
Chumprak | Heritiera ornithocephala | 0.7 | |
Chun | Morus alba | 0.6 | |
Chupi cara | Byrsonima coriacea | 0.68 | |
Chupi-cara | Byrsonima coriacea | 0.68 | |
Chupon Colorado | Micropholis guianensis | 0.67 | |
Churuli | Mesua ferrea | 0.92 | |
Cigar box | Cedrela huberi | 0.4 | 4 |
Cigar box cedar | Cedrela huberi | 0.4 | 4 |
Cigar box cedar | Cedrela odorata | 0.39 | 4 |
Cigar tree | Catalpa speciosa | 0.37 | |
Cedrela odorata | 0.39 | ||
Hymenaea courbaril | 0.83 | ||
Cinamomo | Melia azedarach | 0.51 | |
Cinnamomo | Melia azedarach | 0.51 | |
Cinnamon wood | Cinnamomum camphora | 0.38 | |
Cipres | Casuarina equisetifolia | 0.87 | |
Cipres | Podocarpus guatemalensis | 0.54 | |
Cipres | Podocarpus neriifolia | 0.48 | |
Taxodium distichum | 0.46 | ||
Cipresillo lorito | Podocarpus guatemalensis | 0.54 | |
Cipresillo lorito | Podocarpus neriifolia | 0.48 | |
Taxodium distichum | 0.46 | ||
Cipricillo | Podocarpus guatemalensis | 0.54 | |
Cipricillo | Podocarpus neriifolia | 0.48 | |
Circassian boxwood | Buxus sempervirens | 0.83 | 13 |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Ciruelo | Dalbergia stevensonii | 0.88 | |
Hymenaea courbaril | 0.83 | ||
Cloeziana gum | Eucalyptus cloeziana | 0.8 | |
Co ky | Hopea odorata | 0.63 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Pseudotsuga menziesii | 0.48 | ||
Arbutus menziesii | 0.64 | ||
Coast redwood | Sequoia sempervirens | 0.35 | |
Coast redwood | Sequoia sempervirens | 0.4 | |
Picea sitchensis | 0.4 | ||
Cobano | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Cobano | Swietenia mahagoni | 0.57 | |
Cochun | Terminalia amazonia | 0.76 | |
Cochun | Terminalia amazonica | 0.76 | |
Cochun | Terminalia guyanensis | 0.6 | |
Coco cabuyo | Couratari pulchra | 0.53 | 4 |
Coco Cristal | Eschweilera sagotiana | 0.9 | |
Coco de Mono | Eschweilera sagotiana | 0.9 | |
Cocobolo | Dalbergia retusa | 0.85 | 4 |
Platymiscium pinnatum | 0.87 | ||
Triplochiton scleroxylon | 0.32 | ||
Coffe nut | Gymnocladus dioicus | 0.4 | |
Coffee mortar | Terminalia amazonia | 0.76 | |
Coffee mortar | Terminalia amazonica | 0.76 | |
Coffetree | Gymnocladus dioicus | 0.4 | |
Tabebuia serratifolia | 0.99 | ||
Colorada | Virola koschnyi | 0.51 | |
Hymenaea courbaril | 0.83 | ||
Cedrela odorata | 0.39 | ||
Pseudotsuga menziesii | 0.48 | ||
Abies concolor | 0.39 | ||
Pseudotsuga menziesii | 0.48 | ||
Pseudotsuga menziesii | 0.48 | ||
Abies concolor | 0.39 | ||
Pseudotsuga menziesii | 0.48 | ||
Comarre | Dipteryx odorata | 0.82 | |
Combo-combo | Musanga cecropioides | 0.23 | |
Hymenaea courbaril | 0.83 | ||
Comino real | Aniba duckei | 0.56 | |
Common alder | Alnus glutinosa | 0.41 | |
Fraxinus excelsior | 0.58 | ||
Taxodium distichum | 0.46 | ||
Fagus sylvatica | 0.67 | ||
Common black kakaralli | Eschweilera sagotiana | 0.9 | |
Buxus sempervirens | 0.83 | ||
Quercus robur | 0.57 | ||
Celtis occidentalis | 0.53 | ||
Tsuga canadensis | 0.4 | ||
Common larch | Larix decidua | 0.48 | 14 |
Common persimmon | Diospyros virginiana | 0.71 | 1 |
Common pine | Pinus sylvestris | 0.45 | 14 |
Common spruce | Picea abies | 0.43 | |
Common willow | Salix alba | 0.38 | |
Common yew | Taxus baccata | 0.63 | 13 |
Abies concolor | 0.39 | ||
Condrotti | Bombax chevalieri | 0.51 | |
Conduru | Brosimum rubescens | 0.63 | |
Terminalia superba | 0.4 | ||
Congo-congo | Musanga cecropioides | 0.23 | |
Congolo garapelo | Couratari pulchra | 0.53 | 4 |
Congowood | Lovoa trichiliodes | 0.46 | |
Congu | Mitragyna parvifolia | 0.59 | |
Pinus contorta | 0.41 | ||
Copachi | Aspidosperma desmanthum | 0.65 | |
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Prioria copaifera | 0.42 | ||
Copal | Daniella thurifera | 0.46 | |
Hymenaea courbaril | 0.83 | ||
Copal | Oxystigma oxyphyllum | 0.53 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Liquidambar styraciflua | 0.52 | ||
Liquidambar styraciflua | 0.52 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Pterocarpus soyauxii | 0.64 | ||
Coral | Hieronyma alchorneoides | 0.58 | |
Tabebuia serratifolia | 0.99 | ||
Cordia | Cordia alliodora | 0.51 | |
Cork bark elm | Ulmus hollandica | 0.53 | |
Ulmus thomasii | 0.63 | ||
Pinus strobus | 0.35 | ||
Abies lasiocarpa | 0.32 | ||
Corkwood | Chlorophora excelsa | 0.7 | |
Corkwood | Musanga cecropioides | 0.23 | |
Cornus florida | 0.72 | ||
Hymenaea courbaril | 0.83 | ||
Coromandel | Diospyros celebica | 0.9 | 13 |
Corosillo | Vochysia ferruginea | 0.52 | |
Corosillo | Vochysia guianensis | 0.52 | |
Corosillo | Vochysia lehmanni | 0.52 | |
Corosillo | Vochysia tomentosa | 0.52 | |
Corpus | Vochysia hondurensis | 0.52 | |
Corpus elosuchil | Magnolia sororum | 0.52 | |
Corpus elosuchil | Magnolia yoroconte | 0.52 | |
Cortes | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Cortez | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Platymiscium pinnatum | 0.87 | ||
Coto | Aniba duckei | 0.56 | |
Nyssa aquatica | 0.5 | ||
Populus balsamifera | 0.34 | ||
Cottonwood | Populus ciliata | 0.37 | |
Populus deltoides | 0.4 | ||
Populus trichocarpa | 0.35 | ||
Couaie | Erisma uncinatum | 0.51 | |
Couaie | Virola surinamensis | 0.51 | |
Couatari | Couratari pulchra | 0.53 | 4 |
Hymenaea courbaril | 0.83 | ||
Coumarouna | Dipteryx odorata | 0.82 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Tabebuia serratifolia | 0.99 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Taxodium distichum | 0.46 | ||
Quercus michauxii | 0.67 | ||
Platymiscium pinnatum | 0.87 | ||
Crab apple | Malus pumila | 0.64 | |
Craboo | Byrsonima coriacea | 0.68 | |
Crack willow | Salix fragilis | 0.38 | |
Cricket bat willow | Salix alba | 0.38 | |
Criollo | Minquartia guianensis | 0.83 | |
Platymiscium pinnatum | 0.87 | ||
Swietenia macrophylla | 0.47 | ||
Cryptomeria | Cryptomeria japonica | 0.36 | |
Cuajo | Virola surinamensis | 0.51 | |
Cuangare | Iryanthera spp. | 0.58 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hura crepitans | 0.4 | ||
Cedrela odorata | 0.39 | ||
Cuban mahogany | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Cuban mahogany | Swietenia mahagoni | 0.57 | |
Cuban pine | Pinus caribaea | 0.7 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Quercus alba | 0.68 | ||
Quercus bicolor | 0.72 | ||
Quercus coccinea | 0.67 | ||
Quercus macrocarpa | 0.64 | ||
Quercus michauxii | 0.67 | ||
Quercus palustris | 0.63 | ||
Cucharillo | Quercus petraea | 0.65 | |
Quercus stellata | 0.67 | ||
Quercus velutina | 0.61 | ||
Cucharillo | Quercus virginiana | 0.84 | |
Cuchillo | Gossypiospermum praecox | 0.77 | |
Magnolia grandiflora | 0.5 | ||
Pometia pinnata | 0.6 | ||
Cuiarana | Terminalia amazonica | 0.76 | |
Cumala | Virola surinamensis | 0.51 | |
Cumare | Amburana cearensis | 0.58 | 4 |
Cumaru | Amburana cearensis | 0.58 | 4 |
Cumaru | Dipteryx odorata | 0.82 | |
Cumaru | Dipteryx odorata syn. Coumarouna odorata | 0.92 | 4 |
Cumaru amarello | Dipteryx odorata | 0.82 | |
Cumaru da folha grande | Dipteryx odorata | 0.82 | |
Amburana cearensis | 0.58 | ||
Cumaru de ceara | Amburana cearensis | 0.58 | 4 |
Cumaru de cheiro | Amburana cearensis | 0.58 | 4 |
Cumaru do Amazonas | Dipteryx odorata | 0.82 | |
Amburana cearensis | 0.58 | ||
Cumaru ebo | Dipteryx odorata | 0.82 | |
Cumaru roxo | Dipteryx odorata | 0.82 | |
Amburana cearensis | 0.58 | ||
Cumarut | Dipteryx odorata | 0.82 | |
Cumbari | Dipteryx odorata | 0.82 | |
Cumbaru das cantingas | Amburana cearensis | 0.58 | 4 |
Cumbillo | Terminalia amazonia | 0.76 | |
Cunuru | Dipteryx odorata | 0.82 | |
Hymenaea courbaril | 0.83 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Hymenaea courbaril | 0.83 | ||
Araucaria angustifolia | 0.49 | ||
Curlet mahogany | Swietenia mahagoni | 0.57 | |
Betula alleghaniensis | 0.62 | ||
Acer saccharum | 0.63 | ||
Curtidor | Hieronyma alchorneoides | 0.58 | |
Curtidor | Hyeronyma laxiflora | 0.58 | |
Prioria copaifera | 0.42 | ||
Araucaria angustifolia | 0.49 | ||
Diospyros virginiana | 0.71 | ||
Cyp | Cordia alliodora | 0.51 | |
Cypre | Cordia alliodora | 0.51 | |
Cypress | Cordia alliodora | 0.51 | |
Cypress | Cupressus sempervirens | 0.42 | |
Cypress | Cupressus torulosa | 0.47 | |
Cypress | Podocarpus guatemalensis | 0.54 | |
Taxodium distichum | 0.46 | ||
Pinus banksiana | 0.43 | ||
Daan | Albizia procera | 0.55 | |
Daba | Peltogyne venosa | 0.69 | |
Dabema | Piptadeniastrum africanum | 0.63 | |
Dagang | Anisoptera curtisii | 0.52 | |
Pometia pinnata | 0.6 | ||
Dagum | Anisoptera curtisii | 0.52 | |
Dahoma | Piptadeniastrum africanum | 0.63 | |
Pometia pinnata | 0.6 | ||
Dakain | Melia azedarach | 0.51 | |
Dakua makadre | Agathis borneensis | 0.41 | |
Dakua makadre | Agathis philippinensis | 0.33 | |
Dakua salusalu | Decussocarpus vitiensis | 0.34 | |
Dalchini | Cinnamomum camphora | 0.38 | |
Dalli | Cedrela serrata | 0.52 | |
Dalli | Virola surinamensis | 0.51 | |
Dallie | Virola surinamensis | 0.51 | |
Dalra | Cedrela serrata | 0.52 | |
Damanu | Calophyllum inophyllum | 0.55 | |
Damanu | Calophyllum tomentosum | 0.59 | |
Damar batu | Pinus merkusii | 0.59 | |
Damar bunga | Pinus merkusii | 0.59 | |
Damar kelasi | Anisoptera costata | 0.52 | |
Damar ketimpun | Anisoptera costata | 0.52 | |
Damar lilin | Anisoptera costata | 0.52 | |
Damar mata kuching | Anisoptera costata | 0.52 | |
Damar miharo | Anisoptera costata | 0.52 | |
Damar minyak | Agathis borneensis | 0.41 | |
Damar minyak | Agathis philippinensis | 0.33 | |
Damar poetih | Hopea odorata | 0.63 | |
Damar tingkis | Anisoptera costata | 0.52 | |
Damoni | Dracontomelon edule | 0.44 | |
Dandad | Piptadeniastrum africanum | 0.63 | |
Dane | Piptadeniastrum africanum | 0.63 | |
Dangila | Koordersiodendron pinnatum | 0.71 | |
Daniellia | Daniella oliveri | 0.49 | |
Daniellia | Daniella thurifera | 0.46 | |
Shorea negrosensis | 0.59 | ||
Danish beech | Fagus sylvatica | 0.67 | 13 |
Pinus sylvestris | 0.45 | ||
Pinus sylvestris | 0.45 | ||
Dao | Dracontomelon edule | 0.44 | |
Dao | Dracontomelum dao | 0.66 | |
Darachik | Melia azedarach | 0.51 | |
Darachk | Melia azedarach | 0.51 | |
Darah darah | Myristica buchneriana | 0.41 | |
Darah darah | Myristica chartacea | 0.48 | |
Darah darah | Myristica hypargyraea | 0.44 | |
Darah darah | Myristica sp. | 0.54 | |
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Dark red lauan | Shorea negrosensis | 0.59 | 4 |
Dark red meranti | Shorea negrosensis | 0.59 | 4 |
Shorea negrosensis | 0.59 | ||
Dark red seraya | Shorea negrosensis | 0.59 | 4 |
Darli | Cedrela serrata | 0.52 | |
Fraxinus pennsylvanica | 0.56 | ||
Darloi | Cedrela serrata | 0.52 | |
Darlu | Cedrela serrata | 0.52 | |
Dasal lanang | Hopea odorata | 0.63 | |
Dastan | Peltogyne porphyrocardia | 0.69 | |
Dastan | Peltogyne venosa | 0.69 | |
Dau | Dipterocarpus basilanicus | 0.54 | |
Dau | Dipterocarpus grandiflorus | 0.68 | |
Dau | Dipterocarpus warburgii | 0.53 | |
Dau heo | Garuga pinnata | 0.51 | |
Daueng | Aglaia gigantea | 0.54 | |
Dauri | Cedrela serrata | 0.52 | |
Dead tree | Gymnocladus dioicus | 0.4 | |
Dedira | Intsia bijuga | 0.65 | |
Degame | Calycophyllum candidissimum | 0.72 | 2 |
Deknoi | Melia azedarach | 0.51 | |
Populus deltoides | 0.4 | ||
Denkan | Melia azedarach | 0.51 | |
Deodar | Cupressus torulosa | 0.47 | |
De-orh | Tarrietia utilis | 0.54 | |
Derekan | Aleurites moluccana | 0.14 | |
Chamaecyparis thyoides | 0.32 | ||
Determa | Ocotea rubra | 0.55 | 2 |
Prunus serotina | 0.5 | ||
Devagarige | Dysoxylum malabaricum | 0.62 | |
Devdari | Cedrela toona | 0.47 | |
Devidiyar | Cupressus torulosa | 0.47 | |
Dhaman | Grewia elastica | 0.63 | |
Dhamma | Grewia elastica | 0.63 | |
Dhundul | Carapa molluccensis | 0.71 | |
Dhupi | Cupressus torulosa | 0.47 | |
Dibetou | Lovoa trichiliodes | 0.46 | |
Dibiue mutshi ditoke | Irvingia gabonensis | 0.76 | |
Dieng doh | Bucklandia populnea | 0.56 | |
Dieng myntat | Bucklandia populnea | 0.56 | |
Dieng-doh | Bucklandia populnea | 0.56 | |
Dieng-ngai | Mesua ferrea | 0.92 | |
Dieng-soh-langhri-that | Grewia elastica | 0.63 | |
Dieng-soh-ryndoh | Bucklandia populnea | 0.56 | |
Dieng-tha-ballich | Grewia elastica | 0.63 | |
Difou | Morus mesozygia | 0.71 | |
Dika | Irvingia gabonensis | 0.76 | |
Dika-bread tree | Irvingia gabonensis | 0.76 | |
Dika-nut tree | Irvingia gabonensis | 0.76 | |
Dikela | Millettia laurentii | 0.81 | 14 |
Dilang butiki | Podocarpus guatemalensis | 0.54 | |
Dilang butiki | Podocarpus neriifolia | 0.48 | |
Dillenia | Dillenia luzoniensis | 0.65 | |
Dillenia | Dillenia pentagyna | 0.55 | |
Dilly | Manilkara zapota | 0.71 | |
Dimori | Tieghemella heckelii | 0.6 | |
Dimpapi | Tieghemella heckelii | 0.6 | |
Dingdah | Bucklandia populnea | 0.56 | |
Dinglas | Lagerstroemia piriformis | 0.67 | |
Dingsa | Pinus insularis | 0.5 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Liquidambar styraciflua | 0.52 | ||
Diseng | Musanga cecropioides | 0.23 | |
Diuka mahogany | Irvingia gabonensis | 0.76 | |
Diutu | Tieghemella heckelii | 0.6 | |
Djamudju | Podocarpus guatemalensis | 0.54 | |
Djamudju | Podocarpus neriifolia | 0.48 | |
Djempina | Hopea odorata | 0.63 | |
Djimbo | Mammea africana | 0.69 | |
Terminalia superba | 0.4 | ||
Djunia | Musanga cecropioides | 0.23 | |
Djuru-tu | Tieghemella heckelii | 0.6 | |
Doaando | Bridelia aubrevillei | 0.59 | |
Dodda | Bassia latifolia | 0.82 | |
Doe | Musanga cecropioides | 0.23 | |
Doekaliballi | Brosimum rubescens | 0.63 | |
Cornus florida | 0.72 | ||
Dohng | Campnosperma brevipetiolata | 0.33 | |
Doi | Alphitonia zizyphoides | 0.43 | |
Doka | Anisoptera costata | 0.52 | |
Doka | Isoberlinia doka | 0.63 | |
Pometia pinnata | 0.6 | ||
Dollywood | Virola surinamensis | 0.51 | |
Dominican mahogany | Sickingia salvadorense | 0.65 | |
Dominican mahogany | Swietenia mahagoni | 0.57 | |
Doncella | Byrsonima coriacea | 0.68 | |
Dong | Mitragyna stipulosa | 0.53 | |
Dorea | Dracontomelon edule | 0.44 | |
Dormilon | Vochysia lehmanni | 0.52 | |
Dormilon | Vochysia tomentosa | 0.52 | |
Dort | Intsia bijuga | 0.65 | |
Dotial | Cupressus torulosa | 0.47 | |
Pseudotsuga menziesii | 0.48 | ||
Pseudotsuga menziesii | 0.48 | ||
Douglas-fir | Pseudotsuga menziesii | 0.48 | 5 |
Pseudotsuga menziesii | 0.48 | ||
Douka | Tieghemella heckelii | 0.6 | |
Doussie | Afzelia bipindensis | 0.62 | |
Doussie | Afzelia pachyloba | 0.62 | |
Doussie | Afzelia quanzensis | 0.62 | |
Dowora | Intsia bijuga | 0.65 | |
Drago | Pterocarpus vernalis | 0.63 | |
Drawi | Cedrela serrata | 0.52 | |
Drawi | Cedrela toona | 0.47 | |
Drek | Melia azedarach | 0.51 | |
Acer rubrum | 0.54 | ||
Turraeanthus africanus | 0.51 | ||
Duali | Anisoptera curtisii | 0.52 | |
Dubima | Piptadeniastrum africanum | 0.63 | |
Dubin biri | Lovoa trichiliodes | 0.46 | |
Dud phras | Populus ciliata | 0.37 | |
Dudley willow | Salix alba | 0.38 | |
Salix nigra | 0.39 | ||
Duforokoto | Mammea africana | 0.69 | |
Duguan | Myristica buchneriana | 0.41 | |
Duguan | Myristica chartacea | 0.48 | |
Duguan | Myristica hypargyraea | 0.44 | |
Duguan | Myristica sp. | 0.54 | |
Duika | Irvingia gabonensis | 0.76 | |
Platymiscium pinnatum | 0.87 | ||
Duklap | Pygeum turnerianum | 0.44 | |
Dumate | Lagerstroemia piriformis | 0.67 | |
Diospyros ebenum | 0.94 | ||
Dumizulu | Pygeum africanum | 0.61 | |
Dumone | Tieghemella heckelii | 0.6 | |
Dumori | Tieghemella heckelii | 0.6 | |
Ilex opaca | 0.55 | ||
Dungon | Heritiera javanica | 0.65 | |
Dungon | Tarrietia sylvatica | 0.82 | |
Dungun | Heritiera javanica | 0.65 | |
Dungun gungung | Heritiera javanica | 0.65 | |
Dungun-dungun | Heritiera javanica | 0.65 | |
Duong-lieu | Casuarina equisetifolia | 0.87 | |
Dupdupan | Diplodiscus paniculatus | 0.62 | |
Durian | Durio carinatus Masters | 0.63 | 18 |
Durian | Durio zibethinus Murray | 0.61 | 18 |
Durian | Neesia altissima | 0.44 | 18 |
Durla | Cedrela serrata | 0.52 | |
Durmast | Quercus petraea | 0.65 | |
Durmast oak | Quercus petraea | 0.65 | |
Dutch elm | Ulmus hollandica | 0.53 | |
Dwema | Musanga cecropioides | 0.23 | |
Dwini | Morus mesozygia | 0.71 | |
Dzama | Musanga cecropioides | 0.23 | |
Dzogbedodo | Terminalia ivorensis | 0.54 | |
E. African black camphorwood | Ocotea comoriensis | 0.51 | |
Eas | Excoecaria agallocha | 0.42 | |
East African afzelia | Afzelia quanzensis | 0.62 | |
East African cypress | Cupressus sempervirens | 0.42 | |
East African mahogany | Khaya nyassica | 0.44 | |
East African Olive | Olea hochstetteri | 0.81 | 10 |
East African silky oak | Grevillea robusta | 0.54 | |
Larix laricina | 0.53 | ||
East indian ebony | Diospyros ebenaster | 0.61 | 4 |
Diospyros ebenum | 0.94 | ||
East Indian ebony | Diospyros inclusa | 0.7 | 14 |
East Indian ebony | Diospyros melanoxylon | 0.67 | |
East Indian ebony | Diospyros mindanaensis | 0.78 | 14 |
East Indian ebony | Diospyros pyrrhocarpa | 0.69 | 14 |
Pterocarpus indicus | 0.57 | ||
East Indian satinwood | Chloroxylon swietenia | 0.88 | |
East London boxwood | Gonioma kamassi | 0.85 | |
Thuja occidentalis | 0.31 | ||
Juglans nigra | 0.55 | ||
Larix laricina | 0.53 | ||
Eastern Canadian Spruce | Picea glauca | 0.36 | 3 |
Eastern cedar | Thuja occidentalis | 0.31 | |
Eastern cottonwood | Populus deltoides | 0.40 | 1 |
Abies balsamea | 0.35 | ||
Eastern hemlock | Tsuga canadensis | 0.40 | 1 |
Eastern hophornbeam | Ostrya virginiana | 0.70 | 3 |
Larix laricina | 0.53 | ||
Populus deltoides | 0.4 | ||
Eastern redcedar | Juniperus virginiana | 0.47 | 1 |
Eastern Spruce | Picea glauca | 0.36 | 3 |
Picea mariana | 0.42 | ||
Picea rubens | 0.4 | ||
Juglans nigra | 0.55 | ||
Thuja occidentalis | 0.31 | ||
Eastern White Pine | Pinus strobus | 0.35 | 1 |
Thuja occidentalis | 0.31 | ||
Prioria copaifera | 0.42 | ||
Eba | Lophira alata | 0.94 | |
Eba | Mitragyna stipulosa | 0.53 | |
Ebano verde | Tabebuia serratifolia | 0.99 | 4 |
Diospyros ebenum | 0.94 | ||
Ebar | Mitragyna stipulosa | 0.53 | |
Ebba | Lophira alata | 0.94 | |
Ebe | Cordia platythyrsa | 0.39 | |
Eben | Mitragyna ciliata | 0.52 | |
Eben | Mitragyna stipulosa | 0.53 | |
Tabebuia serratifolia | 0.99 | ||
Ebene vert | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Pterocarpus soyauxii | 0.64 | ||
Ebi | Terminalia ivorensis | 0.54 | |
Ebiara | Berlinia acuminata | 0.64 | |
Ebo | Dipteryx odorata | 0.82 | |
Pometia pinnata | 0.6 | ||
Ebone plaqueminier | Diospyros ebenaster | 0.61 | 4 |
Diospyros ebenum | 0.94 | ||
Ebony persimmon | Diospyros ebenaster | 0.61 | 4 |
Diospyros ebenum | 0.94 | ||
Ebony persimmon | Diospyros inclusa | 0.7 | 14 |
Ebony persimmon | Diospyros melanoxylon | 0.67 | |
Ebony persimmon | Diospyros mindanaensis | 0.78 | 14 |
Ebony persimmon | Diospyros pyrrhocarpa | 0.69 | 14 |
Ebornzork | Mammea africana | 0.69 | |
Tabebuia serratifolia | 0.99 | ||
Echites mahagoni | Swietenia mahagoni | 0.57 | |
Ecuador laurel | Cordia alliodora | 0.51 | |
Edel | Mangifera indica | 0.53 | |
Castanea sativa | 0.51 | ||
Edinam | Tieghemella heckelii | 0.6 | |
Terminalia superba | 0.4 | ||
Edumoi | Tieghemella heckelii | 0.6 | |
Prunus serotina | 0.5 | ||
Efok | Pterygota bequaertii | 0.53 | |
Efremeli | Terminalia ivorensis | 0.54 | |
Egbesu | Musanga cecropioides | 0.23 | |
Terminalia superba | 0.4 | ||
Egeun | Musanga cecropioides | 0.23 | |
Egg fruit | Pouteria pomifera | 0.84 | |
Eghoinmebbi | Terminalia ivorensis | 0.54 | |
Eghoin-nebi | Terminalia ivorensis | 0.54 | |
Egimamfuk | Musanga cecropioides | 0.23 | |
Triplochiton scleroxylon | 0.32 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Egoyn odan | Terminalia ivorensis | 0.54 | |
Egoyne lukan | Terminalia ivorensis | 0.54 | |
Egoyne nebi | Terminalia ivorensis | 0.54 | |
Egoyne-lukan | Terminalia ivorensis | 0.54 | |
Egoyne-nebi | Terminalia ivorensis | 0.54 | |
Egoyn-odan | Terminalia ivorensis | 0.54 | |
Egui | Musanga cecropioides | 0.23 | |
Eguni | Musanga cecropioides | 0.23 | |
Egunli | Musanga cecropioides | 0.23 | |
Eh | Intsia bijuga | 0.65 | |
Ehie | Guibourtia ehie | 0.71 | 4 |
Ehyedua | Daniella thurifera | 0.46 | |
Quercus robur | 0.57 | ||
Quercus robur | 0.57 | ||
Eis | Alnus glutinosa | 0.41 | |
Terminalia superba | 0.4 | ||
Triplochiton scleroxylon | 0.32 | ||
Triplochiton scleroxylon | 0.32 | ||
Ekhimi | Piptadeniastrum africanum | 0.63 | |
Ekhivi | Piptadeniastrum africanum | 0.63 | |
Ekki | Lophira alata | 0.94 | |
Ekom | Poga oleosa | 0.39 | |
Ekomba | Musanga cecropioides | 0.23 | |
Ekombo | Musanga cecropioides | 0.23 | |
Ekop | Staudtia stipitata | 0.79 | |
Ekop evene | Brachystegia laurentii | 0.57 | |
Ekop lele | Brachystegia laurentii | 0.57 | |
Ekop zing | Didelotia brevipaniculata | 0.54 | |
Ekor belangkas | Endospermum macrophyllum | 0.41 | |
Ekoune | Cephalosphaera usambarensis | 0.44 | |
Ekpogi | Berlinia acuminata | 0.64 | |
Elae | Piptadeniastrum africanum | 0.63 | |
Elak | Campnosperma brevipetiolata | 0.33 | |
Elany | Piptadeniastrum africanum | 0.63 | |
Eleba | Lophira alata | 0.94 | |
Elelom | Mitragyna ciliata | 0.52 | |
Elelom n'zame | Mitragyna ciliata | 0.52 | |
Elelome n'zame | Mitragyna ciliata | 0.52 | |
Elelon | Mitragyna ciliata | 0.52 | |
Elilom | Mitragyna stipulosa | 0.53 | |
Pinus Elliottii | 0.59 | ||
Ellongrypho | Peltogyne porphyrocardia | 0.69 | |
Ellongrypho | Peltogyne venosa | 0.69 | |
Elm | Ulmus alata | 0.65 | |
Ulmus americana | 0.5 | ||
Elm | Ulmus campestris | 0.52 | 13 |
Elm | Ulmus crassifolia | 0.62 | |
Elm | Ulmus glabra | 0.53 | |
Elm | Ulmus procera | 0.53 | 13 |
Ulmus rubra | 0.53 | ||
Ulmus thomasii | 0.63 | ||
Elolom | Mitragyna ciliata | 0.52 | |
Elowa | Chlorophora excelsa | 0.7 | |
Els | Alnus glutinosa | 0.41 | |
Elua | Chlorophora excelsa | 0.7 | |
Elui | Chlorophora excelsa | 0.7 | |
Elupa | Bassia latifolia | 0.82 | |
Emang | Chlorophora excelsa | 0.7 | |
Embero | Lovoa trichiliodes | 0.46 | |
Embora | Melia azedarach | 0.51 | |
Amburana cearensis | 0.58 | ||
Emen | Terminalia ivorensis | 0.54 | |
Emeri | Terminalia ivorensis | 0.54 | |
Emeri | Vochysia hondurensis | 0.52 | |
Emery | Vochysia hondurensis | 0.52 | |
Emil | Terminalia ivorensis | 0.54 | |
Emine | Terminalia ivorensis | 0.54 | |
Emola | Oxystigma oxyphyllum | 0.53 | |
Emoli | Oxystigma oxyphyllum | 0.53 | |
Emolo | Oxystigma oxyphyllum | 0.53 | |
Emory | Vochysia hondurensis | 0.52 | |
Empas | Koompassia malaccensis | 0.76 | |
Emri | Terminalia ivorensis | 0.54 | |
Emyu | Poga oleosa | 0.39 | |
Tabebuia serratifolia | 0.99 | ||
Encens rouge | Tetragastris altissima | 0.74 | |
Quercus alba | 0.68 | ||
Quercus bicolor | 0.72 | ||
Quercus coccinea | 0.67 | ||
Quercus macrocarpa | 0.64 | ||
Quercus michauxii | 0.67 | ||
Quercus palustris | 0.63 | ||
Encino | Quercus petraea | 0.65 | |
Quercus stellata | 0.67 | ||
Quercus velutina | 0.61 | ||
Encino | Quercus virginiana | 0.84 | |
Quercus alba | 0.68 | ||
Quercus bicolor | 0.72 | ||
Quercus coccinea | 0.67 | ||
Quercus macrocarpa | 0.64 | ||
Quercus michauxii | 0.67 | ||
Quercus palustris | 0.63 | ||
Encino negro | Quercus petraea | 0.65 | |
Quercus stellata | 0.67 | ||
Quercus velutina | 0.61 | ||
Encino negro | Quercus virginiana | 0.84 | |
Terminalia superba | 0.4 | ||
Endra-endra | Humbertia madagascariensis | 1.18 | |
Endui | Lophira alata | 0.94 | |
Endwi | Lophira alata | 0.94 | |
Eng | Dipterocarpus basilanicus | 0.54 | |
Eng | Dipterocarpus grandiflorus | 0.68 | |
Eng | Dipterocarpus warburgii | 0.53 | |
Turraeanthus africanus | 0.51 | ||
Engelmann spruce | Picea engelmannii | 0.35 | 1 |
Enggaris | Koompassia malaccensis | 0.76 | |
Enggeris | Koompassia malaccensis | 0.76 | |
English ash | Fraxinus excelsior | 0.58 | 14 |
English beech | Fagus sylvatica | 0.67 | 13 |
English birch | Betula sp. | 0.61 | |
English brown oak | Quercus petraea | 0.65 | |
Prunus avium | 0.58 | ||
Castanea dentata | 0.43 | ||
English elm | Ulmus campestris | 0.52 | 13 |
English elm | Ulmus procera | 0.53 | 13 |
English harewood | Acer pseudoplatanus | 0.57 | 13 |
Acer pseudoplatanus | 0.57 | ||
English oak | Quercus petraea | 0.65 | |
English oak | Quercus robur | 0.57 | 16 |
English plane | Platanus hybrida | 0.59 | |
Enoi | Poga oleosa | 0.39 | |
Enoupou | Mitragyna ciliata | 0.52 | |
Entenam | Anisoptera costata | 0.52 | |
Entuyut | Tetramerista glabra | 0.73 | |
Microberlinia brazzavillensis | 0.77 | ||
Enwan | Lophira alata | 0.94 | |
Turraeanthus africanus | 0.51 | ||
Pterocarpus soyauxii | 0.64 | ||
Epepe | Terminalia ivorensis | 0.54 | |
Epi | Cedrela huberi | 0.4 | 4 |
Epi | Cedrela odorata | 0.39 | 4 |
Epi | Cedrela toona | 0.47 | |
Abies grandis | 0.37 | ||
Pterocarpus soyauxii | 0.64 | ||
Epoukou | Mitragyna ciliata | 0.52 | |
Erable | Acer campestre | 0.55 | |
Eran | Piptadeniastrum africanum | 0.63 | |
Ereru | Planchonella euphlebia | 0.89 | |
Erle | Alnus glutinosa | 0.41 | |
Erundu | Piptadeniastrum africanum | 0.63 | |
Prunus serotina | 0.5 | ||
Pterocarpus soyauxii | 0.64 | ||
Esemi | Terminalia amazonia | 0.76 | |
Esemi | Terminalia arjuna | 0.71 | |
Esemi | Terminalia ivorensis | 0.54 | |
Esemi | Terminalia procera | 0.54 | |
Esire | Lophira alata | 0.94 | |
Esore | Lophira alata | 0.94 | |
Espatodea | Spathodea campanulata | 0.25 | |
Espave | Anacardium excelsum | 0.33 | |
Espavel | Anacardium excelsum | 0.33 | |
Espavel amarillo | Anacardium excelsum | 0.33 | |
Espavel rosado | Anacardium excelsum | 0.33 | |
Populus tremuloides | 0.38 | ||
Plathymenia reticulata | 0.56 | ||
Essaben | Berlinia acuminata | 0.64 | |
Essai | Mansonia altissima | 0.55 | |
Essoule | Berlinia acuminata | 0.64 | |
Liquidambar styraciflua | 0.52 | ||
Turraeanthus africanus | 0.51 | ||
Etekele | Drypetes gossweileri | 0.63 | |
Eti-ayip | Mitragyna stipulosa | 0.53 | |
Etu | Irvingia gabonensis | 0.76 | |
Etue | Irvingia gabonensis | 0.76 | |
Eucalyptus | Eucalyptus citriodora | 0.65 | |
Eucalyptus | Eucalyptus obliqua | 0.68 | 14 |
European alder | Alnus glutinosa | 0.41 | |
European ash | Fraxinus excelsior | 0.58 | 14 |
European aspen | Populus tremula | 0.42 | |
European beech | Fagus sylvatica | 0.67 | 13 |
European birch | Betula sp. | 0.61 | |
European boxwood | Buxus sempervirens | 0.83 | 13 |
European cherry | Prunus avium | 0.58 | 13 |
Castanea dentata | 0.43 | ||
European chestnut | Castanea sativa | 0.51 | 13 |
European hornbeam | Carpinus betulus | 0.61 | |
European horse chestnut | Aesculus hippocastanum | 0.39 | |
European larch | Larix decidua | 0.48 | 14 |
European lime | Tilia vulgaris | 0.51 | 13 |
European maple | Acer campestre | 0.55 | |
European maple | Acer platanus | 0.54 | |
Acer pseudoplatanus | 0.57 | ||
European oak | Quercus petraea | 0.65 | |
European oak | Quercus robur | 0.57 | 16 |
European plane | Platanus hybrida | 0.59 | |
European spruce | Picea abies | 0.43 | |
European walnut | Juglans regia | 0.56 | 16 |
Quercus robur | 0.57 | ||
European whitewood | Picea abies | 0.43 | |
European yew | Taxus baccata | 0.63 | 13 |
Fraxinus excelsior | 0.58 | ||
Evergreen chinkapin | Castanopsis acuminatissima | 0.56 | |
Magnolia grandiflora | 0.5 | ||
Ewe | Mitragyna stipulosa | 0.53 | |
Ewe aiye | Morus mesozygia | 0.71 | |
Triplochiton scleroxylon | 0.32 | ||
Eyan | Lovoa trichiliodes | 0.46 | |
Pterocarpus soyauxii | 0.64 | ||
Tsuga heterophylla | 0.45 | ||
Faboy | Lophira alata | 0.94 | |
Falis | Populus ciliata | 0.37 | |
Robinia pseudoacacia | 0.69 | ||
Chamaecyparis lawsoniana | 0.43 | ||
Chamaecyparis nootkatensis | 0.44 | ||
Chamaecyparis thyoides | 0.32 | ||
Celtis occidentalis | 0.53 | ||
False mopane | Guibourtia coleosperma | 0.66 | |
False opepe | Mitragyna ciliata | 0.52 | |
False opepe | Mitragyna stipulosa | 0.53 | |
Falso pao brasil | Brosimum rubescens | 0.63 | |
Fantsinakoko | Humbertia madagascariensis | 1.18 | |
Fara | Daniella thurifera | 0.46 | |
Terminalia superba | 0.4 | ||
F'araeneri | Terminalia ivorensis | 0.54 | |
Farayemile | Terminalia ivorensis | 0.54 | |
Farayomile | Terminalia ivorensis | 0.54 | |
Faro | Daniella thurifera | 0.46 | |
Fata | Vitex cofassus | 0.67 | |
Fataromile | Terminalia ivorensis | 0.54 | |
Faux balata | Micropholis guianensis | 0.67 | |
Faux gayac | Dipteryx odorata | 0.82 | |
Taxodium distichum | 0.46 | ||
Fagus sylvatica | 0.67 | ||
Fela | Terminalia ivorensis | 0.54 | |
Feli kouali | Erisma uncinatum | 0.51 | |
Felli kouali | Erisma uncinatum | 0.51 | |
Female rosewood | Aniba duckei | 0.56 | |
Fereng | Canangium odoratum | 0.28 | |
Ferolia | Brosimum rubescens | 0.63 | |
Feurier | Dipteryx odorata | 0.82 | |
Acer saccharum | 0.63 | ||
Field maple | Acer campestre | 0.55 | |
Fiji pine | Pinus caribaea | 0.7 | |
Fijian Sterculia | Sterculia vitiensis | 0.34 | |
Filao | Casuarina equisetifolia | 0.87 | |
Finnish aspen | Populus tremula | 0.42 | |
Finnish birch | Betula sp. | 0.61 | |
Pinus sylvestris | 0.45 | ||
Pinus sylvestris | 0.45 | ||
Finnish whitewood | Picea abies | 0.43 | |
Finuki-ukaba | Intsia bijuga | 0.65 | |
Abies amabilis | 0.43 | ||
Abies balsamea | 0.35 | ||
Abies grandis | 0.37 | ||
Abies lasiocarpa | 0.32 | ||
Abies magnifica | 0.38 | ||
Abies procera | 0.39 | ||
Fir | Picea abies | 0.43 | |
Pinus sylvestris | 0.45 | ||
Fira-wase | Terminalia ivorensis | 0.54 | |
Flambeau rouge | Catostemma fragrans | 0.66 | |
Flameau rouge | Catostemma fragrans | 0.66 | |
Flindersia | Flindersia pimenteliana | 0.51 | |
Flindersia | Flindersia pubescens | 0.6 | |
Tabebuia serratifolia | 0.99 | ||
Flor amarillo | Vochysia hondurensis | 0.52 | |
Flor de paraiso | Melia azedarach | 0.51 | |
Swietenia macrophylla | 0.47 | ||
Florecillo | Qualea paraensis | 0.58 | |
Prioria copaifera | 0.42 | ||
Tilia americana | 0.37 | ||
Taxodium distichum | 0.46 | ||
Cornus florida | 0.72 | ||
Ulmus americana | 0.5 | ||
Tilia americana | 0.37 | ||
Pinus palustris | 0.59 | ||
Pinus palustris | 0.59 | ||
Flowered satinwood | Chloroxylon swietenia | 0.88 | |
Flowering dogwood | Cornus florida | 0.72 | 3 |
Platymiscium pinnatum | 0.87 | ||
Forescom | Morus mesozygia | 0.71 | |
Forest gum | Eucalyptus tereticornis | 0.82 | |
Forest red gum | Eucalyptus tereticornis | 0.82 | |
Forest tamarind | Marmaroxylon racemosum | 1.07 | |
Formosan camphor | Cinnamomum camphora | 0.38 | |
Fountain tree | Spathodea campanulata | 0.25 | |
Pinus taeda | 0.51 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Frameri | Terminalia ivorensis | 0.54 | |
Terminalia superba | 0.4 | ||
Framine | Terminalia ivorensis | 0.54 | |
Framire | Terminalia ivorensis | 0.54 | |
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Freijo | Cordia alliodora | 0.51 | |
French ash | Fraxinus excelsior | 0.58 | 14 |
French aspen | Populus tremula | 0.42 | |
French beech | Fagus sylvatica | 0.67 | 13 |
French oak | Quercus petraea | 0.65 | |
Quercus robur | 0.57 | ||
French plane | Platanus hybrida | 0.59 | |
Fraxinus americana | 0.6 | ||
Fresno | Fraxinus excelsior | 0.58 | 14 |
Fraxinus nigra | 0.49 | ||
Fraxinus pennsylvanica | 0.56 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Frijolillo | Pseudosamanea guachapele | 0.58 | |
Fruit cherry | Prunus avium | 0.58 | 13 |
Fruta dorada | Virola koschnyi | 0.51 | |
Fruta dorda | Virola koschnyi | 0.51 | |
Fteh | Calophyllum inophyllum | 0.55 | |
Fteh | Calophyllum tomentosum | 0.59 | |
Fukadi | Terminalia amazonia | 0.76 | |
Fukadi | Terminalia amazonica | 0.76 | |
Fungunigalo | Gonystylus macrophyllum | 0.54 | |
Guibourtia ehie | 0.71 | ||
Gabon Tulip Tree | Spathodea campanulata | 0.25 | |
Gad pipal | Populus ciliata | 0.37 | |
Gagil | Hopea iriana | 0.8 | |
Gagil | Hopea odorata | 0.63 | |
Gagil | Koordersiodendron pinnatum | 0.71 | |
Turraeanthus africanus | 0.51 | ||
Galla | Cupressus torulosa | 0.47 | |
Abies balsamea | 0.35 | ||
Galumpit | Heritiera javanica | 0.65 | |
Pometia pinnata | 0.6 | ||
Gambiri | Aleurites moluccana | 0.14 | |
Gan man naga | Catostemma fragrans | 0.66 | |
Gangau | Mesua ferrea | 0.92 | |
Gangaw | Mesua ferrea | 0.92 | |
Gangwa | Excoecaria agallocha | 0.42 | |
Garamut | Vitex cofassus | 0.67 | |
Garis | Koompassia malaccensis | 0.76 | |
Garry oak | Quercus garryanna | 0.68 | |
Garu | Excoecaria agallocha | 0.42 | |
Garu-buaja | Gonystylus macrophyllum | 0.54 | |
Garuga | Garuga pinnata | 0.51 | |
Pometia pinnata | 0.6 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Gateado | Sickingia salvadorense | 0.65 | |
Swietenia macrophylla | 0.47 | ||
Gateado | Swietenia mahagoni | 0.57 | |
Gau | Piptadeniastrum africanum | 0.63 | |
Hymenaea courbaril | 0.83 | ||
Gauri | Polyalthia fragans | 0.46 | |
Gavetillo | Aspidosperma desmanthum | 0.65 | |
Gawasa | Vitex cofassus | 0.67 | |
Gawi | Anisoptera costata | 0.52 | |
Gayac | Dipteryx odorata | 0.82 | |
Gayac de cayennee | Dipteryx odorata | 0.82 | |
Gayal | Dipteryx odorata | 0.82 | |
Gba | Beilschmiedia mannii | 0.62 | |
Terminalia superba | 0.4 | ||
Gbasi | Terminalia ivorensis | 0.54 | |
Gbawo | Musanga cecropioides | 0.23 | |
Gbei | Beilschmiedia mannii | 0.62 | |
Gbele | Irvingia gabonensis | 0.76 | |
Gboko nisa | Beilschmiedia mannii | 0.62 | |
Gborduorh | Berlinia acuminata | 0.64 | |
Gbwei | Beilschmiedia mannii | 0.62 | |
Gean | Prunus avium | 0.58 | 13 |
Pinus sylvestris | 0.45 | ||
Geh | Chlorophora excelsa | 0.7 | |
Gelam | Syzygium buettnerianum | 0.73 | |
Gelso bianco | Morus alba | 0.6 | |
Gelupang batu | Heritiera javanica | 0.65 | |
Pometia pinnata | 0.6 | ||
Gemaris | Koompassia malaccensis | 0.76 | |
Gembris | Koompassia malaccensis | 0.76 | |
Gemeris | Koompassia malaccensis | 0.76 | |
Genuine | Cinnamomum camphora | 0.38 | |
Geon | Excoecaria agallocha | 0.42 | |
Geor | Excoecaria agallocha | 0.42 | |
Pinus palustris | 0.59 | ||
Pinus palustris | 0.59 | ||
Geremo | Heritiera javanica | 0.65 | |
Geria | Excoecaria agallocha | 0.42 | |
Geringging | Melia azedarach | 0.51 | |
Gerok | Bucklandia populnea | 0.56 | |
Geva | Excoecaria agallocha | 0.42 | |
Gevlambe bostamarinde | Marmaroxylon racemosum | 1.07 | |
Gewa | Excoecaria agallocha | 0.42 | |
Triplochiton scleroxylon | 0.32 | ||
Guibourtia ehie | 0.71 | ||
Triplochiton scleroxylon | 0.32 | ||
Ghana walnut | Lovoa trichiliodes | 0.46 | |
Ghiriya | Chloroxylon swietenia | 0.88 | |
Prunus serotina | 0.5 | ||
Ghughole | Intsia bijuga | 0.65 | |
Pometia pinnata | 0.6 | ||
Swietenia macrophylla | 0.47 | ||
Thuja plicata | 0.32 | ||
Thuja plicata | 0.32 | ||
Thuja plicata | 0.32 | ||
Giant chinkapin | Castanopsis chrysophylla | 0.44 | |
Abies grandis | 0.37 | ||
Thuja plicata | 0.32 | ||
Pinus lambertiana | 0.36 | ||
Prunus serotina | 0.5 | ||
Pometia pinnata | 0.6 | ||
Ginja hoehoe | Terminalia amazonia | 0.76 | |
Ginoo | Koompassia excelsa | 0.75 | |
Ginsek | Anisoptera curtisii | 0.52 | |
Chamaecyparis lawsoniana | 0.43 | ||
Pterocarpus angolensis | 0.59 | ||
Glu | Musanga cecropioides | 0.23 | |
Gluta | Melanorrhoea spp. | 0.75 | |
Go nuoe | Intsia palembanica | 0.65 | |
Go nvoe | Intsia bijuga | 0.65 | |
Gofassa | Vitex cofassus | 0.67 | |
Gofilei | Tieghemella heckelii | 0.6 | |
Goi | Aglaia gigantea | 0.54 | |
Goi tia | Aglaia gigantea | 0.54 | |
Betula alleghaniensis | 0.62 | ||
Golden chestnut | Castanopsis chrysophylla | 0.44 | |
Golden deal | Doryphora sassafras | 0.49 | |
Golden ebony | Diospyros celebica | 0.9 | 13 |
Abies magnifica | 0.38 | ||
Robinia pseudoacacia | 0.69 | ||
Golden spoon | Byrsonima coriacea | 0.68 | |
Plathymenia reticulata | 0.56 | ||
Goli karam | Mitragyna parvifolia | 0.59 | |
Hymenaea courbaril | 0.83 | ||
Goma amarilla | Vochysia lehmanni | 0.52 | |
Goma amarilla | Vochysia tomentosa | 0.52 | |
Gombeira | Swartzia leiocalycina | 1 | 4 |
Hymenaea courbaril | 0.83 | ||
Gomo | Vochysia lehmanni | 0.52 | |
Gomo | Vochysia tomentosa | 0.52 | |
Gomorrow | Dipteryx odorata | 0.82 | |
Goncalo alves | Astronium graveolens | 0.89 | 19 |
Goncalo alves | Astronium graveolens | 0.8 | 19 |
Gonfolo | Qualea albiflora | 0.54 | |
Gonfolo | Qualea paraensis | 0.58 | |
Gonfolo Rose | Qualea paraensis | 0.58 | |
Go-nuoe | Intsia bijuga | 0.65 | |
Gonyer | Grewia elastica | 0.63 | |
Goodding willow | Salix alba | 0.38 | |
Salix nigra | 0.39 | ||
Goraci | Koompassia malaccensis | 0.76 | |
Gore | Mitragyna parvifolia | 0.59 | |
Goria nim | Cedrela toona | 0.47 | |
Goum ne wet | Aleurites moluccana | 0.14 | |
Goure karam | Mitragyna parvifolia | 0.59 | |
Govwi | Musanga cecropioides | 0.23 | |
Gox nuwowse | Intsia bijuga | 0.65 | |
Pometia pinnata | 0.6 | ||
Gran | Picea abies | 0.43 | |
Gran cashew | Anacardium excelsum | 0.33 | |
Platymiscium pinnatum | 0.87 | ||
Swietenia macrophylla | 0.47 | ||
Grand Fir | Abies grandis | 0.37 | 1 |
Gravilea | Grevillea robusta | 0.54 | |
Grawa | Cedrela toona | 0.47 | |
Betula alleghaniensis | 0.62 | ||
Ulmus rubra | 0.53 | ||
Tsuga heterophylla | 0.45 | ||
Acer pseudoplatanus | 0.57 | ||
Quercus rubra | 0.63 | ||
Pinus banksiana | 0.43 | ||
Great maple | Acer pseudoplatanus | 0.57 | 13 |
Abies amabilis | 0.43 | ||
Pinus lambertiana | 0.36 | ||
Fraxinus americana | 0.6 | ||
Green Ash | Fraxinus pennsylvanica | 0.56 | 1 |
Liriodendron tulipifera | 0.42 | ||
Robinia pseudoacacia | 0.69 | ||
Tabebuia serratifolia | 0.99 | ||
Greirllea | Grevillea robusta | 0.54 | |
Tabebuia serratifolia | 0.99 | ||
Grevilea | Grevillea robusta | 0.54 | |
Grevilia | Grevillea robusta | 0.54 | |
Grevillea | Grevillea robusta | 0.54 | |
Grey alder | Alnus glutinosa | 0.41 | |
Grey alder | Alnus nepalensis | 0.26 | |
Grey box | Eucalyptus hemiphloia | 0.93 | |
Tsuga heterophylla | 0.45 | ||
Pinus banksiana | 0.43 | ||
Grey sassafras | Doryphora sassafras | 0.49 | |
Tabebuia serratifolia | 0.99 | ||
Grignon Fou | Qualea albiflora | 0.54 | |
Grignon fou | Qualea paraensis | 0.58 | |
Grignon fou | Vochysia ferruginea | 0.52 | |
Grignon fou | Vochysia guianensis | 0.52 | |
Groenhart | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Gronfoeloe | Qualea paraensis | 0.58 | |
Gronfolo | Qualea albiflora | 0.54 | |
Groot locus | Dipteryx odorata | 0.82 | |
Grumixava | Micropholis guianensis | 0.67 | |
Guaba | Terminalia amazonia | 0.76 | |
Guachapele | Pseudosamanea guachapele | 0.58 | |
Guachapeli | Pseudosamanea guachapele | 0.58 | |
Guacharaco | Terminalia amazonia | 0.76 | |
Guacimil | Cordia alliodora | 0.51 | |
Guamarillo | Pseudosamanea guachapele | 0.58 | |
Guanacaste | Enterolobium cyclocarpum | 0.35 | 4 |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Guarabœ | Peltogyne venosa | 0.69 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Guarabu | Peltogyne porphyrocardia | 0.69 | |
Guaraburajado | Peltogyne venosa | 0.69 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Guaruba | Qualea albiflora | 0.54 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Guasimo nogal | Cordia alliodora | 0.51 | |
Turraeanthus africanus | 0.51 | ||
Guatambu (Brazil) | Balfourodendron riedelianum | 0.79 | 11 |
Guatambu (Argentinean) | Balfourodendron riedelianum | 0.7 | 11 |
Swietenia macrophylla | 0.47 | ||
Guatuso | Terminalia amazonia | 0.76 | |
Guayabo | Terminalia amazonia | 0.76 | |
Guayabo | Terminalia amazonica | 0.76 | |
Guayabo | Terminalia guyanensis | 0.6 | |
Guayabo de montana | Terminalia guyanensis | 0.6 | |
Guayabo leon | Terminalia amazonia | 0.76 | |
Guayabo leon | Terminalia amazonica | 0.76 | |
Guayabo negro | Terminalia amazonia | 0.76 | |
Guayabon | Terminalia amazonia | 0.76 | |
Guayacan | Guaiacum spp. | 1.26 | 10 |
Guayacan | Minquartia guianensis | 0.83 | |
Guayacan | Tabebuia serratifolia | 0.99 | 4 |
Guayacan pech | Minquartia guianensis | 0.83 | |
Guayacan pechiche | Minquartia guianensis | 0.83 | |
Tabebuia serratifolia | 0.99 | ||
Guayo | Terminalia guyanensis | 0.6 | |
Gubas | Endospermum macrophyllum | 0.41 | |
Gue | Lophira alata | 0.94 | |
Guela-china | Manilkara zapota | 0.71 | |
Gueladao guenda-china | Manilkara zapota | 0.71 | |
Guele | Chlorophora excelsa | 0.7 | |
Guenda-guina | Manilkara zapota | 0.71 | |
Guendaxina | Manilkara zapota | 0.71 | |
Guh | Chlorophora excelsa | 0.7 | |
Gui | Mitragyna parvifolia | 0.59 | |
Guiba | Irvingia gabonensis | 0.76 | |
Guijo | Shorea guiso | 0.75 | |
Guima | Musanga cecropioides | 0.23 | |
Guingamadou | Virola surinamensis | 0.51 | |
Guinguamadou | Virola surinamensis | 0.51 | |
Guissepa | Mansonia altissima | 0.55 | |
Pterocarpus soyauxii | 0.64 | ||
Pinus elliottii | 0.59 | ||
Taxodium distichum | 0.46 | ||
Guli | Piptadeniastrum africanum | 0.63 | |
Gulla | Cupressus torulosa | 0.47 | |
Gulrai | Cupressus torulosa | 0.47 | |
Liquidambar styraciflua | 0.52 | ||
Nyssa aquatica | 0.5 | ||
Gum copal | Daniella thurifera | 0.46 | |
Nyssa aquatica | 0.5 | ||
Liquidambar styraciflua | 0.52 | ||
Hymenaea courbaril | 0.83 | ||
Juglans nigra | 0.55 | ||
Tabebuia serratifolia | 0.99 | ||
Gupasa | Vitex cofassus | 0.67 | |
Gupasa | Vitex parviflora | 0.68 | |
Gupit | Pygeum turnerianum | 0.44 | |
Guri | Mitragyna parvifolia | 0.59 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Gutumba | Chlorophora excelsa | 0.7 | |
Guyabillo | Terminalia amazonia | 0.76 | |
Guyana cedar | Cedrela odorata | 0.39 | 4 |
Guyana ebony | Swartzia leiocalycina | 1 | 4 |
Gwa | Tieghemella heckelii | 0.6 | |
Gyabizito | Pygeum africanum | 0.61 | |
Turraeanthus africanus | 0.51 | ||
Gympie messmate | Eucalyptus cloeziana | 0.8 | |
Haagbeuk | Carpinus betulus | 0.61 | |
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hura crepitans | 0.4 | ||
Hacano | Micropholis guianensis | 0.67 | |
Hackberry | Celtis occidentalis | 0.53 | 1 |
Hackia | Tabebuia serratifolia | 0.99 | 4 |
Larix laricina | 0.53 | ||
Larix occidentalis | 0.52 | ||
Populus balsamifera | 0.34 | ||
Larix occidentalis | 0.52 | ||
Tabebuia serratifolia | 0.99 | ||
Celtis occidentalis | 0.53 | ||
Turraeanthus africanus | 0.51 | ||
Tabebuia serratifolia | 0.99 | ||
Triplochiton scleroxylon | 0.32 | ||
Hagakhak | Dipterocarpus warburgii | 0.53 | |
Hagbuche | Carpinus betulus | 0.61 | |
Hagebuche | Carpinus betulus | 0.61 | |
Turraeanthus africanus | 0.51 | ||
Tabebuia serratifolia | 0.99 | ||
Haiawaballi | Tetragastris altissima | 0.74 | |
Hainbuche | Carpinus betulus | 0.61 | |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Turraeanthus africanus | 0.51 | ||
Halda | Chloroxylon swietenia | 0.88 | |
Haleban | Vitex cofassus | 0.67 | |
Hampas | Koompassia malaccensis | 0.76 | |
Hangilo | Michelia excelsa | 0.42 | |
Hangilo | Michelia sp. | 0.42 | |
Hannoki | Alnus glutinosa | 0.41 | |
Hara | Excoecaria agallocha | 0.42 | |
Betula alleghaniensis | 0.62 | ||
Hard Elm | Ulmus alata | 0.65 | |
Hard Maple | 0.60 | 6 | |
Acer nigrum | 0.57 | ||
Acer saccharum | 0.63 | ||
Pinus echinata | 0.51 | ||
Pinus palustris | 0.59 | ||
Pinus resinosa | 0.46 | ||
Acer nigrum | 0.57 | ||
Hardbeam | Carpinus betulus | 0.61 | |
Hardy catalpa | Catalpa speciosa | 0.37 | |
Acer pseudoplatanus | 0.57 | ||
Hasara | Vitex cofassus | 0.67 | |
Hasi | Excoecaria agallocha | 0.42 | |
Hata | Vitex cofassus | 0.67 | |
Pometia pinnata | 0.6 | ||
Haudan | Eschweilera sagotiana | 0.9 | |
Liquidambar styraciflua | 0.52 | ||
Nyssa aquatica | 0.5 | ||
Liquidambar styraciflua | 0.52 | ||
Picea rubens | 0.4 | ||
Pinus palustris | 0.59 | ||
Populus balsamifera | 0.34 | ||
Heavy Hopea | Hopea iriana | 0.8 | |
Hedge | Maclura pomifera | 0.72 | |
Hedge Apple | Maclura pomifera | 0.72 | |
Hediondo | Piptadeniastrum africanum | 0.63 | |
Hedu | Mitragyna parvifolia | 0.59 | |
Hekakoro | Melanorrhoea spp. | 0.75 | |
Helecho | Grevillea robusta | 0.54 | |
Tsuga canadensis | 0.4 | ||
Tsuga canadensis | 0.4 | ||
Tsuga heterophylla | 0.45 | ||
Hendui | Lophira alata | 0.94 | |
Henduri Poma | Cedrela toona | 0.47 | |
Heng | Dipterocarpus basilanicus | 0.54 | |
Heng | Dipterocarpus grandiflorus | 0.68 | |
Heng | Dipterocarpus warburgii | 0.53 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hicha | Byrsonima coriacea | 0.68 | |
Carya aquatica | 0.62 | ||
Carya cordiformis | 0.66 | ||
Carya illinoensis | 0.66 | ||
Carya lacinosa | 0.69 | ||
Carya myristiciformis | 0.6 | ||
Carya ovata | 0.72 | ||
Carya tomentosa | 0.72 | ||
Hickory boxwood | Planchonella euphlebia | 0.89 | |
Ulmus thomasii | 0.63 | ||
Liriodendron tulipifera | 0.42 | ||
Nyssa aquatica | 0.5 | ||
Hill fukadi | Terminalia amazonia | 0.76 | |
Hill toon | Cedrela serrata | 0.52 | |
Shorea negrosensis | 0.59 | ||
Himalayan cypress | Cupressus torulosa | 0.47 | |
Shorea negrosensis | 0.59 | ||
Hintsy | Intsia palembanica | 0.65 | |
Hintzy | Intsia bijuga | 0.65 | |
Hlafuta | Afzelia quanzensis | 0.62 | |
Hochioo | Tieghemella heckelii | 0.6 | |
Hoeboeballi | Loxopterygium sagotii | 0.62 | |
Triplochiton scleroxylon | 0.32 | ||
Hogberry | Byrsonima coriacea | 0.68 | |
Holia | Byrsonima coriacea | 0.68 | |
Ilex opaca | 0.55 | ||
Hollyhock | Byrsonima coriacea | 0.68 | |
Honduras cedar | Cedrela odorata | 0.39 | 4 |
Swietenia macrophylla | 0.47 | ||
Honduras Pitch Pine | Pinus caribaea | 0.7 | |
Honduras Rosenholz | Dalbergia stevensonii | 0.88 | |
Honduras Rosewood | Dalbergia stevensonii | 0.88 | |
Honeylocust | Gleditsia triacanthos | 0.62 | |
Honge | Bassia latifolia | 0.82 | |
Hoobodia | Anacardium excelsum | 0.33 | |
Hoobooballi | Loxopterygium sagotii | 0.62 | |
Celtis occidentalis | 0.53 | ||
Fraxinus nigra | 0.49 | ||
Hoop Pine | Araucaria cunninghamii | 0.44 | 3 |
Hoop Tree | Melia azedarach | 0.51 | |
Horeni | Cedrela toona | 0.47 | |
Platymiscium pinnatum | 0.87 | ||
Hormiguero | Cordia alliodora | 0.51 | |
Hornbaum | Carpinus betulus | 0.61 | |
Hornbeam | Carpinus betulus | 0.61 | |
Horse Apple | Maclura pomifera | 0.72 | |
Horse Chestnut | Aesculus hippocastanum | 0.39 | |
Horseflesh | Manilkara bidentata | 0.95 | |
Horseflesh Mahogany | Hieronyma alchorneoides | 0.58 | |
Horsetail | Casuarina equisetifolia | 0.87 | |
Horsetail Beefwood | Casuarina equisetifolia | 0.87 | |
Horsetail Casuarina | Casuarina equisetifolia | 0.87 | |
Horsetail Tree | Casuarina equisetifolia | 0.87 | |
Hpang | Mitragyna parvifolia | 0.59 | |
Huacapu | Minquartia guianensis | 0.83 | |
Hububalli | Loxopterygium sagotii | 0.62 | |
Pinus banksiana | 0.43 | ||
Huevos de Gato | Dipterocarpus basilanicus | 0.54 | |
Huevos de Gato | Dipterocarpus grandiflorus | 0.68 | |
Huevos de Gato | Dipterocarpus warburgii | 0.53 | |
Huevos de Gato | Pterocarpus marsupium | 0.71 | 4 |
Huevos de Gato | Pterocarpus vernalis | 0.63 | |
Huhugwe | Brachylaena hutchinsii | 0.85 | |
Huicon | Pouteria izabalensis | 0.64 | |
Huicon | Pouteria pomifera | 0.84 | |
Huilca | Piptadeniastrum africanum | 0.63 | |
Humeg | Pygeum turnerianum | 0.44 | |
Ilex opaca | 0.55 | ||
Fraxinus excelsior | 0.58 | ||
Huntingdon willow | Salix alba | 0.38 | |
Hunug | Pygeum turnerianum | 0.44 | |
Hura | Hura crepitans | 0.40 | 2 |
Hura crepitans | 0.4 | ||
Huragalli | Chloroxylon swietenia | 0.88 | |
Huragatu | Chloroxylon swietenia | 0.88 | |
Tsuga heterophylla | 0.45 | ||
Huruk | Cedrela toona | 0.47 | |
Hutchu Bevu | Melia azedarach | 0.51 | |
Huyam | Pinus merkusii | 0.59 | |
Huynh | Heritiera javanica | 0.65 | |
Huynh | Heritiera ornithocephala | 0.7 | |
Guibourtia ehie | 0.71 | ||
Hyeduanini | Guibourtia ehie | 0.71 | 4 |
Guibourtia ehie | 0.71 | ||
Ias | Excoecaria agallocha | 0.42 | |
Iban | Manilkara zapota | 0.71 | |
Ibeka | Mammea africana | 0.69 | |
Ibelea | Mammea africana | 0.69 | |
Ibira camby | Micropholis guianensis | 0.67 | |
Pometia pinnata | 0.6 | ||
Liquidambar styraciflua | 0.52 | ||
Cedrela odorata | 0.39 | ||
Idabakoror | Mitragyna stipulosa | 0.53 | |
Pinus monticola | 0.35 | ||
Taxus baccata | 0.63 | ||
Idigbo | Terminalia ivorensis | 0.54 | |
Iedel | Mangifera indica | 0.53 | |
Liquidambar styraciflua | 0.52 | ||
Iep | Ulmus hollandica | 0.53 | |
Ifet | Intsia bijuga | 0.65 | |
Ifil | Intsia bijuga | 0.65 | |
Igaganga | Dacryodes le testui | 0.56 | |
Igonde | Brachystegia spiciformis | 0.7 | |
Igondi | Brachystegia spiciformis | 0.7 | |
Pometia pinnata | 0.6 | ||
Ihili | Intsia bijuga | 0.65 | |
Hymenaea courbaril | 0.83 | ||
Ijaws | Terminalia ivorensis | 0.54 | |
Tabebuia serratifolia | 0.99 | ||
Ikame | Pterygota bequaertii | 0.53 | |
Ikame | Pterygota macrocarpa | 0.54 | |
Ikoi | Poga oleosa | 0.39 | |
Ikomba | Musanga cecropioides | 0.23 | |
Iku | Poga oleosa | 0.39 | |
Ikumbu | Musanga cecropioides | 0.23 | |
Ila Evin | Daniella oliveri | 0.49 | |
Ilang-ilang | Canangium odoratum | 0.28 | |
Illupei | Bassia latifolia | 0.82 | |
Illupei | Dichopsis elliptica | 0.56 | |
Iluku | Mitragyna stipulosa | 0.53 | |
Iluli | Khaya nyassica | 0.44 | |
Pterocarpus angolensis | 0.59 | ||
Imbirema | Couratari pulchra | 0.53 | 4 |
Amburana cearensis | 0.58 | ||
Imburana de cheiro | Amburana cearensis | 0.58 | 4 |
Platymiscium pinnatum | 0.87 | ||
Immortel etranger | Spathodea campanulata | 0.25 | |
Imono | Poga oleosa | 0.39 | |
Imonon | Poga oleosa | 0.39 | |
Imonor | Poga oleosa | 0.39 | |
Impa | Pterygota bequaertii | 0.53 | |
Impas | Koompassia malaccensis | 0.76 | |
In | Dipterocarpus basilanicus | 0.54 | |
In | Dipterocarpus warburgii | 0.53 | |
Incense Cedar | Libocedrus decurrens | 0.37 | 1 |
Incenso | Daniella thurifera | 0.46 | |
Incienso | Tetragastris altissima | 0.74 | |
Incorruptible | Minquartia guianensis | 0.83 | |
Indana | Byrsonima coriacea | 0.68 | |
Indana Colorado | Byrsonima coriacea | 0.68 | |
Indano | Byrsonima coriacea | 0.68 | |
Indano Colorado | Byrsonima coriacea | 0.68 | |
India Boxwood | Gossypiospermum praecox | 0.77 | |
Indian Alder | Alnus nepalensis | 0.26 | |
Buxus sempervirens | 0.83 | ||
Indian Cedar | Cedrela toona | 0.47 | |
Indian Chestnut | Castanopsis acuminatissima | 0.56 | |
Indian Cigar Tree | Catalpa speciosa | 0.37 | |
Indian Crabwood | Carapa molluccensis | 0.71 | |
Indian Ebony | Diospyros celebica | 0.9 | 13 |
Indian Ebony | Diospyros melanoxylon | 0.67 | |
Indian Gurjun | Dipterocarpus grandiflorus | 0.68 | |
Indian Laurel | Terminalia elliptica (syn. T. tomentosa) | 0.79 | 16 |
Indian Laurelwood | Terminalia celerica | 0.68 | 4 |
Indian Lilac | Melia azedarach | 0.51 | |
Indian Padauk | Pterocarpus marsupium | 0.71 | 4 |
Pinus taeda | 0.51 | ||
Pterocarpus indicus | 0.57 | ||
Indian Rosewood | Dalbergia latifolia | 0.79 | 2 |
Indian Walnut | Aleurites moluccana | 0.14 | |
Indian White Cedar | Dysoxylum malabaricum | 0.62 | |
Indigbo | Terminalia ivorensis | 0.54 | |
Indo-China Pine | Pinus merkusii | 0.59 | |
Inga Cagtitu | Marmaroxylon racemosum | 1.07 | |
Liquidambar styraciflua | 0.52 | ||
Ingarana | Marmaroxylon racemosum | 1.07 | |
Ingarana da terra firme | Marmaroxylon racemosum | 1.07 | |
Inggeris | Koompassia malaccensis | 0.76 | |
Ingiepipa | Couratari pulchra | 0.53 | 4 |
Ingipipa | Couratari pulchra | 0.53 | 4 |
Ingoe | Cedrela toona | 0.47 | |
Inguipipa | Couratari pulchra | 0.53 | 4 |
Araucaria angustifolia | 0.49 | ||
Taxodium distichum | 0.46 | ||
Pseudotsuga menziesii | 0.48 | ||
Inoi | Poga oleosa | 0.39 | |
Inoi nut | Poga oleosa | 0.39 | |
Inoye | Poga oleosa | 0.39 | |
Pinus radiata | 0.45 | ||
Pinus radiata | 0.45 | ||
Pinus radiata | 0.45 | ||
Pinus radiata | 0.45 | ||
Pseudotsuga menziesii | 0.48 | ||
Intule | Chlorophora excelsa | 0.7 | |
Inyere | Poga oleosa | 0.39 | |
Ipaki | Tieghemella heckelii | 0.6 | |
Ipawhaw | Lophira alata | 0.94 | |
Ipe | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Ipi | Intsia bijuga | 0.65 | |
Ipil | Intsia bijuga | 0.65 | |
Ipil | Intsia palembanica | 0.65 | |
Ipoh | Antiaris toxicaria | 0.35 | |
Ippa | Bassia latifolia | 0.82 | |
Ippa | Dichopsis elliptica | 0.56 | |
Ippi | Dichopsis elliptica | 0.56 | |
Ipus-ipus | Pygeum turnerianum | 0.44 | |
Ira Rosa | Virola koschnyi | 0.51 | |
Iranian Boxwood | Buxus sempervirens | 0.83 | 13 |
Irhu | Bassia latifolia | 0.82 | |
Iriar | Manilkara bidentata | 0.95 | |
Irikwa | Virola surinamensis | 0.51 | |
Iroko | Chlorophora spp. | 0.57 | 2 |
Iroko | Chlorophora regia | 0.59 | |
Iron Wood | Pygeum africanum | 0.61 | |
Iron Wood Tree | Mesua ferrea | 0.92 | |
Ironbark | Eucalyptus dives | 0.68 | |
Ironbark | Eucalyptus hemiphloia | 0.93 | |
Ironbark | Eucalyptus nitens | 0.59 | |
Ironbark | Eucalyptus wilkinsoniana | 0.71 | |
Ironpost | Lophira alata | 0.94 | |
Tabebuia serratifolia | 0.99 | ||
Ostrya virginiana | 0.7 | ||
Ironwood | Tabebuia serratifolia | 0.99 | 4 |
Irpi | Bassia latifolia | 0.82 | |
Irrip | Bassia latifolia | 0.82 | |
Irup | Bassia latifolia | 0.82 | |
Isbin | Afzelia quanzensis | 0.62 | |
Pometia pinnata | 0.6 | ||
Isere | Intsia bijuga | 0.65 | |
Ishpingo | Amburana cearensis | 0.58 | 4 |
Isiqalaba se Hlati | Rapanea melanophleos | 0.74 | |
Isiquaqu | Rapanea melanophleos | 0.74 | |
Isiqwane se Hlati | Rapanea melanophleos | 0.74 | |
Isiqwane-Wehlati | Rapanea melanophleos | 0.74 | |
Isombe | Testulea gabonensis | 0.76 | |
Hymenaea courbaril | 0.83 | ||
Italian Olive Ash | Fraxinus excelsior | 0.58 | 14 |
Itauba | Mezilaurus navalium | 0.79 | |
Itauba Amarella | Mezilaurus navalium | 0.79 | |
Itauba Preta | Mezilaurus navalium | 0.79 | |
Iteballi | Vochysia ferruginea | 0.52 | |
Iteballi | Vochysia guianensis | 0.52 | |
Iteballi | Vochysia lehmanni | 0.52 | |
Iteballi | Vochysia tomentosa | 0.52 | |
Iteballi Korero | Vochysia guianensis | 0.52 | |
Iterballi | Vochysia guianensis | 0.52 | |
Itom Itom | Diospyros mindanaensis | 0.78 | 14 |
Itoumbe | Piptadeniastrum africanum | 0.63 | |
Ivili | Intsia bijuga | 0.65 | |
Guibourtia ehie | 0.71 | ||
Microberlinia brazzavillensis | 0.77 | ||
Izombe | Testulea gabonensis | 0.76 | |
Jaas | Manilkara zapota | 0.71 | |
Jabilla Extranjera | Aleurites moluccana | 0.14 | |
Hura crepitans | 0.4 | ||
Jaboti | Erisma uncinatum | 0.51 | |
Jaboty | Erisma uncinatum | 0.51 | |
Jaboty da Terra Firma | Erisma uncinatum | 0.51 | |
Jacamim | Aspidosperma desmanthum | 0.65 | |
Jacana | Pouteria izabalensis | 0.64 | |
Jacana | Pouteria pomifera | 0.84 | |
Jacaranda | Jacaranda copaia | 0.34 | 4 |
Machaerium villosum | 0.78 | ||
Jacarandaholz | Dalbergia retusa | 0.85 | 4 |
Dalbergia nigra | 0.84 | ||
Jacaranda do brejo | Platymiscium ulei | 0.96 | 14 |
Jacaranda do brejo | Platymiscium yucatanum | 0.96 | 14 |
Machaerium villosum | 0.78 | ||
Machaerium villosum | 0.78 | ||
Machaerium villosum | 0.78 | ||
Jacaranda Para | Machaerium villosum | 0.78 | 13 |
Jacaranda Pardo | Machaerium scleroxylon | 0.78 | 13 |
Machaerium villosum | 0.78 | ||
Machaerium villosum | 0.78 | ||
Machaerium villosum | 0.78 | ||
Jacaranda Rosa | Dalbergia decipularis | 0.87 | 13 |
Dalbergia frutescens | 1.02 | ||
Machaerium villosum | 0.78 | ||
Jacinto | Melia azedarach | 0.51 | |
Jack Pine | Pinus banksiana | 0.43 | 1 |
Pinus contorta | 0.41 | ||
Pometia pinnata | 0.6 | ||
Jaiphal | Aleurites moluccana | 0.14 | |
Jam | Syzygium buettnerianum | 0.73 | |
Jamaica Mahogany | Sickingia salvadorense | 0.65 | |
Jamaica Mahogany | Swietenia mahagoni | 0.57 | |
Jamaican Cedar | Cedrela odorata | 0.39 | 4 |
Jamar | Anisoptera costata | 0.52 | |
Jambire | Millettia stuhlmannii | 0.83 | 13 |
Pometia pinnata | 0.6 | ||
Jangkang | Hopea odorata | 0.63 | |
Japan Camphor Tree | Cinnamomum camphora | 0.38 | |
Japanese Alder | Alnus glutinosa | 0.41 | |
Japanese Ash | Fraxinus mandshurica | 0.63 | |
Japanese Beech | Fagus sylvatica | 0.67 | 13 |
Buxus sempervirens | 0.83 | ||
Japanese Camphor | Cinnamomum camphora | 0.38 | |
Japanese Cedar | Cryptomeria japonica | 0.36 | |
Japanese Larch | Larix leptolepis | 0.49 | |
Japanese Maple | Acer palmatum | 0.54 | |
Japanese oak | Quercus mongolica | 0.64 | |
Japanese Zelkova | Zelkova serrata | 0.6 | |
Jarana | Eschweilera sagotiana | 0.9 | |
Jarrah | Eucalyptus marginata | 0.75 | 2 |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Jatoba | Hymenaea courbaril | 0.83 | 16 |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Jaune | Mezilaurus navalium | 0.79 | |
Jaune d'Oeuf | Pouteria izabalensis | 0.64 | |
Jaune d'Oeuf | Pouteria pomifera | 0.84 | |
Hura crepitans | 0.4 | ||
Jega | Manilkara zapota | 0.71 | |
Jelutong | Dyera costulata | 0.38 | 2 |
Jelutong | Kibatalia arborea | 0.38 | 14 |
Jempinis | Melia azedarach | 0.51 | |
Hymenaea courbaril | 0.83 | ||
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Jersey Pine | Pinus caribaea | 0.7 | |
Jersey Pine | Pinus insularis | 0.5 | |
Pinus virginiana | 0.48 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Jewalidanni | Minquartia guianensis | 0.83 | |
Jia | Gossypiospermum praecox | 0.77 | |
Jia de monte | Gossypiospermum praecox | 0.77 | |
Jiga | Manilkara zapota | 0.71 | |
Astronium graveolens | 0.89 | ||
Astronium graveolens | 0.8 | ||
Joeliballi Tataroe | Tetragastris altissima | 0.74 | |
Jondo | Piptadeniastrum africanum | 0.63 | |
Jucarillo | Terminalia guyanensis | 0.6 | |
Hymenaea courbaril | 0.83 | ||
Juma | Musanga cecropioides | 0.23 | |
Jumit | Heritiera javanica | 0.65 | |
Juna | Musanga cecropioides | 0.23 | |
Juniperus virginiana | 0.47 | ||
Pinus banksiana | 0.43 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Ka | Campnosperma brevipetiolata | 0.33 | |
Ka Ronko | Terminalia ivorensis | 0.54 | |
Ka Thang Han | Calophyllum inophyllum | 0.55 | |
Ka Thang Han | Calophyllum tomentosum | 0.59 | |
Ka Thang Lan | Calophyllum inophyllum | 0.55 | |
Ka Thang Lan | Calophyllum tomentosum | 0.59 | |
Kaapse Boekenhout | Rapanea melanophleos | 0.74 | |
Ka-Ar | Vitex cofassus | 0.67 | |
Kabaak Khok | Anisoptera costata | 0.52 | |
Kabaak Thong | Anisoptera curtisii | 0.52 | |
Kaban | Anisoptera costata | 0.52 | |
Kaban Kaunghmu | Anisoptera costata | 0.52 | |
Kaban Kaunghmu | Anisoptera curtisii | 0.52 | |
Kaban-Kaunghmu | Anisoptera curtisii | 0.52 | |
Ka-Bari | Piptadeniastrum africanum | 0.63 | |
Kaboing | Intsia bijuga | 0.65 | |
Pometia pinnata | 0.6 | ||
Kabol | Xanthophyllum excelsum | 0.67 | |
Kachein | Melia azedarach | 0.51 | |
Kadamb | Mitragyna parvifolia | 0.59 | |
Kadani | Mitragyna parvifolia | 0.59 | |
Kaddam | Mitragyna parvifolia | 0.59 | |
Kadiala | Mitragyna parvifolia | 0.59 | |
Kadir | Erythrophloeum densiflorum | 0.68 | |
Kadwar | Mitragyna parvifolia | 0.59 | |
Kaem | Mitragyna parvifolia | 0.59 | |
Kagu Pengiran | Anisoptera curtisii | 0.52 | |
Kaikumba | Mammea africana | 0.69 | |
Kaim | Mitragyna parvifolia | 0.59 | |
Kaitana | Zanthoxylum rhetsa | 0.56 | |
Pterocarpus angolensis | 0.59 | ||
Kajanna Manja | Mangifera indica | 0.53 | |
Pterocarpus angolensis | 0.59 | ||
Pterocarpus angolensis | 0.59 | ||
Kajoe Besi | Intsia bijuga | 0.65 | |
Pometia pinnata | 0.6 | ||
Kajoewaballi | Catostemma fragrans | 0.66 | |
Kakan | Anisoptera costata | 0.52 | |
Hymenaea courbaril | 0.83 | ||
Kakaralli | Eschweilera sagotiana | 0.9 | |
Diospyros ebenum | 0.94 | ||
Kakende | Pterygota bequaertii | 0.53 | |
Kakende | Pterygota macrocarpa | 0.54 | |
Kakeralli | Eschweilera sagotiana | 0.9 | |
Turraeanthus africanus | 0.51 | ||
Kaku | Lophira alata | 0.94 | |
Kalai | Albizia procera | 0.55 | |
Kalam | Mitragyna parvifolia | 0.59 | |
Kalamansanai | Anisoptera curtisii | 0.52 | |
Kalamatau | Erythrophloeum densiflorum | 0.68 | |
Pometia pinnata | 0.6 | ||
Kalampe | Heritiera javanica | 0.65 | |
Cedrela odorata | 0.39 | ||
Shorea negrosensis | 0.59 | ||
Kalek | Syzygium buettnerianum | 0.73 | |
Kaleli | Aleurites moluccana | 0.14 | |
Kali | Aningeria altissima | 0.42 | |
Kali | Aningeria dombeyi | 0.39 | |
Kali | Aningeria robusta | 0.42 | |
Shorea negrosensis | 0.59 | ||
Kaliba | Musanga cecropioides | 0.23 | |
Kalingag | Cinnamomum camphora | 0.38 | |
Kalkilingi | Cedrela toona | 0.47 | |
Kallain | Cupressus torulosa | 0.47 | |
Kallam | Mitragyna parvifolia | 0.59 | |
Kalm | Mitragyna parvifolia | 0.59 | |
Kalumanog | Koordersiodendron pinnatum | 0.71 | |
Kalumpang Asok | Heritiera javanica | 0.65 | |
Kamagong | Diospyros ebenaster | 0.61 | 4 |
Kamagong | Diospyros inclusa | 0.7 | 14 |
Kamagong | Diospyros melanoxylon | 0.67 | |
Kamagong | Diospyros mindanaensis | 0.78 | 14 |
Kamagong | Diospyros pyrrhocarpa | 0.69 | 14 |
Kamashi | Staudtia stipitata | 0.79 | |
Kamassi | Gonioma kamassi | 0.85 | |
Kamassi Boxwood | Gonioma kamassi | 0.85 | |
Kamassie | Gonioma kamassi | 0.85 | |
Kamassihout | Gonioma kamassi | 0.85 | |
Kamatana | Catostemma fragrans | 0.66 | |
Kamatog | Erythrophloeum densiflorum | 0.68 | |
Kamba | Mitragyna parvifolia | 0.59 | |
Kambala | Chlorophora excelsa | 0.7 | |
Kambala | Chlorophora regia | 0.59 | |
Kambli | Mitragyna parvifolia | 0.59 | |
Kamere | Aleurites moluccana | 0.14 | |
Kamieh | Aleurites moluccana | 0.14 | |
Kamiri | Aleurites moluccana | 0.14 | |
Kampas | Koompassia malaccensis | 0.76 | |
Kan Ki | Hopea odorata | 0.63 | |
Kana Pila | Artocarpus hirsuta | 0.52 | |
Kanda | Beilschmiedia mannii | 0.62 | |
Kandalanga | Carapa molluccensis | 0.71 | |
Kaneelhout | Mezilaurus navalium | 0.79 | |
Kaneerjoe | Mezilaurus navalium | 0.79 | |
Kanela | Pygeum turnerianum | 0.44 | |
Kangei | Mitragyna parvifolia | 0.59 | |
Pometia pinnata | 0.6 | ||
Kangit | Mangifera indica | 0.53 | |
Kangkangum | Xanthophyllum excelsum | 0.67 | |
Kanit | Mangifera indica | 0.53 | |
Kaniwi | Aglaia gigantea | 0.54 | |
Kankate | Morus mesozygia | 0.71 | |
Kanoaballi | Byrsonima coriacea | 0.68 | |
Kanran | Diospyros ebenaster | 0.61 | 4 |
Kanran | Diospyros mindanaensis | 0.78 | 14 |
Kansayud | Aglaia gigantea | 0.54 | |
Kansiopi | Anisoptera costata | 0.52 | |
Kansulud | Aglaia gigantea | 0.54 | |
Kantingen | Koordersiodendron pinnatum | 0.71 | |
Kanu | Mitragyna parvifolia | 0.59 | |
Kanumog | Pygeum turnerianum | 0.44 | |
Kanzaw | Bassia latifolia | 0.82 | |
Kanze | Heritiera javanica | 0.65 | |
Kanze | Heritiera ornithocephala | 0.7 | |
Khaya nyassica | 0.44 | ||
Kapere | Cedrela huberi | 0.4 | 4 |
Kapere | Cedrela odorata | 0.39 | 4 |
Kapere | Cedrela toona | 0.47 | |
Kapur | Dryobalanops lanceolata | 0.69 | |
Kapur | Dryobalanops spp. | 0.70 | 2 |
Kaputu | Brachystegia spiciformis | 0.7 | |
Karaal | Albizia procera | 0.55 | |
Karail | Albizia procera | 0.55 | |
Karakong | Balanocarpus heimii | 0.78 | |
Karamatsu | Larix leptolepis | 0.49 | |
Kara-Matsu | Larix leptolepis | 0.49 | |
Karamb | Mitragyna parvifolia | 0.59 | |
Pometia pinnata | 0.6 | ||
Kararo | Aningeria altissima | 0.42 | |
Kararo | Aningeria dombeyi | 0.39 | |
Kararo | Aningeria robusta | 0.42 | |
Diospyros ebenum | 0.94 | ||
Terminalia superba | 0.4 | ||
Karhar | Albizia procera | 0.55 | |
Karikowa | Iryanthera spp. | 0.58 | |
Diospyros ebenum | 0.94 | ||
Karimari | Campnosperma brevipetiolata | 0.33 | |
Karmi | Mitragyna parvifolia | 0.59 | |
Karogkog | Koordersiodendron pinnatum | 0.71 | |
Karri | Eucalyptus diversicolor | 0.79 | 10 |
Pometia pinnata | 0.6 | ||
Prioria copaifera | 0.42 | ||
Diospyros ebenum | 0.94 | ||
Diospyros ebenum | 0.94 | ||
Diospyros ebenum | 0.94 | ||
Hymenaea courbaril | 0.83 | ||
Kasabang | Zanthoxylum rhetsa | 0.56 | |
Kasai | Albizia procera | 0.55 | |
Kasai | Pometia pinnata | 0.60 | 4 |
Kasai | Pometia tomentosa | 0.59 | |
Kasai Sibu | Pometia pinnata | 0.6 | 4 |
Pometia pinnata | 0.6 | ||
Pometia pinnata | 0.6 | ||
Kashitka | Cedrela toona | 0.47 | |
Kasrike | Casuarina equisetifolia | 0.87 | |
Kat illippi | Bassia latifolia | 0.82 | |
Kat illupai | Bassia latifolia | 0.82 | |
Kat illupei | Dichopsis elliptica | 0.56 | |
Katangai | Cedrela toona | 0.47 | |
Katmon | Dillenia luzoniensis | 0.65 | |
Katmon | Dillenia pentagyna | 0.55 | |
Katonde | Vitex cofassus | 0.67 | |
Katondeng | Vitex cofassus | 0.67 | |
Katong Matsin | Chisocheton pentandrus | 0.53 | |
Katpila | Artocarpus hirsuta | 0.52 | |
Kattadi | Casuarina equisetifolia | 0.87 | |
Katum Kao | Neonauclea calycinia | 0.79 | |
Kaudamu | Myristica buchneriana | 0.41 | |
Kaudamu | Myristica chartacea | 0.48 | |
Kaudamu | Myristica hypargyraea | 0.44 | |
Kaudamu | Myristica sp. | 0.54 | |
Kaula | Machilus odoratissima | 0.59 | |
Pometia pinnata | 0.6 | ||
Kaunghmu | Anisoptera cochinchinensis | 0.52 | |
Kaunghmu | Anisoptera costata | 0.52 | |
Kaunghmu | Anisoptera curtisii | 0.52 | |
Kaunghmu | Anisoptera laevis | 0.44 | |
Kaunghmu | Anisoptera thurifera | 0.52 | |
Kauri | Agathis borneensis | 0.41 | |
Kauri | Agathis philippinensis | 0.33 | |
Kauri Agathis | Agathis borneensis | 0.41 | |
Kauri Pine | Agathis borneensis | 0.41 | |
Kauri Pine | Agathis philippinensis | 0.33 | |
Kauvula | Endospermum macrophyllum | 0.41 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Kawang | Hopea odorata | 0.63 | |
Kawilia | Grevillea robusta | 0.54 | |
Kawiloe | Aleurites moluccana | 0.14 | |
Kawtanok | Mesua ferrea | 0.92 | |
Kaya Arang | Diospyros ebenaster | 0.61 | 4 |
Kaya Arang | Diospyros inclusa | 0.7 | 14 |
Kaya Arang | Diospyros melanoxylon | 0.67 | |
Kaya Arang | Diospyros mindanaensis | 0.78 | 14 |
Kaya Arang | Diospyros pyrrhocarpa | 0.69 | 14 |
Pometia pinnata | 0.6 | ||
Kayaw | Excoecaria agallocha | 0.42 | |
Kaye Hujan | Tetramerista glabra | 0.73 | |
Kayetana | Zanthoxylum rhetsa | 0.56 | |
Kayu | Cinnamomum camphora | 0.38 | |
Kayu | Excoecaria agallocha | 0.42 | |
Kayu Batu | Koompassia malaccensis | 0.76 | |
Kayu Besi | Intsia bijuga | 0.65 | |
Kayu Malam | Diospyros ebenaster | 0.61 | 4 |
Kayu Malam | Diospyros inclusa | 0.7 | 14 |
Kayu Malam | Diospyros melanoxylon | 0.67 | |
Kayu Malam | Diospyros mindanaensis | 0.78 | 14 |
Kayu Malam | Diospyros pyrrhocarpa | 0.69 | 14 |
Kayu Raja | Koompassia excelsa | 0.75 | |
Kayu Rajah | Koompassia excelsa | 0.75 | |
Kayu Sala | Pinus merkusii | 0.59 | |
Kayu Sugi | Pinus merkusii | 0.59 | |
Kayutana | Zanthoxylum rhetsa | 0.56 | |
K'deng | Lophira alata | 0.94 | |
Keaki | Zelkova serrata | 0.6 | |
Pometia pinnata | 0.6 | ||
Kebuk | Intsia bijuga | 0.65 | |
Kebuni | Morus mesozygia | 0.71 | |
Kechi Lebet | Mitragyna stipulosa | 0.53 | |
Kedao | Anisoptera costata | 0.52 | |
Kedemoet | Hopea odorata | 0.63 | |
Keega | Irvingia gabonensis | 0.76 | |
Kefe | Pterygota bequaertii | 0.53 | |
Kefe | Pterygota macrocarpa | 0.54 | |
Terminalia superba | 0.4 | ||
Kehngid | Mangifera indica | 0.53 | |
Kei Pala | Dichopsis elliptica | 0.56 | |
Keim | Mitragyna parvifolia | 0.59 | |
Pterocarpus angolensis | 0.59 | ||
Kekange | Terminalia ivorensis | 0.54 | |
Kekrefunde | Lophira alata | 0.94 | |
Keladan | Dryobalanops lanceolata | 0.69 | |
Kelat | Syzygium buettnerianum | 0.73 | |
Keledang | Artocarpus hirsuta | 0.52 | |
Kelel A Charm | Campnosperma brevipetiolata | 0.33 | |
Kelela Charm | Campnosperma brevipetiolata | 0.33 | |
Kelinting | Campnosperma brevipetiolata | 0.33 | |
Quercus kelloggii | 0.53 | ||
Kelo | Intsia bijuga | 0.65 | |
Kembang | Heritiera javanica | 0.65 | |
Kembiri | Aleurites moluccana | 0.14 | |
Kemel | Melia azedarach | 0.51 | |
Kemeri | Aleurites moluccana | 0.14 | |
Kemili | Aleurites moluccana | 0.14 | |
Kemiling | Aleurites moluccana | 0.14 | |
Keminting | Aleurites moluccana | 0.14 | |
Kemiri | Aleurites moluccana | 0.14 | |
Kempas | Koompassia malaccensis | 0.76 | |
Kempas Angin | Koompassia malaccensis | 0.76 | |
Kempas Rawang | Koompassia malaccensis | 0.76 | |
Kempu Gandagheri | Cedrela toona | 0.47 | |
Kemunyau | Heritiera javanica | 0.65 | |
Kemwiri | Aleurites moluccana | 0.14 | |
Ken | Hopea odorata | 0.63 | |
Betula papyrifera | 0.55 | ||
Betula papyrifera | 0.55 | ||
Kenanga | Canangium odoratum | 0.28 | |
Diospyros ebenum | 0.94 | ||
Kentucky Coffeetree | Gymnocladus dioicus | 0.4 | |
Kentucky Mahogany | Gymnocladus dioicus | 0.4 | |
Kenyau | Anisoptera costata | 0.52 | |
Kepayang | Neonauclea calycinia | 0.79 | |
Keralm | Campnosperma brevipetiolata | 0.33 | |
Kereh | Aleurites moluccana | 0.14 | |
Kermiri | Aleurites moluccana | 0.14 | |
Kers | Prunus avium | 0.58 | 13 |
Keruing | Dipterocarpus grandiflorus | 0.68 | |
Keruing | Dipterocarpus spp. | 0.76 | 2 |
Keruing Kuching | Anisoptera curtisii | 0.52 | |
Keruing Kucing | Anisoptera curtisii | 0.52 | |
Kesaramu | Mesua ferrea | 0.92 | |
Kesse | Morus mesozygia | 0.71 | |
Kete | Planchonella euphlebia | 0.89 | |
Ketimpun | Anisoptera costata | 0.52 | |
Keyaki | Zelkova serrata | 0.6 | |
Khacho | Millettia pendula | 0.87 | |
Khaen | Hopea odorata | 0.63 | |
Khan Thong | Swintonia sp. | 0.62 | |
Kharpat | Garuga pinnata | 0.51 | |
Khasi Pine | Pinus insularis | 0.5 | |
Khaso | Pinus insularis | 0.5 | |
Khasya Pine | Pinus insularis | 0.5 | |
Khen | Hopea odorata | 0.63 | |
Khen Hua | Hopea odorata | 0.63 | |
Khengkhriwakbik | Grewia elastica | 0.63 | |
Khinam | Cedrela serrata | 0.52 | |
Khishing | Cedrela serrata | 0.52 | |
Ki Beureum | Cedrela toona | 0.47 | |
Pterocarpus angolensis | 0.59 | ||
Pometia pinnata | 0.6 | ||
Kiantioutiou | Aspidosperma desmanthum | 0.65 | |
Pterocarpus angolensis | 0.59 | ||
Kibibi | Berlinia acuminata | 0.64 | |
Millettia laurentii | 0.81 | ||
Kideng | Diplodiscus paniculatus | 0.62 | |
Kigere | Musanga cecropioides | 0.23 | |
Kil | Terminalia amazonia | 0.76 | |
Kil | Terminalia arjuna | 0.71 | |
Kil | Terminalia ivorensis | 0.54 | |
Kil | Terminalia procera | 0.54 | |
Shorea negrosensis | 0.59 | ||
Kilikowa | Virola surinamensis | 0.51 | |
Kilkova | Zelkova serrata | 0.6 | |
Killu Sisa | Vochysia ferruginea | 0.52 | |
Killu Sisa | Vochysia guianensis | 0.52 | |
Kilu-Sisa | Vochysia guianensis | 0.52 | |
Kimeyong | Heritiera javanica | 0.65 | |
Kimurumba | Chlorophora excelsa | 0.7 | |
King Tree | Mora excelsa | 0.89 | |
Carya lacinosa | 0.69 | ||
Kingue | Bombax brevicuspe | 0.35 | |
Kingwood | Dalbergia cearensis | 1.16 | 16 |
Kipapa | Afzelia quanzensis | 0.62 | |
Kipoleng | Heritiera javanica | 0.65 | |
Kipugupugu | Brachylaena hutchinsii | 0.85 | |
Kirikawa | Iryanthera spp. | 0.58 | |
Pometia pinnata | 0.6 | ||
Kirsche | Prunus avium | 0.58 | 13 |
Kirundu | Antiaris toxicaria | 0.35 | |
Turraeanthus africanus | 0.51 | ||
Pterocarpus soyauxii | 0.64 | ||
Pterocarpus soyauxii | 0.64 | ||
Kitola | Oxystigma oxyphyllum | 0.53 | |
Kiu | Campnosperma brevipetiolata | 0.33 | |
Kivili | Intsia bijuga | 0.65 | |
Kjanarie | Mezilaurus navalium | 0.79 | |
Kjarie | Mezilaurus navalium | 0.79 | |
K-Kuperb | Piptadeniastrum africanum | 0.63 | |
Klibbal | Alnus glutinosa | 0.41 | |
Knicker tree | Gymnocladus dioicus | 0.4 | |
Pinus contorta | 0.41 | ||
Pinus ponderosa | 0.4 | ||
Knysna | Gonioma kamassi | 0.85 | |
Knysna boxwood | Gonioma kamassi | 0.85 | |
Ko Ki | Hopea odorata | 0.63 | |
Koa | Acacia koa | 0.63 | 13 |
Kobero | Manilkara bidentata | 0.95 | |
Kodanji | Polyalthia fragans | 0.46 | |
Kodanyi | Polyalthia fragans | 0.46 | |
Koe | Alnus nepalensis | 0.26 | |
Koeipjarie | Loxopterygium sagotii | 0.62 | |
Koemaroe | Dipteryx odorata | 0.82 | |
Platymiscium pinnatum | 0.87 | ||
Pometia pinnata | 0.6 | ||
Pometia pinnata | 0.6 | ||
Koes | Micropholis guianensis | 0.67 | |
Koesiri Balatarie | Micropholis guianensis | 0.67 | |
Triplochiton scleroxylon | 0.32 | ||
Kofo | Mitragyna stipulosa | 0.53 | |
Kohi | Alnus nepalensis | 0.26 | |
Pometia pinnata | 0.6 | ||
Terminalia superba | 0.4 | ||
Terminalia superba | 0.4 | ||
Kokadaka | Anisoptera costata | 0.52 | |
Kokango | Terminalia ivorensis | 0.54 | |
Kokank | Lophira alata | 0.94 | |
Koki | Hopea iriana | 0.8 | |
Koki | Hopea odorata | 0.63 | |
Koki Mosau | Hopea odorata | 0.63 | |
Koki Thmar | Hopea odorata | 0.63 | |
Kokko | Albizia lebbeck | 0.54 | 3 |
Kokko | Albizia procera | 0.55 | |
Kokopaie | Erisma uncinatum | 0.51 | |
Terminalia superba | 0.4 | ||
Liquidambar styraciflua | 0.52 | ||
Liquidambar styraciflua | 0.52 | ||
Komatti | Excoecaria agallocha | 0.42 | |
Komba | Mitragyna parvifolia | 0.59 | |
Komere | Aleurites moluccana | 0.14 | |
Kompas | Koompassia malaccensis | 0.76 | |
Tabebuia serratifolia | 0.99 | ||
Kondroti | Bombax brevicuspe | 0.35 | |
Kondroti | Bombax chevalieri | 0.51 | |
Terminalia superba | 0.4 | ||
Kong | Balanocarpus heimii | 0.78 | |
Pometia pinnata | 0.6 | ||
Terminalia superba | 0.4 | ||
Konhout | Minquartia guianensis | 0.83 | |
Konoo-Findo | Tieghemella heckelii | 0.6 | |
Konthout | Minquartia guianensis | 0.83 | |
Kooel Pialli | Loxopterygium sagotii | 0.62 | |
Kooroobooelli | Peltogyne porphyrocardia | 0.69 | |
Kooroobovelli | Peltogyne porphyrocardia | 0.69 | |
Cedrela odorata | 0.39 | ||
Kora | Anisoptera costata | 0.52 | |
Terminalia superba | 0.4 | ||
Korob | Manilkara zapota | 0.71 | |
Koroboreli | Peltogyne porphyrocardia | 0.69 | |
Koroboreli | Peltogyne venosa | 0.69 | |
Koroborelli | Peltogyne porphyrocardia | 0.69 | |
Koroborezi | Peltogyne venosa | 0.69 | |
Koron Paku | Catostemma fragrans | 0.66 | |
Kosau | Isoberlinia doka | 0.63 | |
Terminalia superba | 0.4 | ||
Koto | Pterygota bequaertii | 0.53 | |
Koto | Pterygota macrocarpa | 0.54 | |
Kotublassu | Lophira alata | 0.94 | |
Kouali | Qualea albiflora | 0.54 | |
Kouali | Qualea paraensis | 0.58 | |
Kouali | Vochysia ferruginea | 0.52 | |
Kouali | Vochysia guianensis | 0.52 | |
Kouali | Vochysia lehmanni | 0.52 | |
Kouali | Vochysia tomentosa | 0.52 | |
Kouburelli | Peltogyne porphyrocardia | 0.69 | |
Koul | Mansonia altissima | 0.55 | |
Pterocarpus soyauxii | 0.64 | ||
Koumanti Oudou | Aspidosperma desmanthum | 0.65 | |
Koungou | Piptadeniastrum africanum | 0.63 | |
Kowa | Terminalia arjuna | 0.71 | |
Kowal | Alnus nepalensis | 0.26 | |
Pometia pinnata | 0.6 | ||
Kpa | Beilschmiedia mannii | 0.62 | |
Triplochiton scleroxylon | 0.32 | ||
Kpeh | Irvingia gabonensis | 0.76 | |
Kpele | Irvingia gabonensis | 0.76 | |
Kpendei | Afzelia bipindensis | 0.62 | |
Kpendei | Afzelia pachyloba | 0.62 | |
Kpoo | Mitragyna stipulosa | 0.53 | |
Kpowo | Mitragyna stipulosa | 0.53 | |
Krabaak | Anisoptera curtisii | 0.52 | |
Krabaak Daeng | Anisoptera curtisii | 0.52 | |
Krabaak Thong | Anisoptera curtisii | 0.52 | |
Krabak | Anisoptera costata | 0.52 | |
Krabak | Anisoptera curtisii | 0.52 | |
Kra-Bak | Anisoptera costata | 0.52 | |
Krabak Daeng | Anisoptera costata | 0.52 | |
Krabak Dam | Anisoptera costata | 0.52 | |
Krabak Thong | Anisoptera curtisii | 0.52 | |
Krakas Prek | Intsia bijuga | 0.65 | |
Krammal | Populus ciliata | 0.37 | |
Pometia pinnata | 0.6 | ||
Krishing | Cedrela serrata | 0.52 | |
Kromanti | Aspidosperma desmanthum | 0.65 | |
Pometia pinnata | 0.6 | ||
Kuantan | Tetramerista glabra | 0.73 | |
Kuasi | Podocarpus neriifolia | 0.48 | |
Kuba Mahogany | Swietenia mahagoni | 0.57 | |
Kubok | Intsia bijuga | 0.65 | |
Kubuk | Intsia bijuga | 0.65 | |
Kudwal | Mitragyna parvifolia | 0.59 | |
Shorea negrosensis | 0.59 | ||
Pometia pinnata | 0.6 | ||
Kujya | Cedrela toona | 0.47 | |
Kukui | Aleurites moluccana | 0.14 | |
Kukuo | Diospyros ebenaster | 0.61 | 4 |
Kukuo | Diospyros mindanaensis | 0.78 | 14 |
Shorea negrosensis | 0.59 | ||
Kulim Papa | Vitex cofassus | 0.67 | |
Kulim Papa | Vitex parviflora | 0.68 | |
Kuling-Babui | Dysoxylum euphlebium | 0.63 | |
Kulm | Mitragyna parvifolia | 0.59 | |
Kumaru | Dipteryx odorata | 0.82 | |
Kumbuk | Terminalia arjuna | 0.71 | |
Kumiri | Aleurites moluccana | 0.14 | |
Terminalia superba | 0.4 | ||
Kumpang | Myristica buchneriana | 0.41 | |
Kumpang | Myristica chartacea | 0.48 | |
Kumpang | Myristica hypargyraea | 0.44 | |
Kumpang | Myristica sp. | 0.54 | |
Kumpas | Koompassia malaccensis | 0.76 | |
Kumra | Mitragyna parvifolia | 0.59 | |
Kunch | Alnus nepalensis | 0.26 | |
Kung | Terminalia amazonia | 0.76 | |
Kung | Terminalia arjuna | 0.71 | |
Kung | Terminalia ivorensis | 0.54 | |
Kung | Terminalia procera | 0.54 | |
Pometia pinnata | 0.6 | ||
Kunis | Alnus nepalensis | 0.26 | |
Kunsun | Grewia elastica | 0.63 | |
Kuntz | Alnus nepalensis | 0.26 | |
Kunu | Lophira alata | 0.94 | |
Kunukwa | Pygeum africanum | 0.61 | |
Kuraburelli | Peltogyne porphyrocardia | 0.69 | |
Cedrela odorata | 0.39 | ||
Cedrela odorata | 0.39 | ||
Kuren | Intsia bijuga | 0.65 | |
Kuruburelli | Peltogyne porphyrocardia | 0.69 | |
Kuruburelli | Peltogyne venosa | 0.69 | |
Kuruk | Cedrela toona | 0.47 | |
Kurum | Mitragyna parvifolia | 0.59 | |
Kusonoki | Cinnamomum camphora | 0.38 | |
Kutebi | Mitragyna parvifolia | 0.59 | |
Araucaria angustifolia | 0.49 | ||
Turraeanthus africanus | 0.51 | ||
Kwai | Terminalia amazonia | 0.76 | |
Hymenaea courbaril | 0.83 | ||
Hymenaea courbaril | 0.83 | ||
Kwari | Vochysia ferruginea | 0.52 | |
Kwari | Vochysia guianensis | 0.52 | |
Kwari | Vochysia lehmanni | 0.52 | |
Kwari | Vochysia tomentosa | 0.52 | |
Kwarie | Byrsonima coriacea | 0.68 | |
Kwateri | Eschweilera sagotiana | 0.9 | |
Kwatru | Eschweilera sagotiana | 0.9 | |
Kwila | Intsia bijuga | 0.65 | |
Kwila | Intsia palembanica | 0.65 | |
Kwintofi | Beilschmiedia mannii | 0.62 | |
Kwipariye | Loxopterygium sagotii | 0.62 | |
Kwo-Kwo | Mitragyna stipulosa | 0.53 | |
Kyere | Lophira alata | 0.94 | |
Kyere | Pterygota bequaertii | 0.53 | |
Kyere | Pterygota macrocarpa | 0.54 | |
Kyeto | Vitex cofassus | 0.67 | |
Kyirafunti | Lophira alata | 0.94 | |
Kyirebente | Lophira alata | 0.94 | |
Labi | Beilschmiedia mannii | 0.62 | |
Labri | Morus alba | 0.6 | |
Lacewood | Grevillea robusta | 0.54 | |
Lacewood | Platanus hybrida | 0.59 | |
Platanus occidentalis | 0.49 | ||
Lacre de Bajo | Tetragastris altissima | 0.74 | |
Lacreiro | Qualea paraensis | 0.58 | |
Ladet | Cedrela toona | 0.47 | |
Lagan | Dipterocarpus basilanicus | 0.54 | |
Lagan | Dipterocarpus grandiflorus | 0.68 | |
Lagan | Dipterocarpus warburgii | 0.53 | |
Shorea negrosensis | 0.59 | ||
Lago | Pygeum turnerianum | 0.44 | |
Lagunero | Dipterocarpus basilanicus | 0.54 | |
Lagunero | Dipterocarpus grandiflorus | 0.68 | |
Lagunero | Dipterocarpus warburgii | 0.53 | |
Lagunero | Pterocarpus marsupium | 0.71 | 4 |
Lagunero | Pterocarpus vernalis | 0.63 | |
Laguno | Vochysia lehmanni | 0.52 | |
Laguno | Vochysia tomentosa | 0.52 | |
Laiman-Phang | Grewia elastica | 0.63 | |
Lakolako | Koordersiodendron pinnatum | 0.71 | |
Lakuch | Artocarpus hirsuta | 0.52 | |
Lamio | Dracontomelon edule | 0.44 | |
Lamoa | Melia azedarach | 0.51 | |
Lamog | Planchonia papuana | 0.61 | |
Lamong | Planchonia papuana | 0.61 | |
Lampati | Duabanga sonneratioides | 0.37 | |
Lamphu | Duabanga sonneratioides | 0.37 | |
Lanan | Shorea leptoclados | 0.38 | 4 |
Lanan | Shorea smithiana | 0.43 | 4 |
Terminalia superba | 0.4 | ||
Landin | Podocarpus guatemalensis | 0.54 | |
Landin | Podocarpus neriifolia | 0.48 | |
Landojan | Aningeria altissima | 0.42 | |
Landojan | Aningeria dombeyi | 0.39 | |
Landojan | Aningeria robusta | 0.42 | |
Landosan | Aningeria altissima | 0.42 | |
Landosan | Aningeria dombeyi | 0.39 | |
Landosan | Aningeria robusta | 0.42 | |
Pometia pinnata | 0.6 | ||
Pometia pinnata | 0.6 | ||
Langbian pine | Pinus insularis | 0.5 | |
Langbian Three-Leaved Pine | Pinus insularis | 0.5 | |
Pometia pinnata | 0.6 | ||
Lanutan-Bagio | Gonystylus macrophyllum | 0.54 | |
Lanutan-Bagyo | Gonystylus macrophyllum | 0.54 | |
Tabebuia serratifolia | 0.99 | ||
Lapacho | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Tabebuia serratifolia | 0.99 | ||
Lapacho Negro | Tabebuia serratifolia | 0.99 | 4 |
Tabebuia serratifolia | 0.99 | ||
Triplochiton scleroxylon | 0.32 | ||
Abies amabilis | 0.43 | ||
Abies grandis | 0.37 | ||
Larix laricina | 0.53 | ||
Larix occidentalis | 0.52 | ||
Larel de costa | Cordia alliodora | 0.51 | |
Large false mopane | Guibourtia coleosperma | 0.66 | |
Swietenia macrophylla | 0.47 | ||
Swietenia macrophylla | 0.47 | ||
Lark | Larix decidua | 0.48 | 14 |
Larut | Tetramerista glabra | 0.73 | |
Lasila | Lagerstroemia piriformis | 0.67 | |
Lasilak | Lagerstroemia piriformis | 0.67 | |
Lastan | Peltogyne porphyrocardia | 0.69 | |
Lastan | Peltogyne venosa | 0.69 | |
Latag | Xanthophyllum excelsum | 0.67 | |
Latareko | Gonystylus macrophyllum | 0.54 | |
Nyssa sylvatica | 0.5 | ||
Lau Tau | Tarrietia sylvatica | 0.82 | |
Shorea negrosensis | 0.59 | ||
Shorea negrosensis | 0.59 | ||
Shorea negrosensis | 0.59 | ||
Shorea negrosensis | 0.59 | ||