Remember when relative humidity (RH) test readings under the ASTM F2170 standard required a 72-hour waiting period? Not anymore. The 72-hour wait is history. The standard’s been updated. Beginning this year, RH test readings are now documentable after just 24 hours. Doing away with two extra days of waiting comes about because of an ASTM-commissioned […]