Wood Production: Manufacturing & Kiln Drying

Lumber Mill

Lumber mills turn trees into manufactured wood products. Throughout the process, the moisture content (MC) of the wood is an important factor for producer and end user alike.

The lumber manufacturing process generally follows these steps:

  1. Head Rig: the primary saw cuts the tree into sawn pieces or boards.
  2. Edging: removes irregular edges and defects from sawn pieces or boards.
  3. Trimming: the trimmer squares off the ends of lumber into uniform pieces.
  4. Rough Lumber Sorting: pieces are separated based on dimension and final product production, whether the finished piece will be unseasoned (known as “green”) or dry.
  5. Lumber Grade StickersStickering: lumber destined for kiln drying production is stacked with spacers (known as stickers) that allow air to circulate within the stack (green product skips this stage and the next).
  6. Drying: kiln drying wood speeds up the natural evaporation of the wood’s moisture content in a controlled environment.
  7. Planing: smoothes the wood's surfaces and ensures that each piece has a uniform width and thickness.
  8. Grading: assigns a “grade” to each piece of lumber that indicates its quality level, based on a variety of characteristics, including its MC.

Kiln Drying Wood for Maximum Value and Usability

In order to maximize wood's value and strength, mills invest both time and money in the kiln drying processes to remove excessive moisture from the lumber stack. In fact, kiln drying on some hardwood species can take up to (and beyond) a month, depending on the initial MC of the wood.

Properly-dried wood has many advantages over green wood for both producers and consumers alike. It reduces waste in manufacturing and extends the service life and usefulness of wood products, giving the consumer a stable product that will last for years.

The kiln drying process can vary considerably, depending on the species and starting MC of the wood. In general, however, these are the steps in the process:

  1. Lumber producers carefully stack "green" wood, using spacers or “stickers” to create gaps for air to freely circulate throughout the stack.
  2. Once wood is placed in the kiln, depending upon wood species, the kiln is heated to temperatures between 110 to 180 degrees (Fahrenheit) for conventional-temperature kilns and 230 to 280 degrees (Fahrenheit) for high-temperature kilns.
  3. Operators constantly monitor kiln temperatures and relative humidity (RH), as well as the lumber's MC. The goal is to bring the entire stack into its Equilibrium Moisture Content (EMC). Wood continually loses or gains moisture until it is in balance with the surrounding environment. The amount of moisture at that balance point is called the Equilibrium Moisture Content (EMC) and the EMC depends mainly on the relative humidity (RH) and the temperature of the surrounding air.

Lumber Stack DryingThe profitability of lumber manufacturing depends on the mill's ability to maximize the wood's quality throughout the entire lumber manufacturing process. If the wood in a mill's production line is too wet or too dry, the finished product will receive a lower grade, and will have a lower dollar value than a piece that that has been properly kiln dried.

In-line moisture content measurement systems can easily identify and mark pieces that are either too wet or too dry. These pieces can then be pulled from the production line before the planning process and be re-dried or re-milled as necessary to create the highest grade lumber possible for that piece, thus increasing the mill's profits and giving consumers access to better quality materials.

Many consumers and builders believe that concerns about the lumber MC end when the wood is shipped out of the mill. In fact, wood products should be constantly measured and monitored to assure that the MC levels are at optimum EMCs. Wood will naturally continually gain or lose moisture until it reaches this EMC balance with the surrounding environment.    

Wagner Meters has been manufacturing moisture measurement products and services for the wood product industry since the early 1960’s and provides a full range of solutions for both lumber producing mills and consumers who want to get the most value and useful life from their end wood products.


 

 
Print Friendly Print Friendly  Bookmark this Page Bookmark Page  Send this page to a friend Send page to a friend  Visit Wagner's Facebook page Find us on Facebook Follow Wagner on Twitter Follow us on Twitter

 

Wagner Meters | Wood Moisture Meters | Concrete Moisture Testing | Large Lumber Moisture Measurement
1.800.634.9961 · Wagner Meters · © 2001-2013 · All Rights Reserved
326 Pine Grove Rd. Rogue River, OR 97537 USA
Please read our warranty and disclaimer and privacy policy, or contact us. View Sitemap.

Find Wagner Electronics on Facebook!Follow Wagner Electronics on Twitter!Watch Wagner Meters Videos on Youtube!

Log In
Your Account  |  Sign Up

Check Out
Shopping Cart (0 Items)

Questions?
1.800.634.9961
info@wagnermeters.com