Wood Type referenced and Manual Language



The rugged L601-3 is specifically designed for the demanding environment of the sawmill or wood products manufacturing plant where quick-scanning of lumber is a must.

Even large boards can be scanned from end to end in seconds.... It makes the job of moisture detection easier, more thorough and more accurate.

The L601-3's "Wood-Friendly" electromagnetic waves penetrate beyond the surface into the wood to a depth of 1" and provides an instant averaged reading of the board's moisture content in a 2.5" x 2.5" x1" scanning area. Even large boards can be scanned from end to end in seconds with the large 2.5" x 2.5" scanning surface.

  • The L601-3 features an automatic shut-off for long battery life.
  • Virtually unaffected by wood temperature.*

The Quick-scanning Model L601-3 Moisture Meter makes the job of moisture detection easier, more thorough, and more accurate in a high-production environment. The L601-3 is available in Douglas Fir or Southern Yellow Pine referenced versions. An accompanying instruction book includes species adjustment tables for more than a hundred of the most used hardwood, softwood, and imported species.

  • *Contact Wagner Meters' technical support for guidelines when wood is below freezing.
  • Size:L 8.5" x W 4" x H 3.75"
  • Scanning Area: 2.5" x 2.5"
  • Scanning Depth: 1"
  • Weight: 16oz
  • Power: 4AA batteries
  • Measurement Range for Reference:
  • Species (Douglas Fir Southern Yellow Pine) 5% to 30% moisture content

To request a brochure, use the form here.

L601-3 Repair Form

Note: The standard model is for Douglas Fir (in English). For other languages and Southern Yellow Pine (SYP) option please see the drop down menu below:

 

 
Print Friendly Print Friendly  Bookmark this Page Bookmark Page  Send this page to a friend Send page to a friend  Visit Wagner's Facebook page Find us on Facebook Follow Wagner on Twitter Follow us on Twitter

 

Wagner Meters | Wood Moisture Meters | Concrete Moisture Testing | Large Lumber Moisture Measurement
1.800.634.9961 · Wagner Meters · © 2001-2013 · All Rights Reserved
326 Pine Grove Rd. Rogue River, OR 97537 USA
Please read our warranty and disclaimer and privacy policy, or contact us. View Sitemap.

Find Wagner Electronics on Facebook!Follow Wagner Electronics on Twitter!Watch Wagner Meters Videos on Youtube!

Log In
Your Account  |  Sign Up

Check Out
Shopping Cart (0 Items)

Questions?
1.800.634.9961
info@wagnermeters.com