Moisture Meter Home - Wagner Moisture Meters

Wood Moisture Meters

 



Wood Flooring and Woodworking > MMC210 Digital Proline Moisture Meter


MMC210 Digital Proline Moisture Meter

(Click Thumbnail For Larger Image)

Price: $375.00
Quantity:


Item No: #890-00210-001

For purchasing outside of the United States or Canada, please click here

About this Moisture Meter
The MMC210 moisture meter is ideal for wood flooring and woodworking applications that specify common softwood and hardwood species. We recommend the MMC220 moisture meter when your applications include the harder tropical species.

Materials to Measure
Common softwood and hardwood species
Other Building Products – relative reading on materials with similar densities to wood.

Specific Applications
For flooring installers or manufacturers, cabinet or furniture manufacturers, inspectors or lumber suppliers, the MMC210 offers a complete and portable moisture meter designed for domestic woods with a standard specific gravity (SG) range. Easy to use and easy to adjust, the MMC210 can quickly and accurately scan many board feet of incoming lumber or many pieces of wood flooring in just seconds.

Wagner Meters' IntelliSense™ Technology ensures that the MMC210 is measuring deeply IN the wood for a true moisture picture without damage to the wood surface and without interference from surface moisture. Two-button controls make one-handed operation simple. And like all meters at Wagner Meters, there is no need to adjust moisture content (MC) readings for temperature.

The MMC210, with its Press and Hold feature, lets you get into tight places without needing a visual line to the meter display. . Beneath a sink, under a cabinet overhang or in a tight corner, with the Press and Hold Feature you can take the MC reading and the display holds the reading once the meter is removed, letting you quickly and easily document MC readings in all parts of your project.

Lightweight and easy to operate, the MMC210 gives quick and accurate MC readings on the job.

Meter Specifications

Size & Weight

Length – 4 9/16"; Width – 2 3/4"; Height – 1 1/16"; Weight – .37 lbs

Power

Power – 9 volt battery
Auto Power Shut Down – 60 seconds

Control

Two button control for on/off and species settings
Press & Hold feature

Depth of Measurement

3/4"

Moisture Content

5% - 30%

Digital Display in .1% increments

Scanning Area

1 1/2" x 2 1/2"

Specific Gravity

Selectable wood species setting .30-.70

Calibration

Verifiable with Calibration Block (sold separately)

Other

7 year warranty
Battery Included
Shock Resistant Carrying Case with Belt Clip Included
Reference Library CD included with meter
Operating Temperature 30-110° F


Download PDF Moisture Meter Manual

Download PDF Moisture Meter Species Adjustment Tables

Specific Gravity Determination Help

MMC 210 Moisture Meter Repair Form

 

 
Print Friendly Print Friendly  Bookmark this Page Bookmark Page  Send this page to a friend Send page to a friend  Visit Wagner's Facebook page Find us on Facebook Follow Wagner on Twitter Follow us on Twitter

 

Wagner Moisture Meter | Wood Moisture Meters | Concrete Moisture Testing | Large Lumber Moisture Measurement
1.800.634.9961 · Wagner Meters · © 2001-2012 · All Rights Reserved
326 Pine Grove Rd. Rogue River, OR 97537 USA
Please read our warranty and disclaimer and privacy policy, or contact us. View Sitemap.

Find Wagner Electronics on Facebook!Follow Wagner Electronics on Twitter!Watch Wagner Meters Videos on Youtube!

Log In
Your Account  |  Sign Up

Check Out
Shopping Cart (0 Items)

Questions?
1.800.634.9961
info@wagnermeters.com