temperature measurment
05-29-2010, 10:18 AM
Post: #1
temperature measurment
hi !

could anyone help me to find an instrument which i could measure the temperature at one point inside of concrete!!

Wink
Find all posts by this user
Quote this message in a reply
05-31-2010, 08:12 AM
Post: #2
RE: temperature measurment
Hello!

You can use the Wagner Rapid RH to accurately measure temperature inside concrete. You can place the probe at any depth and read both relative humidity and temperature with certified accuracy. The probes are fast, easy to install and inexpensive.
Find all posts by this user
Quote this message in a reply
06-01-2010, 08:36 AM
Post: #3
RE: temperature measurment
could you please tell me how does it measure the temperature?
i though that it just measure the moisture!!
Find all posts by this user
Quote this message in a reply
06-01-2010, 08:20 PM
Post: #4
RE: temperature measurment
The sensor accurately measures both temperature and humidity. They are NIST certified and easy to use. You will not be disappointed!

The LCD display will show you both temperature and relative humidity.
Find all posts by this user
Quote this message in a reply
06-04-2010, 03:29 AM
Post: #5
RE: temperature measurment
ok! tnx
but just one another question!
are rapidrh just for one usage?
or i can use them for several times?
Find all posts by this user
Quote this message in a reply
06-04-2010, 09:31 PM
Post: #6
RE: temperature measurment
The Rapid RH probes were designed to seal quite tightly in the hole they are inserted in. This insures precise measurement at a precise depth, which is one reason the probes are so accurate and reliable.

This tight fit makes them very hard to remove, and if they are removed the sealing flange may be damaged. They are intended for a single installation in concrete. Although I have seen some removed and re-used, I don't recommend the practice.