RE: VCT Over CutBack
The thing to remember is that new VCT has a lower Perm Rating than old VCT. VCT has improved and made much more dense now. (still more C than V in VCT) So, while you can go two layers watch out if you are moving from brand to brand. Perhaps Armstrong is now more perm but usually the stuff is lower perm.

I often get people asking us to put sheet over VCT which is just a bad idea. VCT on VCT is borderline. Carpet over VCT is skim and go since Carpet breathes
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
VCT Over CutBack - Ernesto - 02-04-2014, 10:27 AM
RE: VCT Over CutBack - eaadams - 02-19-2014, 10:37 AM
RE: VCT Over CutBack - CC Solutions - 02-25-2014, 06:04 PM
RE: VCT Over CutBack - eaadams - 02-25-2014, 10:50 PM
RE: VCT Over CutBack - hausenheimer - 02-26-2014, 06:58 AM
RE: VCT Over CutBack - M.K.Pecou - 02-26-2014, 07:30 AM
RE: VCT Over CutBack - CC Solutions - 02-26-2014, 04:37 PM
RE: VCT Over CutBack - Ernesto - 02-27-2014, 03:02 PM