Bikram Yoga
10-09-2013, 04:26 PM,
#1
Bikram Yoga
So do you test at the standing temp in the room, 85deg or at the high point in the room 105deg (hits 105 during classes but then they ramp down)
Quote this message in a reply
10-15-2013, 08:05 PM,
#2
RE: Bikram Yoga
That's a bewdy.

When F2170 said "service conditions" they may not have considered a Yoga class...
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Quote this message in a reply
10-23-2013, 01:28 PM,
#3
RE: Bikram Yoga
Something I just realized. Often when we do a gym in California we will install at 80 but in the summer when the kids go home the room can easily get into the 100-115 range.

I wonder what effect that has?