Relative Humidity Hysteresis

#5
Have a slab that is sitting at 99% but some probes are dropping. It is new, closed off from elements all winter, no sand under slab. How do I know if the stuff hanging at 99% are subject to Hysteresis?
Reply


Messages In This Thread
Relative Humidity Hysteresis - eaadams - 05-24-2013, 09:53 AM
RE: Relative Humidity Hysteresis - eaadams - 05-28-2013, 10:35 AM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:35 PM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:41 PM