hysteresis |ˌhistəˈrēsis| noun Physics
the phenomenon in which the value of a physical property lags behind changes in the effect causing it, as for instance when magnetic induction lags behind the magnetizing force.


Layman's terms: RH probes can lag behind the actual reading by a small amount as the concrete humidity changes. You'll have to ask Jason or Ed if hysteresis can cause a lag greater than the percentage of variation inherent in the probes.

If I am close to a target RH before a go / no-go decision is going to be made, I insert a couple fresh probes to get new readings to compare.

I think this is really important if the probes started out reading in the high 90's. The alkalinity is so high at that RH I don't see how the sensors resist damage if they are exposed to it for a long period of time.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
Relative Humidity Hysteresis - eaadams - 05-24-2013, 09:53 AM
RE: Relative Humidity Hysteresis - CC Solutions - 05-27-2013, 10:32 AM
RE: Relative Humidity Hysteresis - eaadams - 05-28-2013, 10:35 AM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:35 PM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:41 PM

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)