12-07-2012, 01:00 PM,
#11
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
It was all the big CSI spec writers around the county. Gensler, AECOM, Perkins & Will, HOK etc... Probably 150+ on the call.

But it was pretty basic. Focused, I think, too much on mitigation and not enough on concrete design to avoid the issues in the first place.

There was a consensus they need to do it again and perhaps less 'general' I would hope.

I'll post a link to you YouTube video when uploaded
Quote this message in a reply
12-07-2012, 01:08 PM, (This post was last modified: 12-07-2012, 01:09 PM by CCR.)
#12
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
Thanks for the thoughtLightbulb Don't think so. I have given talks on the subject to upwards of 100 people, but I would never want to do something via Skype...I'd be a nervous wreck.

Thanks!!
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Quote this message in a reply
12-22-2012, 12:41 PM, (This post was last modified: 12-22-2012, 12:46 PM by eaadams.)
#13
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
(12-01-2012, 09:36 AM)CC Solutions Wrote:  Count me in.
They still use blotter layers by you? Huh

Dealing with this plan right now. They just will not listen.

[Image: A-lH1DzCYAAIR9h.jpg:large]

I need to learn what the control vs weakened plane joints are. I suspect control = active joints = NO GOOD for a gym. Any help?

What does E.W. mean?

Infact if someone wanted to take the above and do a point by point transaltion of what it 'says' and what someone needs to know when I read this it would be a good contribution.
Quote this message in a reply
12-22-2012, 03:26 PM,
#14
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
E.W. = Each Way.

Blotter layers suck. And sand? How do they keep that from displacing while they are pouring unless they wet it first???
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply
12-22-2012, 03:43 PM,
#15
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
I haven't seen a blotter course specified in ages. Not a good idea at all. What is their rationale? Perhaps another example of "cut and paste spec writing"
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Quote this message in a reply
12-22-2012, 04:15 PM,
#16
RE: Event: 12/6 CSI Topic: Floor Slab Moisture
In California I see it on >90% of jobs. At least every week. It may be cut and paste / lazy specs. When I confront the engineers on it, it is usually in hopes of lessening for slab curl since the prices people get for grinding off some curled edges are outrageous.