Might there be a new product idea here? Could wagner make a RH profile testing stick that could be placed in a single hole and test the RH profile or gradient of the floor?

The cost of doing five tests on each slab at different depths adds a lot of cost to (for me) a 6000 sf gym with 5" slab. I already have to pay for 6 probes. To do another 5 more probes further increases the cost by more than $250. A re-usable stick in a 5" hole might be a better product.

OR must the tests be exposed to the bottom of a hole to get a good RH reading?
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Reverse Curl & Relaxation - eaadams - 10-03-2012, 11:36 AM
RE: Reverse Curl & Relaxation - rapidrhrep - 10-03-2012, 07:45 PM
RE: Reverse Curl & Relaxation - eaadams - 10-04-2012, 10:21 AM
RE: Reverse Curl & Relaxation - eaadams - 10-02-2013, 12:58 PM