This is not uncommon even with an experienced installer. Light grinding is fastest and you don't need to "blend" the ridges into surrounding areas in order to achieve a nice flat surface for the floor covering.

As far as pinholes, that is typically a result of the K15 being installed over a highly absorbant slab, resulting in the mix water being sucked out of the K15 too fast. Did they prime the concrete with P-51 Primer as required? Highly absorbant concrete needs to be "double primed" with P-51. Prime with P-51 mixed with 3 parts water, dry for an hour or so, then prime 1:1 with water (normal mix ratio), before installing the K-15.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Reply


Messages In This Thread
SLU - eaadams - 06-29-2012, 05:38 PM
RE: SLU - CCR - 07-01-2012, 04:44 AM
RE: SLU - CC Solutions - 07-01-2012, 08:49 AM

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)