4.0
I have set 100's if not 1000's of wagner probes. I went to a job today and opened a new pack of probes and found that they were a new series 4.0 probes. I had to set 7ea probes. I totally destroyed 3 probes and I have no confidence that the ones I was able to set are at the bottom of the hole.

Wagner has taken a very good system and Rube Goldberged it into a system that is barely usable. Please fix this 4.0 system or go back to the old system.