Successful floor repair after failure!
09-29-2011, 06:53 AM,
#14
RE: Successful floor repair after failure!
(09-29-2011, 06:48 AM)Ernesto Wrote:  I never reccomend chemical cleaning, good luck to ya.

I never do either. I said that several posts prior.
I use hot water pressure washing in a process to remove chemicals, fats and oils from the concrete. Often this is after someone used a chemical stripper.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]