(09-27-2011, 06:39 AM)CC Solutions Wrote:  Or they do a bond test on an area they rinsed really well.

Uh huh, rinsing a home throughly is kinda out of the question unless the sheetrock is a foot off the ground. Smile not to mention all the water that goes back into the concrete that takes ten times longer to exit than mix water.


Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com








Messages In This Thread
Successful floor repair after failure! - CC Solutions - 09-23-2011, 06:27 AM
RE: Successful floor repair after failure! - Ernesto - 09-26-2011, 10:29 AM
RE: Successful floor repair after failure! - CC Solutions - 09-26-2011, 06:16 PM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 06:33 AM
RE: Successful floor repair after failure! - CC Solutions - 09-27-2011, 06:39 AM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 08:10 PM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 06:20 AM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 06:44 AM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 02:20 PM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 02:51 PM
RE: Successful floor repair after failure! - FloorMedic's - 09-28-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 05:07 AM
RE: Successful floor repair after failure! - Ernesto - 09-29-2011, 06:48 AM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 06:53 AM
RE: Successful floor repair after failure! - eaadams - 09-29-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-30-2011, 07:55 AM
RE: Successful floor repair after failure! - foxgeorge - 12-15-2011, 01:46 AM
RE: Successful floor repair after failure! - Adonis - 12-19-2011, 11:54 PM
RE: Successful floor repair after failure! - mableswift - 12-22-2011, 10:13 PM
RE: Successful floor repair after failure! - eaadams - 12-22-2011, 10:29 PM
RE: Successful floor repair after failure! - CC Solutions - 12-23-2011, 06:37 AM

Users browsing this thread:
3 Guest(s)