RFID = Radio Frequency Identification?

Do you mean a probe that will transmit the data? I know they have those.

I always have a witness look at the readings. Not every time, but if the installer is ready to go, I walk around with him and we check the readings. Or usually someone from the GC is always looking over my shoulder.

Then I follow up with a report stating the readings, all parameters of the testing, and any attendees that watched the testing. I email that to whoever hired me and file a copy in my office.

Usually a dated copy of a report is enough evidence that if any problems came up you could use that as the basis. If there was a question about the readings at the date of the original report, someone would have mentioned it then.


JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
metal disks - eaadams - 09-14-2011, 05:12 PM
RE: metal disks - CC Solutions - 09-14-2011, 06:23 PM
RE: metal disks - eaadams - 09-14-2011, 06:32 PM
RE: metal disks - CC Solutions - 09-15-2011, 04:56 AM
RE: metal disks - rapidrhrep - 09-15-2011, 08:30 AM
RE: metal disks - CC Solutions - 09-15-2011, 01:02 PM
RE: metal disks - rapidrhrep - 09-15-2011, 01:58 PM
RE: metal disks - CC Solutions - 09-15-2011, 02:23 PM
RE: metal disks - eaadams - 09-15-2011, 02:29 PM
RE: metal disks - CC Solutions - 09-15-2011, 05:39 PM
RE: metal disks - eaadams - 09-15-2011, 06:25 PM
RE: metal disks - CC Solutions - 09-15-2011, 06:44 PM
RE: metal disks - eaadams - 09-15-2011, 06:51 PM
RE: metal disks - CC Solutions - 09-15-2011, 07:17 PM
RE: metal disks - Ernesto - 09-18-2011, 03:03 PM
RE: metal disks - CC Solutions - 09-18-2011, 06:18 PM
RE: metal disks - Ernesto - 09-20-2011, 07:18 PM
RE: metal disks - FloorMedic's - 09-20-2011, 08:43 PM
RE: metal disks - CC Solutions - 09-21-2011, 05:58 AM
RE: metal disks - Ernesto - 09-21-2011, 07:38 PM
RE: metal disks - CC Solutions - 09-21-2011, 09:16 PM

Users browsing this thread:
2 Guest(s)