My method of adressing cracks is:
1. Make sure they are dormant
2, Clean them out thoroughly all the way to the bottom, usually 1-inch
3, Use a high compressive strength patch about 7 -8,000 psi
4. don't over water the patch, instead dampen the crack with a damp rag.

Remember if the crack moves it will move.
Regards
Rayt