Thread Rating:
  • 0 Vote(s) - 0 Average
  • 1
  • 2
  • 3
  • 4
  • 5
How are you addressing cracks?
08-19-2011, 04:20 PM,
#5
RE: How are you addressing cracks?
The concrete in the trenches is new. The surrounding concrete is old.
The vapor retarder was compromised when the trenches were cut. The moisture is coming through the joints. The flooring is vinyl sheet. The trench was doweled and for the most part stable, but the concrete will cure for about 30 years and may shrink a bit over that time.
Roadware is a good product, like I said, I use a polyurea semi-rigid.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious