08-15-2011, 04:04 AM,
#11
RE: Cold Expansion Joint
Sometimes it works out to be the best. I lose jobs every day because people don't want to do it right. Sad
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply
08-16-2011, 08:11 PM,
#12
RE: Cold Expansion Joint
Doin it right is cheaper than crossing fingers.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Quote this message in a reply
08-19-2011, 07:14 AM,
#13
RE: Cold Expansion Joint
(08-16-2011, 08:11 PM)Ernesto Wrote:  Doin it right is cheaper than crossing fingers.

I may steal that line.... I like it a lot! Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply
10-21-2011, 06:53 PM,
#14
RE: Cold Expansion Joint
Jd you mentioned the euco quikjoint 200. Perhaps you know the other products.

I have a job where GC put euco 700 in a stress crack (poorly spaced joints) running the whole width of slab 80'.

Now we can see a line tracking the crack repair under the flooring. Does that jive in your mind?

I am having a hard time understanding the difference between them.
Quote this message in a reply
10-21-2011, 07:30 PM,
#15
RE: Cold Expansion Joint
(10-21-2011, 06:53 PM)eaadams Wrote:  Jd you mentioned the euco quikjoint 200. Perhaps you know the other products.

I have a job where GC put euco 700 in a stress crack (poorly spaced joints) running the whole width of slab 80'.

Now we can see a line tracking the crack repair under the flooring. Does that jive in your mind?

I am having a hard time understanding the difference between them.

Understanding the difference between what?

If you see a crack, the joint has moved. Why else would you see the crack?
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply
10-21-2011, 07:49 PM,
#16
RE: Cold Expansion Joint
Between why the structural engineer would spec a epoxy euco 700 vs the polyurea euco 200.

When I read about the two it seems to say the.same thing.
Quote this message in a reply
10-22-2011, 07:24 AM,
#17
RE: Cold Expansion Joint
The 700 is an epoxy and harder. Has a longer open time and would flow to the bottom of the crack better.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]