I had a request to install two different Rh probes.

#5
$60 per hole is a steal and you know it! I see some guys charging well over $100. If it's a bigger job a guy can afford to go $60 a hole. Like 25 probes minimum. Or if you're like me and just practically give stuff away.

But I met some players in the business, helped out a regular contractor of mine, and in the end got a decent job from it. Wink
JD Grafton
Concrete Answers for Flooring Problems
[email protected]