I had a request to install two different Rh probes.
|
|
08-07-2011, 09:40 AM
Post: #13
|
|||
|
|||
|
RE: I had a request to install two different Rh probes.
If I drive 30 minutes to do 6 tests, I will invest a total of 2 hours driving, 2 hours installing, 1 hour reading the probes after 72 hours, and 1 hour writing a report. I will have $200 in probe costs.
I will charge $70 each for 6 probes, or $420. My profit is then $220 for 6 hours of my time, or $37 an hour. If I can combine the trips with something else in that area, and get the probes installed without a lot of chit-chat, I can shave an hour or two off that timeline and come a lot closer to the $60 an hour I would like to make. Okay so maybe I am too cheap on installing....
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|