high rh in concrete
|
|
09-07-2009, 03:34 PM
Post: #1
|
|||
|
|||
|
high rh in concrete
Before flooring is installed how can you lower rh to acceptable
levels.concrete is poured six months rh is still reading at 90% |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
high rh in concrete - chas04344 - 09-07-2009 03:34 PM
RE: high rh in concrete - WMiller - 09-10-2009, 09:40 AM
RE: high rh in concrete - chas04344 - 09-11-2009, 07:33 PM
|