Concrete Surface Texture
05-27-2011, 10:38 AM
Post: #11
RE: Concrete Surface Texture
Ray that is not my point. I'm not looking at removing a surface.

I'm talking about the smoothness needed for resilient sheet flooring. A CSP of 3-4 would need to be re surfaced to put flooring on.
Find all posts by this user
Quote this message in a reply
06-21-2011, 11:42 AM
Post: #12
RE: Concrete Surface Texture
Concrete should have the texture of about 100 grit sandpaper to obtain a good mechanical bond for sheet vinyl adhesives and especially epoxies. Burnished concrete not only compromises adhesive bond, but retards the moisture drying in a timely fashion. If the moisture is there it is going to get out eventually.
Regards
Rayt
Find all posts by this user
Quote this message in a reply
06-21-2011, 11:47 AM
Post: #13
RE: Concrete Surface Texture
Agreed Ray. The big issue is open and porous, and sandpaper type texture is an easy reference. Sandpaper is everywhere.

Looking back over the posts, that CC Solutions guy has some good info on this thread... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious