Just had a testing firm do a slab for us.
CaCl went from 3.7-4.7 rH went from 95.3-99.4 (not rapidrh probes, unfortunately) yikes! But what was interesting and relevant to a thread is that the testing firm did a QC test site which I take to mean Quality Check. At one test site they did two rH tests (not on the report but in the picture) and they did two CaCl tests. The CaCl tests came out the same. But I am not sure showing two tests next to each other is necessarily a valid gauge of quality. Does anyone know if this quality check type test is in the ASTM literature? |
|||
|