Moisture issues in concrete slab
I am going over to Hawaii to install a large marble floor on a concrete slab. This will be a new slab. Is there anything I need to know about moisture in the slab in Hawaii that won't be taken care of with the vapor barrier after a 28 day cure due to the humidity or anything else? This is above grade.
|
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Moisture issues in concrete slab - McTile - 08-29-2009 04:49 PM
RE: Moisture issues in concrete slab - Bryan F - 09-01-2009, 01:45 PM
RE: Moisture issues in concrete slab - RCConcrete Consulting - 09-21-2009, 05:17 PM
|