coverage
|
|
08-24-2009, 07:36 AM
Post: #2
|
|||
|
|||
|
RE: coverage
According to the ASTM standard, it's 3 tests for the first 1000 ft^2 and 1 test for each 1000 ft^2 after that.
|
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
RE: coverage - jf222 - 08-24-2009 07:36 AM
|