I am thinking using the RapidRH system but cannot find how many tests should be used for 1000 sqft
|
|||
|
08-24-2009, 07:36 AM
Post: #2
|
|||
|
|||
|
RE: coverage
According to the ASTM standard, it's 3 tests for the first 1000 ft^2 and 1 test for each 1000 ft^2 after that.
|
|||
|