04-09-2011, 02:06 PM
Post: #28
|
|||
|
|||
|
RE: RH Numbers Rising
When a blotter is used, and there is a hole in the vapor retarder, the moisture will impact the entire slab. Example is a 16d nail hole in a vapor retarder will allow 3 pints of water through per day. That water will travel laterally in the blotter layer to affect the entire slab.
Curing compounds and sealers are a major concern to flooring installations. It is just one more thing to fail. Rayt |
|||
|