"the blotter layer" is the main problem in the West. FYI everyone - I know of a major architect who is now being sued because of their use of it in a 2006 slab. Our instructions removed the blotter layer in 1999. I look forward to getting deposed because it is not the Architect's fault. It is the structural engineer to whom they subbed out that work. I can't wait to throw him under the bus.

Even CalGreen (the new building code) still allows for it if the slab is "designed by a structural engineer". Well ... I can't wait to see one of these engineers get sued. They are the ones who are the cause in fact for 80% of the floor failures we have had to deal with. Not the flooring sub, not the gc, not the architect, not the curing compound, not the adhesive, not the material suppler, the engineer should be blamed.

It will be interesting to see what gets decided. But, it will probably settle out of court.
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RH Numbers Rising - COD - 04-05-2011, 09:40 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 10:49 AM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 11:49 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 12:19 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 12:27 PM
RE: RH Numbers Rising - COD - 04-05-2011, 01:16 PM
RE: RH Numbers Rising - CC Solutions - 04-05-2011, 05:26 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 08:42 PM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 06:04 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 07:40 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 08:23 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 08:28 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 04:54 PM
RE: RH Numbers Rising - CC Solutions - 04-07-2011, 06:12 AM
RE: RH Numbers Rising - rthompson - 04-07-2011, 01:08 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 08:01 AM
RE: RH Numbers Rising - CC Solutions - 04-08-2011, 08:06 AM
RE: RH Numbers Rising - rthompson - 04-08-2011, 10:33 AM
RE: RH Numbers Rising - eaadams - 04-08-2011, 04:19 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 04:54 PM
RE: RH Numbers Rising - eaadams - 04-08-2011, 05:00 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 08:59 AM
RE: RH Numbers Rising - rthompson - 04-09-2011, 11:57 AM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:14 PM
RE: RH Numbers Rising - eaadams - 04-09-2011 01:38 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:46 PM
RE: RH Numbers Rising - rthompson - 04-09-2011, 02:06 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 02:39 PM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 09:49 AM
RE: RH Numbers Rising - CC Solutions - 04-11-2011, 09:54 AM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 08:50 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 12:26 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:10 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 01:20 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:28 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 03:08 PM
RE: RH Numbers Rising - eaadams - 04-18-2011, 04:46 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 04:55 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 05:15 PM
RE: RH Numbers Rising - Ernesto - 04-20-2011, 07:58 AM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 08:02 AM
RE: RH Numbers Rising - rthompson - 04-20-2011, 05:15 PM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 09:00 PM
RE: RH Numbers Rising - Ernesto - 04-23-2011, 07:01 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 07:59 PM
RE: RH Numbers Rising - CC Solutions - 04-23-2011, 08:59 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 10:01 PM
RE: RH Numbers Rising - Ernesto - 04-24-2011, 08:24 AM
RE: RH Numbers Rising - eaadams - 09-08-2011, 06:08 PM
RE: RH Numbers Rising - CC Solutions - 09-09-2011, 08:11 AM
RE: RH Numbers Rising - rthompson - 09-09-2011, 09:36 AM
RE: RH Numbers Rising - Ernesto - 09-09-2011, 04:48 PM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 09-10-2011, 11:14 AM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 06:30 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:22 AM
RE: RH Numbers Rising - rthompson - 09-11-2011, 08:25 AM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:40 AM
RE: RH Numbers Rising - CC Solutions - 09-11-2011, 03:54 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 06:50 PM
RE: RH Numbers Rising - rthompson - 09-12-2011, 08:56 AM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 09:07 AM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 05:14 PM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 05:33 PM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 07:27 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:49 AM
RE: RH Numbers Rising - rthompson - 09-13-2011, 08:37 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 08:43 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 10:08 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 11:28 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 01:37 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 01:55 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:14 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 02:17 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:18 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 02:33 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 05:26 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:46 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:56 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 06:03 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 06:06 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:23 PM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 06:29 AM
RE: RH Numbers Rising - CC Solutions - 09-14-2011, 06:54 AM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 07:39 PM
RE: RH Numbers Rising - CC Solutions - 09-15-2011, 04:59 AM
RE: RH Numbers Rising - Ernesto - 09-20-2011, 08:07 PM
RE: RH Numbers Rising - CC Solutions - 09-20-2011, 08:30 PM
RE: RH Numbers Rising - Ernesto - 09-21-2011, 08:19 PM
RE: RH Numbers Rising - CC Solutions - 09-21-2011, 09:18 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:39 AM
RE: RH Numbers Rising - CC Solutions - 09-22-2011, 09:28 AM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 07:14 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 07:50 PM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 08:00 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:48 PM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 05:54 AM
RE: RH Numbers Rising - Ernesto - 09-23-2011, 06:58 AM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 10:37 AM