concrete slab drying time
I've got a deck that I've got to measure, and I hear that they dry differently, or that ASTM classifies them differently, or something along those lines, because it's up off the ground. Is that true?
|
|||
|
07-09-2009, 01:46 PM
Post: #2
|
|||
|
|||
|
RE: concrete slab drying time
Is your concrete slab on a metal deck? How did you pour it?
Basically, ASTM F2170 says that if the slab is drying only from the top, you should drill to 40% into it for your test. If it's drying from both sides (which means it's not on a metal deck or sitting on the ground with a vapor retarder below) than you only should drill down 20% of the thickness |
|||
|