RE: Concrete floor and laminate
(04-01-2011 06:53 AM)Ernesto Wrote:  I don't believe there is anything 100%.Show me the puddin.Big Grin

Like I said, Ardex may warrant 100% if you ask and they inspect the installation.

Koester warrants 100% and unlimited RH every day.

The KEY to any of these systems when pushed to the max is proper preparation.