Relative Humidity Probe Depth
03-23-2011, 09:16 AM
Post: #7
RE: Relative Humidity Probe Depth
I know it sounds crazy but this is a good tool to have just to check to see if a slab does have continual steel reinforcement.
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Relative Humidity Probe Depth - mwoody - 03-21-2011, 07:23 PM
RE: Relative Humidity Probe Depth - mwoody - 03-22-2011, 05:41 AM
RE: Relative Humidity Probe Depth - admin - 03-23-2011, 07:54 AM
RE: Relative Humidity Probe Depth - eaadams - 03-23-2011 09:16 AM
RE: Relative Humidity Probe Depth - mwoody - 03-23-2011, 05:12 PM