RE: Ph Of Concrete
(02-26-2011 12:10 AM)barry88rowe Wrote:  I have no idea why the pH in your influent water varies, I'd check environmental factors such as rainfall, temperature, and time of year for correlation.

Welcome Barry!!

Most of the concrete slabs we deal with will be either on grade with a vapor retarder below them or raised and poured in a pan. There should really be no influent moisture, only the original moisture included in the concrete mix. Temperature should be at service conditions.

Actually if you have incoming water, the PH is irrelevant! You have a real problem. Big Grin

If I'm off-base please don't be shy to say so! I get that a lot around here. Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious