(02-14-2011 11:22 PM)eaadams Wrote: Sounds to me like you used a good adhesive like mapei's new high moisture products for engineered wood. Or it was a floating click together like a tekno. All sort of options are out there No, I do not glue down click systems. I used Bostik Best and thats all. I just had a feeling and the slab was full of spiderweb cracks in the surface so I figured the readings were artificially high due to the cracks.I was patching and you could virtually see the water get sucked out of the patch. And it just looked dry.....OOOOOOOOH lol
Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|