I still to this day cannot understand why people think perforated sleeves or even no sleeve can give you the correct rh number. The concept is not all that hard to grasp.

Take this example, get a dry sponge, dip the bottom part in water and take it out immediately, notice how the bottom is wet and SOME water will wick up the sponge. Now, lets say your going to drill a hole down in there at 40% level and have a perforated tube. Whats it going to read?

Thats how I explain it to people. Next time at lunch n learn take a dry kitchen scrubby sponge with ya.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Was on a job yesterday.... - CC Solutions - 02-12-2011, 12:30 PM
RE: Was on a job yesterday.... - eaadams - 02-12-2011, 03:02 PM
RE: Was on a job yesterday.... - eaadams - 02-12-2011, 09:02 PM
RE: Was on a job yesterday.... - Ernesto - 02-13-2011 08:44 AM
RE: Was on a job yesterday.... - Ernesto - 02-13-2011, 04:47 PM
RE: Was on a job yesterday.... - eaadams - 02-13-2011, 09:53 PM
RE: Was on a job yesterday.... - Ernesto - 02-14-2011, 06:59 AM
RE: Was on a job yesterday.... - Ernesto - 02-14-2011, 08:27 PM
RE: Was on a job yesterday.... - eaadams - 02-14-2011, 11:26 PM
RE: Was on a job yesterday.... - Ernesto - 02-15-2011, 07:52 AM
RE: Was on a job yesterday.... - admin - 10-03-2011, 08:59 AM