(12-23-2008 04:15 PM)Chris Reynold Wrote: What’s the big deal with the HVAC? Do I need it on when testing? Mr. Reynolds, It is a good idea, cold conditions will drive the moisture down deeper giving your test results a false positive. Also the HVAC will help get the slab into equalibrium. Regards Rayt |
|||
|