99% RH in concrete slab
|
|
02-06-2011, 11:31 AM
Post: #14
|
|||
|
|||
|
RE: 99% RH in concrete slab
I wonder what Woody found out?
Maybe the two high readings were drilled right through the slab and then the probes were set at 40% depth... I see that more than I care to!!!
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|