Moisture Meters
|
|
10-21-2008, 11:49 AM
Post: #5
|
|||
|
|||
|
RE: Moisture Meters
Blake,
About 40% the thickness of the slab. 4" slab about 1-1/2 - 1-3/4" Rayt |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Moisture Meters - concreteworker27 - 09-11-2008, 09:00 AM
RE: Moisture Meters - rthompson - 09-12-2008, 01:28 PM
RE: Moisture Meters - Blake McFee - 09-12-2008, 05:42 PM
RE: Moisture Meters - rthompson - 09-15-2008, 04:19 PM
RE: Moisture Meters - rthompson - 10-21-2008 11:49 AM
|