(12-10-2010 11:09 PM)Selah4Makens Wrote:  The Concrete Encounter is a hand-held electronic moisture meter that utilizes non-destructive impedance measurement for moisture determination. Parallel co-planer electrodes are mounted on the unit's base which transmit low-frequency signals into the concrete... The results give the average moisture content to a depth of 2-6 inches during the drying period.

I will argue that 2-6 inches all day long! EI readings are as much witchcraft and hocus-pocus as diving rods and crystal balls.... In my humble opinion that is... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
moisture meter - sbhtennis - 10-29-2010, 09:33 AM
RE: moisture meter - Ernesto - 11-03-2010, 07:18 AM
RE: moisture meter - sbhtennis - 11-03-2010, 09:30 AM
RE: moisture meter - Ernesto - 11-03-2010, 07:04 PM
RE: moisture meter - CC Solutions - 11-07-2010, 12:59 PM
RE: moisture meter - Ernesto - 11-10-2010, 02:02 PM
RE: moisture meter - sbhtennis - 11-10-2010, 06:48 PM
RE: moisture meter - Ernesto - 11-11-2010, 12:02 PM
RE: moisture meter - sbhtennis - 11-11-2010, 06:34 PM
RE: moisture meter - CC Solutions - 11-13-2010, 11:31 AM
RE: moisture meter - sbhtennis - 11-13-2010, 09:20 PM
RE: moisture meter - CC Solutions - 11-14-2010, 10:18 AM
RE: moisture meter - Justin - 11-18-2010, 05:01 PM
RE: moisture meter - CC Solutions - 11-19-2010, 05:31 PM
RE: moisture meter - Ernesto - 11-20-2010, 01:08 PM
RE: moisture meter - sbhtennis - 11-20-2010, 02:28 PM
RE: moisture meter - eaadams - 12-04-2010, 11:02 AM
RE: moisture meter - sbhtennis - 12-04-2010, 04:03 PM
RE: moisture meter - CC Solutions - 12-05-2010, 07:15 AM
RE: moisture meter - eaadams - 12-05-2010, 12:41 PM
RE: moisture meter - sbhtennis - 12-05-2010, 08:04 PM
RE: moisture meter - CC Solutions - 12-05-2010, 09:59 PM
RE: moisture meter - Ernesto - 12-07-2010, 07:48 PM
RE: moisture meter - sbhtennis - 12-07-2010, 10:39 PM
RE: moisture meter - CC Solutions - 12-07-2010, 10:58 PM
RE: moisture meter - sbhtennis - 12-08-2010, 10:00 PM
RE: moisture meter - Ernesto - 12-10-2010, 07:26 AM
RE: moisture meter - sbhtennis - 12-10-2010, 07:33 AM
RE: moisture meter - Selah4Makens - 12-10-2010, 11:09 PM
RE: moisture meter - Ernesto - 12-11-2010, 07:49 AM
RE: moisture meter - CC Solutions - 12-11-2010 06:11 PM