(12-10-2010 11:09 PM)Selah4Makens Wrote: The Concrete Encounter is a hand-held electronic moisture meter that utilizes non-destructive impedance measurement for moisture determination. Parallel co-planer electrodes are mounted on the unit's base which transmit low-frequency signals into the concrete... The results give the average moisture content to a depth of 2-6 inches during the drying period. I will argue that 2-6 inches all day long! EI readings are as much witchcraft and hocus-pocus as diving rods and crystal balls.... In my humble opinion that is...
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|