Multiple Readings?
|
|
11-11-2010, 02:10 PM
Post: #1
|
|||
|
|||
|
Multiple Readings?
I recently read a probe (New Wagner Orange Reader) and got a reading of 89% at 69°. I immediately read the test again and got a reading of 86% at 71°. I read it a third time at 83% at 72°.
Can I assume the first reading is correct? My assumption is when taking multiple readings the electrical current running thru the sensor is causing it to heat up and reducing the RH in the hole. Is this correct? |
|||
|