10-13-2008, 10:11 AM
Post: #1
|
|||
|
|||
|
Rh readings
Ray,
Am I right in assuming that the closer the RH of the Concrete and the RH of the Building enviroment( Bldg with HVAC on), the less likely there will be a moisture problem? I know some manufacturers say that the RH should be no more that 70 percent, but isn't it the difference in the Rh of the concrete and the RH of the air the main reason there may be problems? Dennis McKenzie |
|||
|